ARCALOY 439Ti

Arcaloy 439Ti is a ferritic metal cored wire developed for welding similar ferritic steels requiring 16-17% Cr. The addition of Titanium (Ti) optimizes weld metal transfer.

Features

Arcaloy 439Ti is an 16-17% Cr alloy metal cored electrode stabilized with Titanium (Ti). The high level of chromium provides additional oxidation and corrosion resistance when welding stainless steel catalytic converters, manifolds, mufflers, and exhaust systems. It is also suited for welding parts with poor fit up. Arcaloy 439Ti produces a spray - type metal transfer with minimal spatter.

* This item is subject to Industry Alloy Surcharges

439Ti
  • Industry
  • Automotive

Classifications

  • Classifications/Approvals

    • AWS A5.9; EC439
    • ASME SFA 5.9

Properties

Typical Properties
98% Ar / 2% O2  
C .024 %
Mn .78 %
Si .51 %
P .007 %
S .018 %
Cr 18.0 %
Ti .50 %

Part No.

439Ti
Part No. Model / Product Description UPC
258045533 ARC 439TI 045X500#MP 2/PIGBK 662303037635
258045541 ARC 439TI 045X600#OMP 662303069841
258045525 ARC 439TI 045X44#FSP 662303008543
258045574 ARC 439TI 045X250#OMP 8/PLT 662303075361
258045582 ARC 439TI 052X33#PSP 662303078782
258045590 ARC 439TI 052X250#OMP 8/PLT 662303080129

SAW

Accessories

Depositions/Paramaters

Deposition Table
Diameter Amps Volts Wire Feed Speed Electrical Stickout
.045 in, 1.2 mm 200 A A 20 210 ipm, 533 cm/min 5 inches, 12.7 mm
215 A A 21 230 ipm, 584 cm/min 0.5 inches, 12.7 mm
234 A A 22 250 ipm, 635 cm/min 0.5 inches, 12.7 mm
290 A A 24 300 ipm, 762 cm/min 0.5 inches, 12.7 mm
323 A A 24 350 ipm, 889 cm/min 0.5 inches, 12.7 mm

Extra Info

Shielding Gas

98% Argon / 2% Oxygen