Print this page

DUAL SHIELD II 70 Ultra

Dual Shield II 70 Ultra is an all-position flux cored wire that displays exceptional impact properties in both as-welded and stress-relieved conditions.

Features

Dual Shield II 70 Ultra is an all-position flux cored wire that displays exceptional impact properties when used with 75% Ar/25% CO2. The improved properties qualify this wire to the Navy's "HY" classification. The "Ultra" series produces smoother arc characteristics and lower welding fumes. Dual Shield II 70 Ultra was developed to join low and medium carbon steel. The Military classification allows Dual Shield II 70 Ultra to be used for attaching steels of less than 81 ksi (560 MPa) yield to HY-80 and HY-100. Commercial applications include construction, shipbuilding, railcar, and heavy equipment industries.

Dual Shield II 70 Ultra
  • Industry
  • Rail Road Car
  • Bridge Construction
  • Mobile Machinery
  • Civil Construction
  • Shipbuilding
  • General Fabrication
  • Welding Process
  • FCAW (Flux Core)

Classifications

  • Classifications/Approvals

    • AWS A5.20; E71T-1M/T-12M
    • L.R.- 3S,3YS(H10)
    • QPL-24403/1; MIL-71T-1-HYM
    • QPL-24403/1; MIL-71T-1M
    • A.B.S.- 3SA,3YSA(H5)
    • CERTIFIED BY C.W.B.- CSA W48
    • G.L.- 3YH10S
    • B.V.- SA3YM(HH)
    • D.N.V.- III YMS(H10)
    • ASME SFA 5.20
    • DEUTSCHE BAHN
    • CONTROLAS
    • TUV

Properties

Typical Properties
As Welded 75% Ar / 25% CO2  
Yield Strength 72 ksi, 490 MPa
Tensile Strength 81 ksi, 560 MPa
Reduction in Area 75 %
Elongation in 2" 29 %
Typical Charpy V-Notch Impact Properties  
Testing Temperature 0ºF (-18ºC)  
As Welded 75% Ar / 25% CO2 117 ft.-lbs., 159 J
Testing Temperature -20ºF (-29ºC)  
As Welded 75% Ar / 25% CO2 70 ft.-lbs., 95 J
Typical Undiluted Weld Metal Analysis  
75% Ar / 25% CO2  
C 0.04 %
Mn 1.0 %
Si 0.4 %
P 0.008 %
S 0.009 %

Part No.

II 70 Ultra
Part No. Model / Product Description UPC
245013313 DS II 70 ULT 045X33#PSP 662303004491
245013321 DS II 70 ULT 052X33#PSP 662303004507
245013339 DS II 70 ULT 1/16X33#PSP 662303004514
245013339-03 DS II 70 ULT 1/16X33#PSP 662303077518
245013354 DS II 70 ULT 1/16X60#CL 662303004521
245013362 DS II 70 ULT 1/16X10#PSP 662303004538
245013362-03 DS II 70 ULT 1/16X10#PSP 662303077525
245013370 DS II 70 ULT 045X10#PSP 662303004545
245013370-23 DS II 70 ULT 045X10#PSP 662303055608
245013388 DS II 70 ULT 045X60#CL 662303004552
245013396 DS II 70 ULT 052X10#PSP 662303004569
245013396-03 DS II 70 ULT 052X10#PSP 662303059668
245013453 DS II 70 ULT 045X33#PSP VP 662303004613
245013479 DS II 70 ULT 1/16X33#PSP VP 662303004637
245013743 DS II 70 ULT 035X10#PSP 662303004880
245013750 DS II 70 ULT 035X33#PSP 662303004897
245014493 DS II 70 ULT 1/16X10#FR HS 662303005337
245014519 DS II 70 ULT 1/16X25#FR HS 662303005351
245014600-34 DS II 70 ULT 045X25#FR HS 662303057374
245014618 DS II 70 ULT 045X10#FR HS 662303005436
245014626 DS II 70 ULT 035X10#FR HS 662303005443
245014709 DS II 70 ULT 045X15#PSP 662303005511
245014857 DS II 70 ULT 052X15#PSP 662303005641
245015821-05 DS II 70 ULT 045X10PSP 1/CT/60 662303073817
245013404 DS II 70 ULT 052X60#CL 662303004576
245014758 DS II 70 ULT 045X25#FR VP  
245014808 DS II 70 ULT 1/16X15#PSP 662303005597
245014808-03 DS II 70 ULT 1/16X15#PSP 662303081638
245014857-03 DS II 70 ULT 052X15#PSP 662303081621

SAW

Accessories

Depositions/Paramaters

Deposition Table
Diameter Amps Volts Wire Feed Speed Deposition Rate Efficiency
.045 in, 1.2 mm 145 A 22 V 200 ipm, 508 cm/min 3.94 lbs./hr., 1.79 kg./hr. 86.15 %
210 A 23 V 300 ipm, 762 cm/min 5.99 lbs./hr., 2.72 kg./hr. 85.51 %
247 A 24.5 V 400 ipm, 1016 cm/min 8.10 lbs./hr., 3.68 kg./hr. 87.55 %
275 A 26 V 500 ipm, 1270 cm/min 9.52 lbs./hr., 4.33 kg./hr. 82.08 %
325 A 27.5 V 600 ipm, 1524 cm/min 12.38 lbs./hr., 5.63 kg./hr. 88.39 %
.052 in, 1.4 mm 150 A 21 V 150 ipm, 381 cm/min 4.01 lbs./hr., 1.82 kg./hr. 83.25 %
192 A 22 V 200 ipm, 508 cm/min 5.44 lbs./hr., 2.48 kg./hr. 84.71 %
262 A 23.5 V 300 ipm, 762 cm/min 8.12 lbs./hr., 3.69 kg./hr. 85.48 %
308 A 25 V 400 ipm, 1016 cm/min 10.92 lbs./hr., 4.97 kg./hr. 86.31 %
356 A 26.5 V 500 ipm, 1270 cm/min 14.00 lbs./hr., 6.37 kg./hr. 88.12 %
396 A 28 V 600 ipm, 1524 cm/min 16.81 lbs./hr., 7.65 kg./hr. 87.77 %
1/16 in, 1.6 mm 203 A 23 V 150 ipm, 381 cm/min 5.63 lbs./hr., 2.56 kg./hr. 87.15 %
298 A 24.5 V 250 ipm, 635 cm/min 9.33 lbs./hr., 4.25 kg./hr. 87.56 %
340 A 25.5 V 300 ipm, 762 cm/min 11.10 lbs./hr., 5.05 kg./hr. 87.68 %
375 A 26 V 350 ipm, 889 cm/min 13.24 lbs./hr., 6.02 kg./hr. 88.35 %
408 A 27.5 V 400 ipm, 1016 cm/min 14.49 lbs./hr., 6.59 kg./hr. 85.66 %
469 A 29 V 500 ipm, 1270 cm/min 18.93 lbs./hr., 8.62 kg./hr. 89.10 %

Extra Info

Shielding Gas

75% Argon / 25% CO2

Complementary Products