Print this page

DUAL SHIELD ARC-70

Dual Shield Arc 70 is a large diameter flux cored wire for flat and horizontal welding over heavy rust and mill scale.

Features

Dual Shield Arc 70 is a large diameter flux cored wire for flat and horizontal welding over heavy rust and mill scale. Arc characteristics and spatter levels are extremely low.

Dual Shield Arc-70
  • Industry
  • Shipbuilding
  • Automotive
  • General Fabrication
  • Civil Construction
  • Mobile Machinery
  • Rail Road Car
  • Welding Process
  • FCAW (Flux Core)

Classifications

  • Classifications/Approvals

    • AWS A5.20; E70T-1C/T-1M/T-9C/T-9M
    • CERTIFIED BY C.W.B.- CSA W48
    • ASME SFA 5.20

Properties

Typical Properties
As Welded CO2  
Yield Strength 76 ksi, 530 MPa
Tensile Strength 90 ksi, 620 MPa
Elongation in 2" 26 %
Typical Charpy V-Notch Inpact Properties  
Testing Temperature 0ºF (-18ºC)  
As Welded CO2 30 ft.-lbs., 41 J
Typical Undiluted Weld Metal Analysis  
As Welded CO2  
C 0.07 %
Mn 1.36 %
Si 0.65 %
P 0.016 %
S 0.013 %

Part No.

Arc 70
Part No. Model / Product Description UPC
245002043 DS ARC-70 3/32X250#SPOP 662303075446
245002001 DS ARC-70 1/16X60#CL 662303003678
245002019 DS ARC-70 5/64X60#CL 662303030988
245002027 DS ARC-70 3/32X60#CL 662303003692
245002035 DS ARC-70 7/64X60#CL 662303075460
245002068 DS ARC-70 1/16X500#MP 662303076078

SAW

Accessories

Depositions/Paramaters

Deposition Table
Diameter Amps Volts Wire Feed Speed Deposition Rate Efficiency
1/16 in, 1.6 mm 190 A 27 150 ipm, 38 cm/min 6.1 lbs./hr., 2.77 kg./hr. 87 %
300 A 30 250 ipm, 635 cm/min 10.2 lbs./hr., 4.63 kg./hr. 87 %
365 A 33 300 ipm, 762 cm/min 12.3 lbs./hr., 5.58 kg./hr. 86 %
410 A 33 350 ipm, 889 cm/min 14 lbs./hr., 6.35 kg./hr. 88 %
450 A 33 400 ipm, 1016 cm/min 16.1 lbs./hr., 7.3 kg./hr. 87 %
500 A 39 500 ipm, 1270 cm/min 20.1 lbs./hr., 9.11 kg./hr. 87 %
5/64 in, 2.0 mm 250 A 26 112 ipm, 284 cm/min 6.4 lbs./hr., 2.9 kg./hr. 85 %
350 A 28 176 ipm, 447 cm/min 10.5 lbs./hr., 4.76 kg./hr. 85 %
450 A 31 258 ipm, 655 cm/min 14.8 lbs./hr., 6.71 kg./hr. 85 %
3/32 in, 2.4 mm 350 A 30 124 ipm, 315 cm/min 9.6 lbs./hr., 4.35 kg./hr. 84 %
400 A 30 166 ipm, 422 cm/min 12.7 lbs./hr., 5.76 kg./hr. 85 %
450 A 31 197 ipm, 500 cm/min 15 lbs./hr., 6.8 kg./hr. 86 %
500 A 32 237 ipm, 602 cm/min 18.5 lbs./hr., 8.39 kg./hr. 86 %
550 A 34 278 ipm, 706 cm/min 21.3 lbs./hr., 9.66 kg./hr. 88 %
7/64 in, 2.8 mm 550 A 30 140 ipm, 356 cm/min 17.1 lbs./hr., 7.76 kg./hr. 85 %
625 A 34 161 ipm, 409 cm/min 19.6 lbs./hr., 8.89 kg./hr. 86 %
700 A 36 190 ipm, 483 cm/min 23 lbs./hr., 10.43 kg./hr. 86 %