Dual Shield FC-717 is an all-position flux cored wire.
Dual Shield FC-717 is an all-position flux cored wire. The unique slag system makes it suitable for either 75% Argon/25% CO2 or CO2. The performance characteristics produce low spatter, smooth stable arc and flat to convex bead shape. The wide operating parameters make it suitable for a variety of material thicknesses. Dual Shield FC-717 is designed to weld mild and medium carbon steels. This wire is suitable for structural steel fabrication, storage tank construction, and earth moving and material handling equipment.

| As Welded 75% Ar / 25% CO<sub>2</sub> | |
|---|---|
| Yield Strength | 86 ksi, 590 MPa |
| Tensile Strength | 95 ksi, 655 MPa |
| Elongation in 2" | 24 % |
| As Welded CO2 | |
| Yield Strength | 76 ksi, 525 MPa |
| Tensile Strength | 84 ksi, 580 MPa |
| Elongation in 2" | 27 % |
| Typical Charpy V-Notch Impact Properties | |
| Testing Temperature 0ºF (-18ºC) | |
| As Welded CO2 | 50 ft.-lbs., 68 J |
| As Welded 75% Ar / 25% CO2 | 70 ft.-lbs., 95 J |
| Testing Temperature -20ºF (-29ºC) | |
| As Welded CO2 | 30 ft.-lbs., 41 J |
| As Welded 75% Ar / 25% CO2 | 50 ft.-lbs., 68 J |
| Typical Undiluted Weld Metal Analysis | |
| CO2 | |
| C | 0.03 % |
| Mn | 1.0 % |
| Si | 0.5 % |
| P | 0.007 % |
| S | 0.008 % |
| 75% Ar / 25% CO2 | |
| C | 0.03 % |
| Mn | 1.3 % |
| Si | 0.7 % |
| P | 0.007 % |
| S | 0.008 % |
| Part No. | Model / Product Description | UPC |
|---|---|---|
| 249930967 | DS FC-717 052X60#CL | 662303010737 |
| 249930975 | DS FC-717 045X60#CL | 662303010744 |
| 249930983 | DS FC-717 1/16X60#CL | 662303010751 |
| 249930991 | DS FC-717 052X33#AWS | 662303010768 |
| 249931007 | DS FC-717 045X33#AWS | 662303010775 |
| 249931015 | DS FC-717 1/16X33#AWS | 662303010782 |
| 249931114 | DS FC-717 045X33#AWS BK | 662303048952 |
| 249934522 | DS FC-717 1/16X500#MP | 662303011802 |
| 249934548 | DS FC-717 045X500#MP | 662303011826 |
| 249931122 | DS FC-717 1/16X600#OMP | 662303079123 |
| 249931130 | DS FC-717 045X600#OMP | 662303079253 |
| Diameter | Wire Feed Speed | Amps | Volts | Shielding Gas | TTW Dist. | Deposition Rate | Efficiency |
|---|---|---|---|---|---|---|---|
| 0.045 in., 1.2 mm | 200 ipm, 508 cm/min | 150 A | 25 V | CO2 | 0.625 in. | 3.4 lb/hr, 1.5 kg/hr | 69.6 % |
| 300 ipm, 762 cm/min | 205 A | 26.5 V | CO2 | 0.625 in. | 5.8 lb/hr, 2.6 kg/hr | 78.9 % | |
| 400 ipm, 1016 cm/min | 255 A | 27.5 V | CO2 | 0.625 in. | 8.0 lb/hr, 3.6 kg/hr | 79.6 % | |
| 500 ipm, 1270 cm/min | 290 A | 29 V | CO2 | 0.625 in. | 10.1 lb/hr, 4.6 kg/hr | 83.6 % | |
| 600 ipm, 1524 cm/min | 327 A | 30.5 V | CO2 | 0.625 in. | 12.4 lb/hr, 5.6 kg/hr | 85.4 % | |
| 0.052 in., 1.3 mm | 150 ipm, 381 cm/min | 145 A | 25 V | CO2 | 0.75 in. | 3.4 lb/hr, 1.6 kg/hr | 74.5 % |
| 200 ipm, 508 cm/min | 185 A | 26 V | CO2 | 0.75 in. | 4.9 lb/hr, 2.2 kg/hr | 78.7 % | |
| 300 ipm, 762 cm/min | 245 A | 27.5 V | CO2 | 0.75 in. | 7.7 lb/hr, 3.5 kg/hr | 81.7 % | |
| 400 ipm, 1016 cm/min | 300 A | 29 V | CO2 | 0.75 in. | 10.2 lb/hr, 4.6 kg/hr | 83.1 % | |
| 500 ipm, 1270 cm/min | 340 A | 31.5 V | CO2 | 0.75 in. | 13.3 lb/hr, 6.0 kg/hr | 84.3 % | |
| 600 ipm, 1524 cm/min | 385 A | 32 V | CO2 | 0.75 in. | 16.0 lb/hr, 7.3 kg/hr | 86.9 % | |
| 0.062 in., 1.6 mm | 150 ipm, 381 cm/min | 200 A | 24.5 V | CO2 | 0.75 in. | 5.2 lb/hr, 2.4 kg/hr | 82.2 % |
| 250 ipm, 635 cm/min | 290 A | 26 V | CO2 | 0.75 in. | 8.9 lb/hr, 4.0 kg/hr | 85.0 % | |
| 300 ipm, 762 cm/min | 337 A | 26.5 V | CO2 | 0.75 in. | 10.8 lb/hr, 4.9 kg/hr | 85.9 % | |
| 350 ipm, 889 cm/min | 365 A | 27.5 V | CO2 | 0.75 in. | 13.1 lb/hr, 5.9 kg/hr | 87.3 % | |
| 400 ipm, 1016 cm/min | 400 A | 28 V | CO2 | 0.75 in. | 14.3 lb/hr, 6.5 kg/hr | 87.9 % | |
| 500 ipm, 1270 cm/min | 460 A | 29.5 V | CO2 | 0.75 in. | 18.8 lb/hr, 8.5 kg/hr | 89.3 % |