Print this page

COREWELD 80C-Ni1

Coreweld 80CNil is a metal cored wire designed for applications where good impact toughness is required.

Features

Coreweld 80C-Ni1 is a metal cored wire for application where good low temperature impact toughness or weathering characteristics are required. It operates over a broad range of parameters, produces a smooth, spray transfer with minimal fume and spatter and is tolerant of light rust and millscale. The shielding gas used should be Ar 75-92% / 25-8% CO2.

Coreweld 80C-Ni1
  • Industry
  • Process
  • General Fabrication
  • Mobile Machinery
  • Bridge Construction
  • Welding Process
  • MCAW (Metal Core)

Classifications

  • Classifications/Approvals

    • ASME SFA 5.28
    • AWS A5.28; E80C-Ni1

Properties

Typical Properties
As Welded 85% Ar / 15% CO2  
Yield Strength 70 ksi, 485 MPa
Tensile Strength 82 ksi, 565 MPa
Reduction in Area 66 %
Elongation in 2" 27 %
Typical Charpy V-Notch Impact Properties  
Testing Temperature 0ºF (-18ºC)  
As Welded 75% Ar / 25% CO2 55 ft.-lbs., 75 J
Testing Temperature -50ºF (-46ºC)  
As Welded 85% Ar / 15% CO2 75 ft.-lbs.
Typical Undiluted Weld Metal Analysis  
85% Ar / 15% CO2  
C 0.04 %
Mn 1.5 %
Si 0.3 %
P 0.010 %
S 0.020 %
Ni 0.9 %

Part No.

80C-Ni1
Part No. Model / Product Description UPC
243417003 CW 80C-NI1 045X33#AWS VP 662303070960
243417011 CW 80C-NI1 052X60#CL 662303073589
243417029 CW 80C-NI1 1/16X60#CL 662303073596
243417037 CW 80C-NI1 052X60#CL WCRT 662303075613
243417045 CW 80C-NI1 1/16X60#CL WCRT 662303075620
243417052 CW 80C-NI1 052X600#OMP 662303076344
243417060 CW 80C-NI1 045X33#AWS BOM 662303080730

SAW

Accessories

Depositions/Paramaters

Extra Info

Coreweld 80C-Ni1 is alloyed with 1% Ni to provide good low temperature impact toughness. It also meets the requirements in AWS D1.1 and D1.5 for use on unpainted weathering steels. It is suitable for making single or multi-pass welds in the flat or horizontal position using conventional (DCEP or DCEN) or pulsed power. Typical applications include bridgecomponents, utility poles, storage tanks, and transportation equipment.

Shielding Gas

Ar 75-92% / 25-8% CO2

Complementary Products

Seismic Data