Arcaloy MC308L was developed to maximize performance and reduce the cast to deposit. The alloying elements make it ideal for joining 304 or 304L stainless.
Arcaloy MC308L is a composite metal cored stainless steel wire which has a stainless steel sheath. Arcaloy MC308L is used for welding types 301, 302, 304, and 304L. This may be used for welding types 321 and 347 if service temperatures do not exceed 500°F(260°C). Its higher deposition rate and less penetration compared to solid wire makes it very suitable for making butt, fillet and lap welds on gauge material. Higher speeds are also possible compared to solid wire. The low spatter and slag-free welds make this electrode ideal for automatic and robotic welding. The pushing technique can be used to further minimize the penetration and oxide film formed on the surface of the weld. Typical applications include automobile catalytic converters, manifolds, mufflers, exhaust systems. For welding in the spray mode of metal transfer, the shielding gas should be argon with 1 or 2% oxygen or carbon dioxide. Pulse welding can also be used to further minimize penetration in thin gauge steels. This metal cored wire can also be used in submerged arc welding in combination with 10.93 Flux.
* This item is subject to Industry Alloy Surcharges

| As Welded 98% Ar / 2% CO2 | |
|---|---|
| C | 0.025 % |
| Mn | 1.5 % |
| Si | 0.55 % |
| Cr | 20 % |
| Ni | 10 % |
| Mo | 0.1 % |
| Cu | 0.1 % |
| Ferrite | 10 FN |
| Diameter | Amps | Volts | Wire Feed Speed | Deposition Rate | Efficiency |
|---|---|---|---|---|---|
| .045 in, 1.2 mm | 144 A | 16 | 160 ipm, 406 cm/min | 4.2 lbs./hr., 1.9 kg./hr. | 99.3 % |
| 245 A | 25 | 265 ipm, 673 cm/min | 7.1 lbs./hr., 3.2 kg./hr. | 99.3 % | |
| 321 A | 26 | 370 ipm, 939 cm/min | 10 lbs./hr., 4.5 kg./hr. | 99.4 % | |
| 390 A | 28 | 475 ipm, 1206 cm/min | 13 lbs./hr., 5.9 kg./hr. | 98.5 % | |
| 441 A | 30 | 580 ipm, 1473 cm/min | 16 lbs./hr., 7.2 kg./hr. | 99.2 % | |
| 1/16 in, 1.6 mm | 212 A | 23 | 145 ipm, 368 cm/min | 6.9 lbs./hr., 3.1 kg./hr. | 99.2 % |
| 285 A | 23 | 225 ipm, 571 cm/min | 10.8 lbs./hr., 4.9 kg./hr. | 98.8 % | |
| 332 A | 26 | 300 ipm, 762 cm/min | 13.7 lbs./hr., 6.2 kg./hr. | 98.1 % | |
| 420 A | 28 | 380 ipm, 965 cm/min | 18.3 lbs./hr., 8.3 kg./hr. | 99.5 % | |
| 500 A | 31 | 460 ipm, 1168 cm/min | 22.5 lbs./hr., 10.22 kg./hr. | 98.9 % |
98%Ar / 2%CO2
All listed prices are in U.S. dollars and represent the Manufacturer's Suggested Retail Price (MSRP) for sale in the United States. Actual selling price will be determined by the Distributor. Prices are subject to change without notice.