DUAL SHIELD T-75

Dual Shield T-75 is a flux cored wire with a basic slag system designed for multiple pass welding and produces excellent properties in both the as welded and stress relieved conditions.

Features

Dual Shield T-75 is a flux cored wire with a basic slag system designed for multiple pass welding and produces excellent properties in both the as welded and stress relieved conditions. The exceptional impact toughness and low sensitivity to cracking makes it an ideal choice for a variety of low and medium carbon steels. The arc characteristics are globular, but can be improved with argon gas mixtures. The weld metal analysis is similar to an E7018 low hydrogen electrode.

DUAL SHIELD T-75
  • Industry
  • General Fabrication
  • Rail Road Car
  • Mobile Machinery
  • Civil Construction
  • Welding Process
  • FCAW (Flux Core)

Classifications

  • Classifications/Approvals

    • QPL-24403/1; MIL-70T-5M (.045", 1/16", 5/64", 7/64")
    • AWS A5.20; E71T-5CJH4/T-5MJH4 (.045", 1/16")
    • AWS A5.20; E70T-5CJH4 (3/32", 5/64", 7/64")
    • A.B.S.-3YSA (3/32", 7/64")
    • L.R.-3S,3YS(H15) (3/32", 7/64")
    • D.N.V.-III YMS (3/32", 7/64")
    • ASME SFA 5.20
    • QPL-24403/1; MIL-70T-5C (3/32")

Properties

Typical Properties
As Welded 75% Ar / 25% CO<sub>2</sub>  
Yield Strength 73 ksi, 505 MPa
Tensile Strength 86 ksi, 595 MPa
Reduction in Area 66 %
Elongation in 2" 29 %
As Welded CO2  
Yield Strength 72 ksi, 495 MPa
Tensile Strength 82 ksi, 565 MPa
Reduction in Area 65 %
Elongation in 2" 28 %
Typical Charpy V-Notch Impact Properties  
Testing Temperature -40ºF (-40ºC)  
As Welded 75% Ar / 25% CO2 55 ft.-lbs., 75 J
As Welded CO2 70 ft.-lbs., 95 J
Typical Undiluted Weld Metal Analysis  
CO2  
C 0.04 %
Mn 1.5 %
Si 0.6 %
P 0.006 %
S 0.010 %
75% Ar / 25% CO2  
C 0.04 %
Mn 1.7 %
Si 0.7 %
P 0.004 %
S 0.011 %

Part No.

T-75
Part No. Model / Product Description UPC
243003878 DS T-75 3/32X500#POP 662303077785
243006004 DS T-75 3/32X60#CL 662303002152
245020128 DS T-75 045X33#AWS 662303005924
245020417 DS T-75 1/16X60#CL 662303006068
245020425 DS T-75 5/64X60#CL 662303059958
245020433 DS T-75 5/64X500#POP 662303078461
245020441 DS T-75 1/16X600#OMP 662303080228

SAW

Accessories

Depositions/Paramaters

Deposition Table
Diameter Amps Volts Wire Feed Speed Deposition Rate Efficiency Electrical Stickout
.045 in, 1.2 mm 170 A 19 285 ipm, 724 cm/min 7 lbs./hr., 3.2 kg./hr. 96 % 3/4 inches, 19.1 mm
250 A 30 469 ipm, 1191 cm/min 10.8 lbs./hr., 4.9 kg./hr. 91 % 1 inches, 25.4 mm
300 A 32 606 ipm, 1539 cm/min 14.2 lbs./hr., 6.44 kg./hr. 92 % 1 inches, 25.4 mm
350 A 32 740 ipm, 1880 cm/min 17.5 lbs./hr., 7.94 kg./hr. 93 % 1 inches, 25.4 mm
1/16 in, 1.6 mm 300 A 30 226 ipm, 574 cm/min 9.8 lbs./hr., 4.45 kg./hr. 92 % 1 inches, 25.4 mm
400 A 32 369 ipm, 937 cm/min 16.1 lbs./hr., 7.3 kg./hr. 92 % 1 inches, 25.4 mm
450 A 32 422 ipm, 1072 cm/min 18.5 lbs./hr., 8.4 kg./hr. 93 % 1 inches, 25.4 mm
3/32 in, 2.4 mm 450 A 32 217 ipm, 551 cm/min 17.6 lbs./hr., 8 kg./hr. 85 % 1 inches, 25.4 mm
475 A 32 245 ipm, 622 cm/min 20 lbs./hr., 9.1 kg./hr. 87 % 1 inches, 25.4 mm
500 A 32 270 ipm, 686 cm/min 22.8 lbs./hr., 10.3 kg./hr. 89 % 1 inches, 25.4 mm
550 A 33 346 ipm, 879 cm/min 29.6 lbs./hr., 13.4 kg./hr. 91 % 1 inches, 25.4 mm

Extra Info

Shielding Gas

CO2 for 3/32 and 7/64 (2.4 and 2.8 mm); 75% Argon/25% CO2 for .045 and 1/16 (1.2 and 1.6 mm)