ARCALOY MC410NiMo

Arcaloy MC410NiMo is a martensitic metal cored wire for weld type CA-6NM castings to maximize welding performance and reduce the cast to deposit.

Features

Arcaloy 410NiMo is a low carbon electrode that produces hardness of 21Rc after stress relieving.


* This item is subject to Industry Alloy Surcharges

MC410NiMo
  • Industry
  • Petrochemical
  • Power Generation
  • Process
  • Welding Process
  • MCAW (Metal Core)

Classifications

  • Classifications/Approvals

    • ASME SFA 5.9
    • AWS A5.9; EC410NiMo

Properties

Typical Properties
As Welded 98% Ar / 2% O2  
Stress Relieved 8 hrs. @ 1110ºF (600ºC)  
Tensile Strength 117 ksi, 805 MPa
Yield Strength 95 ksi, 655 MPa
Elongation in 2" 19 %
Charpy V-Notch Impact Properties  
Testing Temperature 32ºF (0ºC) 35 ft.-lbs., 47 J
Hardness 21 Rc
Typical Weld Metal Analysis  
As Welded 98% Ar / 2% CO2  
C .015 %
Mn 0.5 %
Si 0.3 %
P .012 %
S .010 %
Cr 11.5 %
Ni 4.2 %
Mo 0.5 %

Part No.

MC410NiMo
Part No. Model / Product Description UPC
258088202 ARC MC410NIMO 045X33#PSP VP 662303053079

SAW

Accessories

Depositions/Paramaters

Deposition Table
Diameter Amps Volts Wire Feed Speed Deposition Rate Efficiency
.045 in, 1.2 mm 144 A 16 160 ipm, 406 cm/min 4.2 lbs./hr., 1.9 kg./hr. 99.3 %
245 A 25 265 ipm, 673 cm/min 7.1 lbs./hr., 3.2 kg./hr. 99.3 %
321 A 26 370 ipm, 939 cm/min 10 lbs./hr., 4.5 kg./hr. 99.4 %
390 A 28 475 ipm, 1206 cm/min 13 lbs./hr., 5.9 kg./hr. 98.5 %
441 A 30 580 ipm, 1473 cm/min 16 lbs./hr., 7.2 kg./hr. 99.2 %
1/16 in, 1.6 mm 212 A 23 145 ipm, 368 cm/min 6.9 lbs./hr., 3.1 kg./hr. 99.2 %
285 A 23 225 ipm, 571 cm/min 10.8 lbs./hr., 4.9 kg./hr. 98.8 %
332 A 26 300 ipm, 762 cm/min 13.7 lbs./hr., 6.2 kg./hr. 98.1 %
420 A 28 380 ipm, 965 cm/min 18.3 lbs./hr., 8.3 kg./hr. 99.5 %
500 A 31 460 ipm, 1168 cm/min 22.5 lbs./hr., 10.22 kg./hr. 98.9 %