SPOOLARC 83

Spoolarc 83 contains 0.5% Mo to provide higher deposit strength in both the as-welded and stress-relieved conditions. Spoolarc 83 is typically used on heavy equipment and high strength piping.

Features

Spoolarc 83 contains 0.5% Mo to provide higher deposit strength in both the as welded and stress relieved conditions. It contains high levels of Manganese and Silicon to provide good wetting and good rust and scale tolerance. Spoolarc 83 is also used for all-position welding of high tensile pipe and tubing commonly found in earthmoving and construction equipment. It is available in forms suitable for MIG and TIG welding.

Spoolarc 83
  • Industry
  • General Fabrication
  • Mobile Machinery
  • Automotive
  • Shipbuilding
  • Welding Process
  • GTAW (TIG)
  • GMAW (MIG)
  • SAW (Sub Arc)

Classifications

  • Classifications/Approvals

    • Certified by CWB to CSA W48
    • CAN/CSA-ISO14341,B-G 55A 3 G4M31 (ER80S-3)
    • AWS/ASME SFA5.28; ER80S-D2/ER90S-D2
    • MIL-E-23765/2; 80S-3
    • AWS/ASME SFA5.23; EA3K

Properties

Typical Properties
As Welded 98% Ar / 2% O2 Shielding Gas  
Yield Strength 95 ksi, 655 MPa
Tensile Strength 110 ksi, 750 MPa
Elongation in 2" 22 %
As Welded CO2 Shielding Gas  
Yield Strength 77 ksi, 530 MPa
Tensile Strength 92 ksi, 635 MPa
Elongation in 2" 23 %
Typical Charpy V-Notch Impact Properties  
Testing Temperature -20ºF (-29ºC)  
As Welded CO2 Shielding Gas 44 ft.-lbs., 60 J
As Welded 98% Ar / 2% O2 Shielding Gas 87 ft.-lbs., 118 J
Typical Undiluted Weld Metal Analysis  
As Welded CO2 Shielding Gas  
C 0.08 %
Mn 1.16 %
Si 0.34 %
P 0.008 %
S 0.012 %
Mo 0.39 %
98% Ar / O2 Shielding Gas  
C 0.09 %
Mn 1.65 %
Si 0.60 %
P 0.013 %
S 0.012 %
Mo 0.43 %
Typical Wire Analysis  
C 0.07 %
Mn 1.78 %
Si 0.66 %
P 0.009 %
S 0.008 %
Mo 0.49 %

Part No.

83
Part No. Model / Product Description UPC
126KF34 83 5/32X750#RL 662303669850
1266F94 83 5/32X1000#DR 662303670153
1262F07S 83 045X44#SP 662303670481
1266F15 83 3/16X800#DR 662303085902
1264F30 83 3/32X65#CL 662303669805
126KF35 83 3/16X750#RL 662303669867
126UF65S 83 035X550# OMP 20 2/PLT 662303086732
1264F35 83 3/16X65#CL 662303669881
1264F32 83 1/8X65#CL 662303505820
1266F92 83 1/8X1000#DR 662303670146
126UF61 83 052X550 # OMP 20 2/PLT 662303670702
126UF61S 83 052X550 # OMP 20 2/PLT 662303670498
1262F05S 83 035X44#SP 662303670474
126UF67S 83 045X550 # OMP 20 2/PLT 662303086749
1261F08 83 1/16X36X50#CT 662303505615
1261F10 83 3/32X36X50#CT 662303505622
1261F12 83 1/8X36X50#CT 662303505639
1262F04 83 030X44#SP 662303505660
1262F05 83 035X44#SP 662303505677
1262F07 83 045X44#SP 662303505684
1262F08 83 1/16X44#SP 662303505691
1264F28 83 1/16X65#CL 662303505790
1267F30 83 3/32X36X20#CT F2 662303505998
1268F05 83 035X33#SP 662303506032
1268F07 83 045X33#SP 662303506049
1268F41 83 052X60#SP 662303668662
1268F45 83 035X60#SP 662303506087
1268F47 83 045X60#SP 662303506094
1268F48 83 1/16X60#SP 662303506100
126TF45 83 035X11#SPX44#CT 662303520670
126UF41 83 052X900#OMP 2/PLT 662303668600
126UF45 83 035X900#OMP 2/PLT 662303668594
126UF47 83 045X900#OMP 2/PLT 662303668419
126UF65 83 035X550#OMP 20 2/PLT 662303668198
126UF67 83 045X550#OMP 20 2/PLT 662303668181
126XF47 83 045X900#OMP PBPLT 662303080075
1267F28 83 1/16X36X15#CT F2 662303084561
1267F32 83 1/8X36X30#CT F2 662303506001
126UF48 83 1/16X900#OMP 2/PLT 662303668396

SAW

Accessories

Depositions/Paramaters

Spray Transfer Deposition Table
Diameter Wire Feed Speed Amps Volts Deposition Rate
.023 in, 0.6 mm 400 ipm, 1016 cm/min 100 23 2.7 lbs./hr., 1.2 kg./hr.
450 ipm, 1143 cm/min 106 23 3.1 lbs./hr., 1.4 kg./hr.
500 ipm, 1270 cm/min 111 24 3.4 lbs./hr., 1.6 kg./hr.
550 ipm, 1397 cm/min 117 24 3.8 lbs./hr., 1.7 kg./hr.
600 ipm, 1524 cm/min 122 25 4.1 lbs./hr., 1.9 kg./hr.
630 ipm, 1600 cm/min 125 25 4.3 lbs./hr., 2 kg./hr.
.030 in, 0.8 mm 500 ipm, 1270 cm/min 160 24 5.8 lbs./hr., 2.6 kg./hr.
550 ipm, 1397 cm/min 173 25 6.4 lbs./hr., 2.9 kg./hr.
600 ipm, 1524 cm/min 187 25 7 lbs./hr., 3.2 kg./hr.
650 ipm, 1651 cm/min 200 26 7.6 lbs./hr., 3.4 kg./hr.
.035 in, 0.9 mm 400 ipm, 1016 cm/min 180 25 6.3 lbs./hr., 2.9 kg./hr.
450 ipm, 1143 cm/min 197 26 7.1 lbs./hr., 3.2 kg./hr.
500 ipm, 1270 cm/min 213 26 7.9 lbs./hr., 3.6 kg./hr.
550 ipm, 1397 cm/min 230 27 8.7 lbs./hr., 4 kg./hr.
.045 in, 1.2 mm 300 ipm, 762 cm/min 260 25 7.9 lbs./hr., 3.6 kg./hr.
350 ipm, 889 cm/min 280 26 9.2 lbs./hr., 4.2 kg./hr.
400 ipm, 1016 cm/min 300 28 10.5 lbs./hr., 4.8 kg./hr.
450 ipm, 1143 cm/min 320 29 11.8 lbs./hr., 5.4 kg./hr.
500 ipm, 1270 cm/min 340 30 13.1 lbs./hr., 6 kg./hr.
.052 in, 1.3 mm 265 ipm, 673 cm/min 275 26 9.3 lbs./hr., 4.2 kg./hr.
300 ipm, 762 cm/min 310 28 10.5 lbs./hr., 4.8 kg./hr.
350 ipm, 889 cm/min 360 31 12.2 lbs./hr., 5.6 kg./hr.
390 ipm, 991 cm/min 400 33 13.6 lbs./hr., 6.2 kg./hr.
.062 in, 1.6 mm 180 ipm, 457 cm/min 290 26 9.1 lbs./hr., 4.1 kg./hr.
200 ipm, 508 cm/min 310 28 10.1 lbs./hr., 4.6 kg./hr.
230 ipm, 584 cm/min 340 31 11.6 lbs./hr., 5.3 kg./hr.
260 ipm, 660 cm/min 370 34 13.2 lbs./hr., 6 kg./hr.
280 ipm, 711 cm/min 390 36 14.2 lbs./hr., 6.4 kg./hr.
Shortarc Transfer Deposition Table
Diameter Wire Feed Speed Amps Volts Deposition Rate
.023 in, 0.6 mm 150 ipm, 381 cm/min 45 14 1 lbs./hr., 0.4 kg./hr.
200 ipm, 508 cm/min 55 14 1.3 lbs./hr., 0.6 kg./hr.
250 ipm, 635 cm/min 65 15 1.6 lbs./hr., 0.7 kg./hr.
300 ipm, 762 cm/min 74 15 2 lbs./hr., 0.9 kg./hr.
350 ipm, 889 cm/min 84 16 2.3 lbs./hr., 1 kg./hr.
380 ipm, 965 cm/min 90 16 2.5 lbs./hr., 1.1 kg./hr.
.030 in, 0.8 mm 150 ipm, 381 cm/min 60 14 1.7 lbs./hr., 0.8 kg./hr.
200 ipm, 508 cm/min 80 15 202 lbs./hr., 1 kg./hr.
250 ipm, 635 cm/min 100 15 2.8 lbs./hr., 1.3 kg./hr.
300 ipm, 762 cm/min 120 16 3.3 lbs./hr., 1.5 kg./hr.
350 ipm, 889 cm/min 140 16 3.9 lbs./hr., 1.8 kg./hr.
360 ipm, 914 cm/min 144 16 4 lbs./hr., 1.8 kg./hr.
.035 in, 0.9 mm 180 ipm, 457 cm/min 90 15 2.7 lbs./hr., 1.2 kg./hr.
220 ipm, 559 cm/min 113 16 3.3 lbs./hr., 1.5 kg./hr.
260 ipm, 660 cm/min 137 18 4 lbs./hr., 1.8 kg./hr.
300 ipm, 762 cm/min 160 19 4.6 lbs./hr., 2.1 kg./hr.
.045 in, 1.2 mm 125 ipm, 318 cm/min 130 17 3.1 lbs./hr., 1.4 kg./hr.
160 ipm, 406 cm/min 163 18 4 lbs./hr., 1.8 kg./hr.
200 ipm, 508 cm/min 200 19 5 lbs./hr., 2.3 kg./hr.
.052 in, 1.3 mm 135 ipm, 343 cm/min 150 17 4.5 lbs./hr., 2.1 kg./hr.
160 ipm, 406 cm/min 173 18 5.4 lbs./hr., 2.4 kg./hr.
190 ipm, 483 cm/min 200 20 6.4 lbs./hr., 2.9 kg./hr.
Subarc Deposition Data
Diameter Amps Deposition Rate Efficiency %
1/16 in, 1.6 mm 400 A 13.0 lbs/hr, 5.90 kg/hr 99
500 A 17.0 lbs/hr, 7.71 kg/hr 99
5/64 in, 2.0 mm 300 A 10.8 lbs/hr, 4.90 kg/hr 99
400 A 14.5 lbs/hr, 6.58 kg/hr 99
500 A 18.2 lbs/hr, 8.26 kg/hr 99
3/32 in, 2.4 mm 400 A 13.2 lbs/hr, 5.99 kg/hr 99
500 A 17.0 lbs/hr, 7.71 kg/hr 99
600 A 22.0 lbs/hr, 9.98 kg/hr 99
1/8 in, 3.2 mm 400 A 11.0 lbs/hr, 4.99 kg/hr 99
500 A 14.5 lbs/hr, 6.58 kg/hr 99
600 A 18.0 lbs/hr, 8.16 kg/hr 99
700 A 21.2 lbs/hr, 9.62 kg/hr 99
5/32 in, 4.0 mm 500 A 12.5 lbs/hr, 5.67 kg/hr 99
600 A 16.0 lbs/hr, 7.26 kg/hr 99
700 A 19.5 lbs/hr, 23.2 kg/hr 99
800 A 23.0 lbs/hr, 10.43 kg/hr 99
900 A 26.0 lbs/hr, 11.79 kg/hr 99
3/16 in, 4.8 mm 600 A 13.9 lbs/hr, 6.31 kg/hr 99
700 A 17.5 lbs/hr, 7.94 kg/hr 99
800 A 21.0 lbs/hr, 9.53 kg/hr 99
900 A 25.0 lbs/hr, 11.34 kg/hr 99
1,000 A 29.2 lbs/hr, 13.25 kg/hr 99
1,100 A 34.0 lbs/hr, 15.42 kg/hr 99

Extra Info

Usable with OK Flux 231.