Print this page

ARCALOY MC309LMo

Arcaloy MC309LMo was developed to maximize welding performance and reduce the cast to deposit. The alloying elements make it ideal for cladding or joining stainless to low alloy steels.

Features

Arcaloy MC309LMo electrode is designed for applications requiring molybdenum with a standard 309L analsyis. It is used primarily for welding type 316L and 316 clad steels, or welding molybdenum-containing austenitic stainless steel to carbon steel, provided the service temperature is less than 600°F(316°C).

* This item is subject to Industry Alloy Surcharges

Arcaloy MC309LMo
  • Industry
  • Petrochemical
  • Power Generation
  • Process
  • Welding Process
  • MCAW (Metal Core)

Classifications

  • Classifications/Approvals

    • ASME SFA 5.9

Properties

Typical Properties
As Welded 98% Ar / 2% CO2  
C 0.03 %
Mn 1.6 %
Si 0.6 %
P 0.018 %
S 0.008 %
Cr 24 %
Ni 13 %
Mo 2.7 %
Cu 0.09 %

Part No.

MC309LMo
Part No. Model / Product Description UPC
258078104 ARC MC309LMO 045X33#PSP VP 662303075217
258078112 ARC MC309LMO 1/16X33#PSP VP 662303075224

SAW

Accessories

Depositions/Paramaters

Deposition Table
Diameter Amps Volts Wire Feed Speed Deposition Rate Efficiency
.045 in, 1.2 mm 144 A 16 160 ipm, 406 cm/min 4.2 lbs./hr., 1.9 kg./hr. 99.3 %
245 A 25 265 ipm, 673 cm/min 7.1 lbs./hr., 3.2 kg./hr. 99.3 %
321 A 26 370 ipm, 939 cm/min 10 lbs./hr., 4.5 kg./hr. 99.4 %
390 A 28 475 ipm, 1206 cm/min 13 lbs./hr., 5.9 kg./hr. 98.5 %
441 A 30 580 ipm, 1473 cm/min 16 lbs./hr., 7.2 kg./hr. 99.2 %
1/16 in, 1.6 mm 212 A 23 145 ipm, 368 cm/min 6.9 lbs./hr., 3.1 kg./hr. 99.2 %
285 A 23 225 ipm, 571 cm/min 10.8 lbs./hr., 4.9 kg./hr. 98.8 %
332 A 26 300 ipm, 762 cm/min 13.7 lbs./hr., 6.2 kg./hr. 98.1 %
420 A 28 380 ipm, 965 cm/min 18.3 lbs./hr., 8.3 kg./hr. 99.5 %
500 A 31 460 ipm, 1168 cm/min 22.5 lbs./hr., 10.22 kg./hr. 98.9 %