ARCALOY 409Cb

Arcaloy 409Cb is a ferritic metal cored wire developed for welding similar ferritic steels requiring 11-12% Cr. The addition of Niobium (Nb) or Columbium (Cb) helps optimize weld metal transfer.

Features

Arcaloy 409Cb is a 12% Cr alloy metal cored electrode stabilized with niobium (Nb) for arc stability, to improve corrosion resistance, and to increase strength at high temperatures. It was designed for welding stainless steel catalytic converters, manifolds, mufflers, and exhaust systems. It is also suited for welding parts with poor fit up. Arcaloy 409Cb produces a spray-type metal transfer with very minimal spatter.

* This item is subject to Industry Alloy Surcharges

409Cb
  • Industry
  • Automotive
  • Welding Process
  • MCAW (Metal Core)

Classifications

  • Classifications/Approvals

    • ASME SFA 5.9

Properties

Typical Properties
98% Ar / 2% O2  
C .019 %
Mn 0.5 %
Si 0.53 %
P .013 %
S .023 %
Cr 11.5 %
Nb .52 %

Part No.

409Cb
Part No. Model / Product Description UPC
258080159 ARC 409CB 045X500#MP 662303039233
258080167 ARC 409CB 045X600#OMP 662303069827
258080175 ARC 409CB 052X600#OMP 662303071615
258080191 ARC 409CB 045X250#OMP 8/PLT 662303071523
258080100 ARC 409CB 040X33#PSP 662303073640
258080142 ARC 409CB 045X44#FSP 662303039226

SAW

Accessories

Depositions/Paramaters

Deposition Table
Diameter Amps Volts Wire Feed Speed Electrical Stickout
0.045 in, 1.2 mm 200 A 20 210 ipm, 533 cm/min 0.5 inches, 12.7 mm
215 A 21 230 ipm, 584 cm/min 0.5 inches, 12.7 mm
234 A 22 250 ipm, 635 cm/min 0.5 inches, 12.7 mm
290 A 24 300 ipm, 762 cm/min 0.5 inches, 12.7 mm
323 A 24 350 ipm, 889 cm/min 0.5 inches, 12.7 mm

Extra Info

Shielding Gas

98% Argon / 2% Oxygen