SPOOLARC 100

Spoolarc 100 is a Cr, Ni, Mo alloyed submerged arc welding wire suitable for welding of high strength, low alloy quenched and tempered steels.

Features

Designed for low alloy quenched and tempered steels. Weld metal mechanical properties include high yield strength (exceeds 100 ksi/690 MPa) and low temperature impact toughness. Applications include heat treatable valves and fittings, structural weldments and low temperature pipe valves.

SPOOLARC 100
  • Welding Process
  • SAW (Sub Arc)

Classifications

  • Classifications/Approvals

    • AWS/ASME SFA5.23 EF5

Properties

Typical Properties
Typical Wire Analysis  
C 0.12 %
Mn 1.9 %
Si 0.1 %
P 0.006 %
S 0.006 %
Cr 0.4 %
Ni 2.4 %
Mo 0.5 %
Cu 0.3 %
Wire Chemistries  
C 0.12 %
Mn 1.91 %
Si 0.07 %
P 0.007 %
S 0.006 %
Cr 0.38 %
Ni 2.40 %
Mo 0.50 %
Other Cu 0.32  

Part No.

100
Part No. Model / Product Description UPC
2344F30 100 CU 3/32X65#CL 662303668464
2354F28 100 BARE 1/16X65#CL 662303511784
2354F32 100 BARE 1/8X65#CL 662303511814
2354F34 100 BARE 5/32X65#CL 662303511821
2344F28 100 CU 1/16X65#CL 000000000000
2344F32 100 CU 1/8X65#CL 662303668808
2344F34 100 CU 5/32X65#CL 662303668815

SAW

Accessories

Depositions/Paramaters

Spray Transfer Deposition Table
Diameter Wire Feed Speed Amps Volts Deposition Rate
.023 in, 0.6 mm 400 ipm, 1016 cm/min 100 23 2.7 lbs./hr., 1.2 kg./hr.
450 ipm, 1143 cm/min 106 23 3.1 lbs./hr., 1.4 kg./hr.
500 ipm, 1270 cm/min 111 24 3.4 lbs./hr., 1.5 kg./hr.
550 ipm, 1397 cm/min 117 24 3.8 lbs./hr., 1.7 kg./hr.
600 ipm, 1524 cm/min 122 25 4.1 lbs./hr., 1.8 kg./hr.
630 ipm, 1600 cm/min 125 25 4.3 lbs./hr., 1.9 kg./hr.
.030 in, 0.8 mm 500 ipm, 1270 cm/min 160 25 5.8 lbs./hr., 2 kg./hr.
550 ipm, 1397 cm/min 173 25 6.4 lbs./hr., 2.9 kg./hr.
600 ipm, 1524 cm/min 187 25 7 lbs./hr., 3.1 kg./hr.
650 ipm, 1651 cm/min 200 26 7.6 lbs./hr., 3.4 kg./hr.
.035 in, 0.9 mm 400 ipm, 1016 cm/min 180 26 6.3 lbs./hr., 3.4 kg./hr.
450 ipm, 1143 cm/min 197 26 7.1 lbs./hr., 3.2 kg./hr.
500 ipm, 1270 cm/min 213 26 7.9 lbs./hr., 3.5 kg./hr.
550 ipm, 1397 cm/min 230 27 8.7 lbs./hr., 3.9 kg./hr.
.045 in, 1.2 mm 300 ipm, 762 cm/min 260 27 7.9 lbs./hr., 4 kg./hr.
350 ipm, 889 cm/min 280 26 9.2 lbs./hr., 4.1 kg./hr.
400 ipm, 1016 cm/min 300 27 10.5 lbs./hr., 4.6 kg./hr.
450 ipm, 1143 cm/min 320 29 11.8 lbs./hr., 5.2 kg./hr.
500 ipm, 1270 cm/min 340 30 13.1 lbs./hr., 5.8 kg./hr.
.052 in, 1.3 mm 265 ipm, 673 cm/min 275 30 9.3 lbs./hr., 6 kg./hr.
300 ipm, 762 cm/min 310 27 10.5 lbs./hr., 4.6 kg./hr.
350 ipm, 889 cm/min 360 30 12.2 lbs./hr., 5.4 kg./hr.
390 ipm, 991 cm/min 400 32 13.6 lbs./hr., 6 kg./hr.
.062 in, 1.6 mm 180 ipm, 457 cm/min 290 33 9.1 lbs./hr., 6.2 kg./hr.
200 ipm, 508 cm/min 310 27 10.1 lbs./hr., 4.4 kg./hr.
230 ipm, 584 cm/min 340 30 11.6 lbs./hr., 5.1 kg./hr.
260 ipm, 660 cm/min 370 33 13.2 lbs./hr., 5.8 kg./hr.
280 ipm, 711 cm/min 390 35 14.2 lbs./hr., 6.2 kg./hr.
Shortarc Transfer Deposition Table
Diameter Wire Feed Speed Amps Volts Deposition Rate
.023 in, 0.6 mm 150 ipm, 381 cm/min 45 14 1 lbs./hr., 0.4 kg./hr.
200 ipm, 508 cm/min 55 14 1.3 lbs./hr., 0.6 kg./hr.
250 ipm, 635 cm/min 65 15 1.6 lbs./hr., 0.7 kg./hr.
300 ipm, 762 cm/min 74 15 2 lbs./hr., 0.9 kg./hr.
350 ipm, 889 cm/min 84 16 2.3 lbs./hr., 1 kg./hr.
380 ipm, 965 cm/min 90 16 2.5 lbs./hr., 1.1 kg./hr.
.030 in, 0.8 mm 150 ipm, 381 cm/min 60 14 1.7 lbs./hr., 0.8 kg./hr.
200 ipm, 508 cm/min 80 15 2.2 lbs./hr., 1 kg./hr.
250 ipm, 635 cm/min 100 15 2.8 lbs./hr., 1.3 kg./hr.
300 ipm, 762 cm/min 120 16 3.3 lbs./hr., 1.5 kg./hr.
350 ipm, 889 cm/min 140 16 3.9 lbs./hr., 1.8 kg./hr.
360 ipm, 914 cm/min 144 16 4 lbs./hr., 1.8 kg./hr.
.035 in, 0.9 mm 180 ipm, 457 cm/min 90 15 2.7 lbs./hr., 1.2 kg./hr.
220 ipm, 559 cm/min 113 16 3.3 lbs./hr., 1.5 kg./hr.
260 ipm, 660 cm/min 137 18 4 lbs./hr., 1.8 kg./hr.
300 ipm, 762 cm/min 160 19 4.6 lbs./hr., 2.1 kg./hr.
.045 in, 1.2 mm 125 ipm, 318 cm/min 130 17 3.1 lbs./hr., 1.4 kg./hr.
160 ipm, 406 cm/min 163 18 4 lbs./hr., 1.8 kg./hr.
200 ipm, 508 cm/min 200 19 5 lbs./hr., 2.3 kg./hr.
.052 in, 1.3 mm 135 ipm, 343 cm/min 150 17 4.5 lbs./hr., 2.1 kg./hr.
160 ipm, 406 cm/min 173 18 5.4 lbs./hr., 2.4 kg./hr.
190 ipm, 483 cm/min 200 20 6.4 lbs./hr., 2.9 kg./hr.
1.3 mm 483 cm/min

Extra Info

Used with OK Flux 10.62

Complementary Products

Seismic Data