Print this page

COREWELD C6

Coreweld C-6 is a metal-cored wire designed to provide excellent arc characteristics, high travel speeds and minimal spatter.

Features

Coreweld C6 was developed and “fine-tuned” especially for hand-held, automatic and robotic welding in the automotive industry, as well as rail car manufacturing, structural welding and other similar applications. Never before has there been such a perfect pairing of filler metal and industry requirements for quality, productivity and profitability.

  • Exceptionally high travel speeds, critical for automation

  • Enhanced productivity that makes it more cost-effective than solid wires

  • Improved feedability and arc stability as a result of special lubricants & surface treatment

  • Outstanding deposition efficiencies that can exceed 99% at high travel speeds

  • Ideal for flat or horizontal fillet welds, particularly in automated welding

  • Performs well with Argon/CO2 shielding gas mixes from 75-92% Argon

  • Handles rust and mill scale with good sidewall tie-in and wetting

  • Broad operating parameters with both pulse and CVCC

  • Excellent restart characteristics

  • Very few silicon islands

  • Lower spatter levels

Coreweld C6
  • Industry
  • Mobile Machinery
  • Shipbuilding
  • Automotive
  • Bridge Construction
  • Civil Construction
  • General Fabrication
  • Rail Road Car
  • Welding Process
  • MCAW (Metal Core)

Classifications

  • Classifications/Approvals

    • AWS A5.20: SEISMIC
    • AWS A5.18; E70C-6M
    • A.B.S. - 3SA, 4YSA
    • Certified by CWB to CSA W48
    • ASME SFA 5.18

Properties

Typical Properties
As Welded 75% Ar / 25% CO2  
Yield Strength 74 ksi, 505 MPa
Tensile Strength 86 ksi, 595 MPa
Reduction in Area 64.4 %
Elongation in 2" 27 %
As Welded 92% Ar / 8% CO2  
Yield Strength 79 ksi, 545 MPa
Tensile Strength 86 ksi, 595 MPa
Reduction in Area 63 %
Elongation in 2" 25 %
Typical Charpy V-Notch Impact Properties  
Testing Temperature 0ºF (-18ºC)  
As Welded 75% Ar / 25% CO2 55 ft.-lbs., 75 J
Testing Temperature -20ºF (-29ºC)  
As Welded 75% Ar / 25% CO2 38 ft.-lbs., 52 J
As Welded 92% Ar / 8% CO2 56 ft.-lbs., 76 J
Typical Undiluted Weld Metal Analysis  
75% Ar / 25% CO2  
C 0.04 %
Mn 1.6 %
Si 0.7 %
P 0.012 %
S 0.016 %
92% Ar / 8% CO2  
C 0.04 %
Mn 1.6 %
Si 0.8 %
P 0.015 %
S 0.017 %

Part No.

C6
Part No. Model / Product Description UPC
243411022 CW C6 1/16X60#CL 662303054441
243411113 CW C6 045X500#MP 662303056339
243411121 CW C6 1/16X500#MP 662303054861
243411139 CW C6 052X500#MP 662303064297
243411147 CW C6 045X60#CL 662303067663
243411154 CW C6 052X60#CL 662303068141
243411162 CW C6 052X33#AWS 662303068134
243411170 CW C6 045X600#OMP 662303070526
243411188 CW C6 052X600#OMP 662303070267
243411196 CW C6 1/16X600#OMP 662303070274
243411204 CW C6 045X33#AWS 662303056346
243411220 CW C6 1/16X33#AWS 662303059057

SAW

Accessories

Depositions/Paramaters

Deposition Table
Diameter Amps Volts Wire Feed Speed Deposition Rate Efficiency
0.045 in, 1.2 mm 175 A 26 V 233 ipm, 592 cm/min 6.0 lbs./hr., 2.7 kg./hr. 98.4 %
200 A 27 V 275 ipm, 699 cm/min 7.1 lbs./hr., 3.2 kg./hr. 97.9 %
265 A 28 V 420 ipm, 1067 cm/min 12.6 lbs./hr., 5.7 kg./hr. 97.2 %
330 A 29 V 623 ipm, 1582 cm/min 16.4 lbs./hr., 7.4 kg./hr. 98.5 %
350 A 30 V 680 ipm, 1727 cm/min 18.6 lbs./hr., 8.4 kg./hr. 99.3 %
0.052 in, 1.4 mm 225 A 23 V 200 ipm, 508 cm/min 6.1 lbs./hr., 2.8 kg./hr. 87.9 %
300 A 25 V 300 ipm, 762 cm/min 10.1 lbs./hr., 4.6 kg./hr. 92.1 %
370 A 27 V 400 ipm, 1016 cm/min 13.8 lbs./hr., 6.3 kg./hr. 97.5 %
420 A 29 V 500 ipm, 1270 cm/min 17.3 lbs./hr., 7.8 kg./hr. 99.6 %
500 A 31 V 600 ipm, 1524 cm/min 20.9 lbs./hr., 9.5 kg./hr. 95.3 %
1/16 in, 1.6 mm 270 A 24 V 200 ipm, 508 cm/min 8.7 lbs./hr., 3.9 kg./hr. 92.7 %
350 A 27 V 300 ipm, 762 cm/min 13.9 lbs./hr., 6.3 kg./hr. 97.7 %
440 A 30 V 400 ipm, 1016 cm/min 19.2 lbs./hr., 8.7 kg./hr. 98.6 %
480 A 31 V 500 ipm, 1270 cm/min 23.0 lbs./hr., 10.4 kg./hr. 99.6 %
500 A 33 V 600 ipm, 1524 cm/min 28.0 lbs./hr., 12.7 kg./hr. 99.6 %