Print this page

DUAL SHIELD 111-AC

Dual Shield 111-AC is a flux cored wire for single or multipass operation on mild steel and on some low alloy steels.

Features

Dual Shield 111-AC is a flux cored wire for single or multipass operation on mild steel and on some low alloy steels. Dual Shield 111-AC has proven capabilities in fabrication of bridges, pressure vessels, earth moving equipment, construction, shipbuilding and welding pertaining to structural and nuclear codes. There is very little spatter when welded with balanced voltage and amperage. The thin slag cover removes easily. The weld bead appearance and easy operation make this wire an ideal choice for general fabrication and repair. Dual Shield 111-AC wire is designed to weld mild and medium carbon steels and some low alloy steels. The steel should be reasonably clean and, for greater efficiency, the work should be positioned so that the welding is performed in the flat position

DUAL SHIELD 111-AC
  • Industry
  • Mobile Machinery
  • Civil Construction
  • Shipbuilding
  • General Fabrication
  • Welding Process
  • FCAW (Flux Core)

Classifications

  • Classifications/Approvals

    • AWS A5.20; E70T-1C
    • ASME SFA 5.20

Properties

Typical Properties
As Welded CO2  
Yield Strength 72 ksi, 495 MPa
Tensile Strength 84 ksi, 580 MPa
Elongation in 2" 26 %
Reduction in Area 59 %
Typical Charpy V-Notch Inpact Properties  
Testing Temperature 0ºF (-18ºC)  
As Welded CO2 42 ft.-lbs., 57 J
Testing Temperature 70ºF (20ºC)  
As Welded CO2 64 ft.-lbs., 87 J
Typical Undiluted Weld Metal Analysis  
As Welded CO2  
C 0.07 %
Mn 1.45 %
Si 0.48 %
P 0.017 %
S 0.012 %

Part No.

111-AC
Part No. Model / Product Description UPC
242204022 DS 111-AC 1/16X33#AWS 662303001452
242204287 DS 111 A-C 1/16X500#MP 662303009236
242204311 DS 111 A-C 5/64X500#MP 662303046415
242204402 DS 111-AC 5/64X60#CL 662303001476
242204428 DS 111-AC 1/16X60#CL 662303001483
242204436 DS 111-AC 3/32X60#CL 662303001490
242204477 DS 111-AC 7/64X60#CL 662303001513
242204014 DS 111-AC 1/16X600#OMP 662303079291
242204329 DS 111-AC 5/64X600#OMP 662303079307

SAW

Accessories

Depositions/Paramaters

Extra Info

Shielding Gas

CO2

Complementary Products

Seismic Data

All listed prices are in U.S. dollars and represent the Manufacturer's Suggested Retail Price (MSRP) for sale in the United States. Actual selling price will be determined by the Distributor. Prices are subject to change without notice.