ARCALOY MC410

Arcaloy MC410 is a Martensitic metal cored wire for welding similar martensitic steels. Developed to maximize welding performance and reduce the cast to deposit.

Features

Arcaloy MC410 is recommended for welding type 410 straight chromium steel. This alloy is used extensively for corrosion and oxidation resistance at elevated temperatures up to 1200°F(649°C) as well as resistance to stress corrosion cracking at ambient temperatures.


* This item is subject to Industry Alloy Surcharges

ARCALOY MC410
  • Industry
  • Power Generation
  • Process
  • Petrochemical
  • Welding Process
  • MCAW (Metal Core)

Classifications

  • Classifications/Approvals

    • AWS A5.9; EC410
    • ASME SFA 5.9

Properties

Typical Properties
As welded 98% Ar / 2% O2  
C 0.087 %
Mn 0.50 %
Si 0.44 %
P 0.013 %
S 0.022 %
Cr 13.2 %
Ni 0.009 %
Mo 0.017 %
Cu 0.010 %

Part No.

MC410
Part No. Model / Product Description UPC
258076116 ARC MC410 1/16X33#PSP 662303080266
258076108 ARC MC410 045X33#PSP 662303054502

SAW

Accessories

Depositions/Paramaters

Deposition Table
Diameter Amps Volts Wire Feed Speed Deposition Rate Efficiency
.045 in, 1.2 mm 144 A A 16 160 ipm, 406 cm/min 4.2 lbs./hr., 1.9 kg./hr. 99.3 %
245 A A 25 265 ipm, 673 cm/min 7.1 lbs./hr., 3.2 kg./hr. 99.3 %
321 A A 26 370 ipm, 939 cm/min 10 lbs./hr., 4.5 kg./hr. 99.4 %
390 A A 28 475 ipm, 1206 cm/min 13 lbs./hr., 5.9 kg./hr. 98.5 %
441 A A 30 580 ipm, 1473 cm/min 16 lbs./hr., 7.2 kg./hr. 99.2 %
1/16 in, 1.6 mm 212 A A 23 145 ipm, 368 cm/min 6.9 lbs./hr., 3.1 kg./hr. 99.2 %
285 A A 23 225 ipm, 571 cm/min 10.8 lbs./hr., 4.9 kg./hr. 98.8 %
332 A A 26 300 ipm, 762 cm/min 13.7 lbs./hr., 6.2 kg./hr. 98.1 %
420 A A 28 380 ipm, 965 cm/min 18.3 lbs./hr., 8.3 kg./hr. 99.5 %
500 A A 31 460 ipm, 1168 cm/min 22.5 lbs./hr., 10.22 kg./hr. 98.9 %

Extra Info

Shielding Gas

98% Argon / 2% O2