Print this page

DUAL SHIELD 7100 LC

Dual Shield 7100 LC is an all-position flux-cored wire for general
purpose welding. It is tested and certified to meet the new AWS A5.20 ‘D’ designation requirements, making this gas-shielded wire an excellent choice for demand critical welds when FEMA 353, D1.1 or D1.8 Seismic Supplement is utilized.

Features

Dual Shield 7100 LC provides outstanding operator appeal with its easily controlled arc, improved operation at lower current levels, minimal spatter and easily removed slag. Dual Shield 7100 LC can be used with CO2 or 75% Ar – 25% CO2 shielding, however pure CO2 is recommended in applications where restraint is high.

Please see Related Links on the right side of this page to download the Seismic Data Sheet and Seismic Certifications.

DUAL SHIELD 7100 LC
  • Industry
  • Mobile Machinery
  • Process
  • Rail Road Car
  • Shipbuilding
  • Civil Construction
  • General Fabrication
  • Bridge Construction
  • Welding Process
  • FCAW (Flux Core)

Classifications

  • Classifications/Approvals

    • Seismic Certified "D"
    • AWS A5.20; E71T-1CH8/T-1M/T-9CH8/T-9M
    • D.N.V.- III YMS(H10)
    • A.B.S.- 3SA,3YSA(H10)
    • L.R.- 3S,3YS(H10)
    • CERTIFIED BY C.W.B.- CSA W48
    • ASME SFA 5.20

Properties

Typical Properties
As Welded CO2  
Yield Strength 79 ksi, 545 MPa
Tensile Strength 89 ksi, 615 MPa
Reduction in Area 52 %
Elongation in 2" 23 %
As Welded using 75% Ar - 25% CO2  
Yield Strength 93 ksi, 640 MPa
Tensile Strength 96 ksi, 660 MPa
Reduction in Area 56 %
Elongation in 2" 25 %
Typical Charpy V-Notch Impact Properties  
Testing Temperature 0°F (-18°C)  
As Welded CO2 68 ft - lb, 92 J
As Welded 75% Ar - 25% CO2 50 ft - lb, 61 J
Testing Temperature -20°F (-29°C)  
As Welded CO2 41 ft - lb, 56 J
As Welded 75% Ar - 25% CO2 41 ft - lb, 56 J
Typical Undiluted Weld Metal Analysis  
CO2  
C 0.03 %
Mn 1.4 %
Si 0.5 %
P 0.010 %
Si 0.010 %
75% Ar / 25% CO2  
C 0.03 %
Mn 1.6 %
Si 0.6 %
P 0.010 %
Si 0.010 %

Part No.

7100 LC
Part No. Model / Product Description UPC
248000879 DS 7100 LC 1/16X33#AWS VP FEMA 662303076528
248000895 DS 7100 LC 045X60#CL 662303059118
248000903 DS 7100 LC 1/16X33#AWS 662303046057
248000911 DS 7100 LC 045X10#PSP 662303046262
248000929 DS 7100 LC 1/16X60#CL 662303046392
248000937 DS 7100 LC 045X33#AWS 662303048075
248000945 DS 7100 LC 1/16X60#CL BK 662303048099
248000960 DS 7100 LC 052X33#AWS 662303048334
248000978 DS 7100 LC 1/16X33#AWS BK 662303048389
248000986 DS 7100 LC 1/16X500#MP 662303049270
248000994 DS 7100 LC 1/16X600#WR 662303049508
248001018 DS 7100 LC 052X10#PSP 662303049652
248001026 DS 7100 LC 045X15#PSP 662303053208
248001034 DS 7100 LC 052X500#MP 662303058821
248001042 DS 7100 LC 052X60#CL 662303059125
248001059 DS 7100 LC 045X500#MP 662303059156
248001083 DS 7100 LC 1/16X600#OMP 662303076160
248001091 DS 7100 LC 052X15#PSP 662303076306
248001109 DS 7100 LC 1/16X15#PSP 662303076313
248001117 DS 7100 LC 045X600#OMP 662303078546
248001125 DS 7100 LC 052X600#OMP 662303078553

SAW

Accessories

Depositions/Paramaters

Deposition Data
Diameter Wire Feed Speed Amps Volts Shielding Gas TTW Dist Deposition Rate Efficiency
0.045 in, 1.2 mm 200 ipm, 508 cm/min 145 A 24.5 V CO2 0.625 in. 3.6 lbs./hr., 1.6 kg./hr. 81.2 %
300 ipm, 762 cm/min 190 A 26 V CO2 0.625 in. 5.4 lbs./hr., 2.5 kg./hr. 81.4 %
400 ipm, 1016 cm/min 235 A 27.5 V CO2 0.625 in. 7.3 lbs./hr., 3.3 kg./hr. 82.5 %
500 ipm, 1270 cm/min 265 A 29 V CO2 0.625 in. 9.3 lbs./hr., 4.2 kg./hr. 82.8 %
600 ipm, 1524 cm/min 305 A 30 V CO2 0.625 in. 11.3 lbs./hr., 5.1 kg./hr. 83.7 %
0.052 in, 1.3 mm 150 ipm, 381 cm/min 145 A 25 V CO2 0.75 in. 3.4 lbs./hr., 1.5 kg./hr. 74.3 %
200 ipm, 508 cm/min 180 A 25.5 V CO2 0.75 in. 4.5 lbs./hr., 2.0 kg./hr. 74.6 %
300 ipm, 762 cm/min 235 A 27.5 V CO2 0.75 in. 7.0 lbs./hr., 3.2 kg./hr. 78.2 %
400 ipm, 1016 cm/min 285 A 28.5 V CO2 0.75 in. 9.8 lbs./hr., 4.4 kg./hr. 81.3 %
500 ipm, 1270 cm/min 230 A 29.5 V CO2 0.75 in. 12.2 lbs./hr., 5.5 kg./hr. 82.3 %
600 ipm, 1524 cm/min 370 A 30.2 V CO2 0.75 in. 14.7 lbs./hr., 6.7 kg./hr. 82.7 %
0.062 in, 1.6 mm 150 ipm, 381 cm/min 195 A 24.5 V CO2 0.75 in. 4.5 lbs./hr., 2.0 kg./hr. 73.7 %
250 ipm, 635 cm/min 285 A 26 V CO2 0.75 in. 8.1 lbs./hr., 3.7 kg./hr. 79.4 %
300 ipm, 762 cm/min 320 A 28 V CO2 0.75 in. 9.7 lbs./hr., 4.4 kg./hr. 79.9 %
350 ipm, 889 cm/min 345 A 30 V CO2 0.75 in. 11.5 lbs./hr., 5.2 kg./hr. 80.7 %
400 ipm, 1016 cm/min 385 A 32 V CO2 0.75 in. 13.4 lbs./hr., 6.1 kg./hr. 82.6 %
500 ipm, 1270 cm/min 445 A 32.5 V CO2 0.75 in. 16.7 lbs./hr., 7.6 kg./hr. 82.8 %

Extra Info

Shielding Gas

CO2 or Argon/CO2 mixtures up to 75% Ar