SPOOLARC 120

Spoolarc 120 is designed to weld high strength, quenched and tempered steels.

Features

Spoolarc 120 is designed for welding high strength quenched and tempered steels. Weld metal mechanical properties produce high tensile strengths, in excess of 120 ksi (825 MPa). Applications for Spoolarc 120 include military tanks, ships, submarines and other similar fabrication.

Spoolarc 120
  • Industry
  • Shipbuilding
  • General Fabrication
  • Mobile Machinery
  • Welding Process
  • SAW (Sub Arc)
  • GTAW (TIG)
  • GMAW (MIG)

Classifications

  • Classifications/Approvals

    • AWS/ASME SFA 5.23 EM4
    • AWS/ASME SFA 5.28; ER120S-1

Properties

Typical Properties
As Welded GMAW 98% Ar / 2% O2  
Yield Strength 112 ksi, 775 MPa
Tensile Strength 123 ksi, 840 MPa
Elongation in 2" 19 %
Typical Charpy V-Notch Impact Properties  
Testing Temperature -60°F (-51°C)  
As Welded GMAW 98% Ar / 2% O2 75 ft.-lbs., 102 J
Testing Temperature 0°F (-18°C)  
As Welded GMAW 98% Ar / 2% O2 100 ft.-lbs., 136 J
Typical Undiluted Weld Metal Analysis  
GMAW 98% Ar / 2% O2  
C 0.07 %
Mn 1.3 %
Si 0.35 %
P 0.007 %
S 0.008 %
Cr 0.4 %
Ni 2.6 %
Mo 0.45 %
Typical Wire Analysis  
C 0.05 %
Mn 1.6 %
Si 0.3 %
P 0.005 %
S 0.004 %
Cr 0.3 %
Ni 2.3 %
Mo 0.5 %

Part No.

120
Part No. Model / Product Description UPC
2114F30 120 CU 3/32X65#CL 662303668471
2114F32 120 CU 1/8X65#CL 662303510183
211UF87 120 CU 045X550#OMP 20 4/PLT 662303668310
2112F25 120 CU 035X35#SP 662303518318
2112F26 120 CU 040X35#SP 662303667832
2112F27 120 CU 045X35#SP 662303512729
2112F28 120 CU 1/16X35#SP 662303520380
2116F14 120 CU 5/32X800#DR 662303522377
211EFDD 120 CU 045X35#SP MIL 662303510282
211EFDX 120 CU 045X600#MP MIL 662303522728
240BF07 120 BARE 045X600#MP 662303514945
2118F25 120 CU 035X11#SP 662303521752
2118F27 120 CU 045X11#SP 662303521158

SAW

Accessories

Depositions/Paramaters

Spray Transfer Deposition Table
Diameter Wire Feed Speed Amps Volts Deposition Rate
.023 in, 0.6 mm 400 ipm, 1016 cm/min 100 23 2.7 lbs./hr., 1.2 kg./hr.
450 ipm, 1143 cm/min 106 23 3.1 lbs./hr., 1.4 kg./hr.
500 ipm, 1270 cm/min 111 24 3.4 lbs./hr., 1.6 kg./hr.
550 ipm, 1397 cm/min 117 24 3.8 lbs./hr., 1.7 kg./hr.
600 ipm, 1524 cm/min 122 25 4.1 lbs./hr., 1.9 kg./hr.
630 ipm, 1600 cm/min 125 25 4.3 lbs./hr., 2 kg./hr.
.030 in, 0.8 mm 500 ipm, 1270 cm/min 160 24 5.8 lbs./hr., 2.6 kg./hr.
550 ipm, 1397 cm/min 173 25 6.4 lbs./hr., 2.9 kg./hr.
600 ipm, 1524 cm/min 187 25 7 lbs./hr., 3.2 kg./hr.
650 ipm, 1651 cm/min 200 26 7.6 lbs./hr., 3.4 kg./hr.
.035 in, 0.9 mm 400 ipm, 1016 cm/min 180 25 6.3 lbs./hr., 2.9 kg./hr.
450 ipm, 1143 cm/min 197 26 7.1 lbs./hr., 3.2 kg./hr.
500 ipm, 1270 cm/min 213 26 7.9 lbs./hr., 3.6 kg./hr.
550 ipm, 1397 cm/min 230 27 8.7 lbs./hr., 4 kg./hr.
.045 in, 1.2 mm 300 ipm, 762 cm/min 260 25 7.9 lbs./hr., 3.6 kg./hr.
350 ipm, 889 cm/min 280 26 9.2 lbs./hr., 4.2 kg./hr.
400 ipm, 1016 cm/min 300 28 10.5 lbs./hr., 4.8 kg./hr.
450 ipm, 1143 cm/min 320 29 11.8 lbs./hr., 5.4 kg./hr.
500 ipm, 1270 cm/min 340 30 13.1 lbs./hr., 6 kg./hr.
.052 in, 1.3 mm 265 ipm, 673 cm/min 275 26 9.3 lbs./hr., 4.2 kg./hr.
300 ipm, 762 cm/min 310 28 10.5 lbs./hr., 4.8 kg./hr.
350 ipm, 889 cm/min 360 31 12.2 lbs./hr., 5.6 kg./hr.
390 ipm, 991 cm/min 400 33 13.6 lbs./hr., 6.2 kg./hr.
.062 in, 1.6 mm 180 ipm, 457 cm/min 290 26 9.1 lbs./hr., 4.1 kg./hr.
200 ipm, 508 cm/min 310 28 10.1 lbs./hr., 4.6 kg./hr.
230 ipm, 584 cm/min 340 31 11.6 lbs./hr., 5.3 kg./hr.
260 ipm, 660 cm/min 370 34 13.2 lbs./hr., 6 kg./hr.
280 ipm, 711 cm/min 390 36 14.2 lbs./hr., 6.4 kg./hr.
Shortarc Transfer Deposition Table
Diameter Wire Feed Speed Amps Volts Deposition Rate
.023 in, 0.6 mm 150 ipm, 381 cm/min 45 14 1 lbs./hr., 0.4 kg./hr.
200 ipm, 508 cm/min 55 14 1.3 lbs./hr., 0.6 kg./hr.
250 ipm, 635 cm/min 65 15 1.6 lbs./hr., 0.7 kg./hr.
300 ipm, 762 cm/min 74 15 2 lbs./hr., 0.9 kg./hr.
350 ipm, 889 cm/min 84 16 2.3 lbs./hr., 1 kg./hr.
380 ipm, 965 cm/min 90 16 2.5 lbs./hr., 1.1 kg./hr.
.030 in, 0.8 mm 150 ipm, 381 cm/min 60 14 1.7 lbs./hr., 0.8 kg./hr.
200 ipm, 508 cm/min 80 15 2.2 lbs./hr., 1 kg./hr.
250 ipm, 635 cm/min 100 15 2.8 lbs./hr., 1.3 kg./hr.
300 ipm, 762 cm/min 120 16 3.3 lbs./hr., 1.5 kg./hr.
350 ipm, 889 cm/min 140 16 3.9 lbs./hr., 1.8 kg./hr.
360 ipm, 914 cm/min 144 16 4 lbs./hr., 1.8 kg./hr.
.035 in, 0.9 mm 180 ipm, 457 cm/min 90 15 2.7 lbs./hr., 1.2 kg./hr.
220 ipm, 559 cm/min 113 16 3.3 lbs./hr., 1.5 kg./hr.
260 ipm, 660 cm/min 137 18 4 lbs./hr., 1.8 kg./hr.
300 ipm, 762 cm/min 160 19 4.6 lbs./hr., 2.1 kg./hr.
.045 in, 1.2 mm 125 ipm, 318 cm/min 130 17 3.1 lbs./hr., 1.4 kg./hr.
160 ipm, 406 cm/min 163 18 4 lbs./hr., 1.8 kg./hr.
200 ipm, 508 cm/min 200 19 5 lbs./hr., 2.3 kg./hr.
.052 in, 1.3 mm 135 ipm, 343 cm/min 150 17 4.5 lbs./hr., 2.1 kg./hr.
160 ipm, 406 cm/min 173 18 5.4 lbs./hr., 2.4 kg./hr.
190 ipm, 483 cm/min 200 20 6.4 lbs./hr., 2.9 kg./hr.

Extra Info

Used with OK Flux 10.62