SPOOLARC 40

Spoolarc 40 is a submerged arc wire that is typically used to weld carbon and low alloy steels. It contains 1/2% Mo and elevated levels of Mn which make it suitable for stress relieved applications requiring 80 ksi tensile strength.

Features

Designed for single or multipass wire for welding carbon and low alloy steels. Produces good as welded and stress relieved impact toughness. Weld metal tensile strength is in excess of 80 ksi (552 MPa). Applications include pressure vessel fabrication and other similar welds which require postweld heat treatment.

SPOOLARC 40
  • Welding Process
  • SAW (Sub Arc)

Classifications

  • Classifications/Approvals

    • AWS/ASME SFA5.23 EA3

Properties

Typical Properties
C 0.1 %
Mn 1.0 %
Si 0.2 %
P 0.008 %
S 0.010 %
Typical wire analysis  
C 0.15 %
Mn 2.00 %
Si 0.03 %
P 0.017 %
S 0.015 %
Mo 0.50 %

Part No.

40
Part No. Model / Product Description UPC
1101F12 40 1/8X36 662303502157
1104F30 40 3/32X65#CL 662303502263
1104F32 40 1/8X65#CL 662303502270
1104F34 40 5/32X65#CL 662303502287
1104F35 40 3/16X65#CL 662303502294
1106F14 40 5/32X800#DR 662303502355
1106F55 40 3/16X700#DR 662303502393

SAW

Accessories

Depositions/Paramaters

Spray Transfer Deposition Table
Diameter Amps Deposition Rate Average Deposition Efficiency
1/16 in, 1.6 mm 400 13.0 lbs./hr., 5.90 kg./hr. 99 %
500 17.0 lbs./hr., 7.71 kg./hr. 99 %
5/64 in, 2.0 mm 300 10.8 lbs./hr., 4.90 kg./hr. 99 %
400 14.5 lbs./hr., 6.58 kg./hr. 99 %
500 18.2 lbs./hr., 8.26 kg./hr. 99 %
3/32 in, 2.4 mm 400 13.2 lbs./hr., 5.99 kg./hr. 99 %
500 17.0 lbs./hr., 7.71 kg./hr. 99 %
600 22.0 lbs./hr., 9.98 kg./hr. 99 %
1/8 in, 3.2 mm 400 11.0 lbs./hr., 4.99 kg./hr. 99 %
500 14.5 lbs./hr., 6.58 kg./hr. 99 %
600 18.0 lbs./hr., 8.16 kg./hr. 99 %
700 21.2 lbs./hr., 9.62 kg./hr. 99 %
5/32 in, 4.0 mm 500 12.5 lbs./hr., 5.67 kg./hr. 99 %
600 16.0 lbs./hr., 7.26 kg./hr. 99 %
700 19.5 lbs./hr., 8.85 kg./hr. 99 %
800 23.0 lbs./hr., 10.43 kg./hr. 99 %
900 26.0 lbs./hr., 11.79 kg./hr. 99 %
3/16 in, 4.8 mm 600 13.9 lbs./hr., 6.31 kg./hr. 99 %
700 17.5 lbs./hr., 7.94 kg./hr. 99 %
800 21.0 lbs./hr., 9.53 kg./hr. 99 %
900 25.0 lbs./hr., 11.34 kg./hr. 99 %
1000 29.2 lbs./hr., 13.25 kg./hr. 99 %
1100 34.0 lbs./hr., 15.42 kg./hr. 99 %
Shortarc Transfer Deposition Table
Diameter Wire Feed Speed Amps Volts Deposition Rate
.023 in, 0.6 mm 150 ipm, 381 cm/min 45 14 1 lbs./hr., 0.4 kg./hr.
200 ipm, 508 cm/min 55 14 1.3 lbs./hr., 0.6 kg./hr.
250 ipm, 635 cm/min 65 15 1.6 lbs./hr., 0.7 kg./hr.
300 ipm, 762 cm/min 74 15 2 lbs./hr., 0.9 kg./hr.
350 ipm, 889 cm/min 84 16 2.3 lbs./hr., 1 kg./hr.
380 ipm, 965 cm/min 90 16 2.5 lbs./hr., 1.1 kg./hr.
.030 in, 0.8 mm 150 ipm, 381 cm/min 60 14 1.7 lbs./hr., 0.8 kg./hr.
200 ipm, 508 cm/min 80 15 2.2 lbs./hr., 1 kg./hr.
250 ipm, 635 cm/min 100 15 2.8 lbs./hr., 1.3 kg./hr.
300 ipm, 762 cm/min 120 16 3.3 lbs./hr., 1.5 kg./hr.
350 ipm, 889 cm/min 140 16 3.9 lbs./hr., 1.8 kg./hr.
360 ipm, 914 cm/min 144 16 4 lbs./hr., 1.8 kg./hr.
.035 in, 0.9 mm 180 ipm, 457 cm/min 90 15 2.7 lbs./hr., 1.2 kg./hr.
220 ipm, 559 cm/min 113 16 3.3 lbs./hr., 1.5 kg./hr.
260 ipm, 660 cm/min 137 18 4 lbs./hr., 1.8 kg./hr.
300 ipm, 762 cm/min 160 19 4.6 lbs./hr., 2.1 kg./hr.
.045 in, 1.2 mm 125 ipm, 318 cm/min 130 17 3.1 lbs./hr., 1.4 kg./hr.
160 ipm, 406 cm/min 163 18 4 lbs./hr., 1.8 kg./hr.
200 ipm, 508 cm/min 200 19 5 lbs./hr., 2.3 kg./hr.
.052 in, 1.3 mm 135 ipm, 343 cm/min 150 17 4.5 lbs./hr., 2.1 kg./hr.
190 ipm, 483 cm/min 200 20 6.4 lbs./hr., 2.9 kg./hr.
160 ipm, 406 cm/min 173 18 5.4 lbs./hr., 2.4 kg./hr.

Extra Info

Usable with OK Flux 80.