Dual Shield II 70 Ultra is an all-position flux cored wire that displays exceptional impact properties in both as-welded and stress-relieved conditions.
Dual Shield II 70 Ultra is an all-position flux cored wire that displays exceptional impact properties when used with 75% Ar/25% CO2. The improved properties qualify this wire to the Navy's "HY" classification. The "Ultra" series produces smoother arc characteristics and lower welding fumes. Dual Shield II 70 Ultra was developed to join low and medium carbon steel. The Military classification allows Dual Shield II 70 Ultra to be used for attaching steels of less than 81 ksi (560 MPa) yield to HY-80 and HY-100. Commercial applications include construction, shipbuilding, railcar, and heavy equipment industries.

| As Welded 75% Ar / 25% CO2 | |
|---|---|
| Yield Strength | 72 ksi, 490 MPa |
| Tensile Strength | 81 ksi, 560 MPa |
| Reduction in Area | 75 % |
| Elongation in 2" | 29 % |
| Typical Charpy V-Notch Impact Properties | |
| Testing Temperature 0ºF (-18ºC) | |
| As Welded 75% Ar / 25% CO2 | 117 ft.-lbs., 159 J |
| Testing Temperature -20ºF (-29ºC) | |
| As Welded 75% Ar / 25% CO2 | 70 ft.-lbs., 95 J |
| Typical Undiluted Weld Metal Analysis | |
| 75% Ar / 25% CO2 | |
| C | 0.04 % |
| Mn | 1.0 % |
| Si | 0.4 % |
| P | 0.008 % |
| S | 0.009 % |
| Part No. | Model / Product Description | UPC |
|---|---|---|
| 245013313 | DS II 70 ULT 045X33#PSP | 662303004491 |
| 245013321 | DS II 70 ULT 052X33#PSP | 662303004507 |
| 245013339 | DS II 70 ULT 1/16X33#PSP | 662303004514 |
| 245013339-03 | DS II 70 ULT 1/16X33#PSP | 662303077518 |
| 245013354 | DS II 70 ULT 1/16X60#CL | 662303004521 |
| 245013362 | DS II 70 ULT 1/16X10#PSP | 662303004538 |
| 245013362-03 | DS II 70 ULT 1/16X10#PSP | 662303077525 |
| 245013370 | DS II 70 ULT 045X10#PSP | 662303004545 |
| 245013370-23 | DS II 70 ULT 045X10#PSP | 662303055608 |
| 245013388 | DS II 70 ULT 045X60#CL | 662303004552 |
| 245013396 | DS II 70 ULT 052X10#PSP | 662303004569 |
| 245013396-03 | DS II 70 ULT 052X10#PSP | 662303059668 |
| 245013453 | DS II 70 ULT 045X33#PSP VP | 662303004613 |
| 245013479 | DS II 70 ULT 1/16X33#PSP VP | 662303004637 |
| 245013743 | DS II 70 ULT 035X10#PSP | 662303004880 |
| 245013750 | DS II 70 ULT 035X33#PSP | 662303004897 |
| 245014493 | DS II 70 ULT 1/16X10#FR HS | 662303005337 |
| 245014519 | DS II 70 ULT 1/16X25#FR HS | 662303005351 |
| 245014600-34 | DS II 70 ULT 045X25#FR HS | 662303057374 |
| 245014618 | DS II 70 ULT 045X10#FR HS | 662303005436 |
| 245014626 | DS II 70 ULT 035X10#FR HS | 662303005443 |
| 245014709 | DS II 70 ULT 045X15#PSP | 662303005511 |
| 245014857 | DS II 70 ULT 052X15#PSP | 662303005641 |
| 245015821-05 | DS II 70 ULT 045X10PSP 1/CT/60 | 662303073817 |
| 245013404 | DS II 70 ULT 052X60#CL | 662303004576 |
| 245014758 | DS II 70 ULT 045X25#FR VP | |
| 245014808 | DS II 70 ULT 1/16X15#PSP | 662303005597 |
| 245014808-03 | DS II 70 ULT 1/16X15#PSP | 662303081638 |
| 245014857-03 | DS II 70 ULT 052X15#PSP | 662303081621 |
| Diameter | Amps | Volts | Wire Feed Speed | Deposition Rate | Efficiency |
|---|---|---|---|---|---|
| .045 in, 1.2 mm | 145 A | 22 V | 200 ipm, 508 cm/min | 3.94 lbs./hr., 1.79 kg./hr. | 86.15 % |
| 210 A | 23 V | 300 ipm, 762 cm/min | 5.99 lbs./hr., 2.72 kg./hr. | 85.51 % | |
| 247 A | 24.5 V | 400 ipm, 1016 cm/min | 8.10 lbs./hr., 3.68 kg./hr. | 87.55 % | |
| 275 A | 26 V | 500 ipm, 1270 cm/min | 9.52 lbs./hr., 4.33 kg./hr. | 82.08 % | |
| 325 A | 27.5 V | 600 ipm, 1524 cm/min | 12.38 lbs./hr., 5.63 kg./hr. | 88.39 % | |
| .052 in, 1.4 mm | 150 A | 21 V | 150 ipm, 381 cm/min | 4.01 lbs./hr., 1.82 kg./hr. | 83.25 % |
| 192 A | 22 V | 200 ipm, 508 cm/min | 5.44 lbs./hr., 2.48 kg./hr. | 84.71 % | |
| 262 A | 23.5 V | 300 ipm, 762 cm/min | 8.12 lbs./hr., 3.69 kg./hr. | 85.48 % | |
| 308 A | 25 V | 400 ipm, 1016 cm/min | 10.92 lbs./hr., 4.97 kg./hr. | 86.31 % | |
| 356 A | 26.5 V | 500 ipm, 1270 cm/min | 14.00 lbs./hr., 6.37 kg./hr. | 88.12 % | |
| 396 A | 28 V | 600 ipm, 1524 cm/min | 16.81 lbs./hr., 7.65 kg./hr. | 87.77 % | |
| 1/16 in, 1.6 mm | 203 A | 23 V | 150 ipm, 381 cm/min | 5.63 lbs./hr., 2.56 kg./hr. | 87.15 % |
| 298 A | 24.5 V | 250 ipm, 635 cm/min | 9.33 lbs./hr., 4.25 kg./hr. | 87.56 % | |
| 340 A | 25.5 V | 300 ipm, 762 cm/min | 11.10 lbs./hr., 5.05 kg./hr. | 87.68 % | |
| 375 A | 26 V | 350 ipm, 889 cm/min | 13.24 lbs./hr., 6.02 kg./hr. | 88.35 % | |
| 408 A | 27.5 V | 400 ipm, 1016 cm/min | 14.49 lbs./hr., 6.59 kg./hr. | 85.66 % | |
| 469 A | 29 V | 500 ipm, 1270 cm/min | 18.93 lbs./hr., 8.62 kg./hr. | 89.10 % | |
75% Argon / 25% CO2