Print this page

DUAL SHIELD B6

Dual Shield B6 is an all position flux cored wire designed to weld Mo steels.

Features

Dual Shield B6 is an all-position flux cored electrode designed for using with 75% Ar / 25% CO2 or 100% CO2 shielding gas. Dual Shield B6 is intended for use on pipe and plate steels having a nominal 5% Chromium - 0.5% Molybdenum composition. These steels are typically used in process piping in the oil, gas, petrochemical, and marine industries.

Dual Shield B6
  • Industry
  • Power Generation
  • Pipeline
  • Petrochemical
  • Welding Process
  • FCAW (Flux Core)

Classifications

  • Classifications/Approvals

    • AWS A5.29;E81T1-B6C/B6M
    • ASME SFA 5.29

Properties

Typical Properties
Typical Mechanical Properties  
Stress Relieved 2 hrs. @ 1375ºF (746ºC) 75% Ar / 25% CO2  
Yield Strength 84 ksi, 580 MPa
Tensile Strength 98 ksi, 675 MPa
Reduction of Area 65 %
Elongation in 2" 20 %
Stress Relieved 2 hrs. @ 1375ºF (746ºC) CO2  
Yield Strength 78 ksi, 540 MPa
Tensile Strength 93 ksi, 640 MPa
Reduction of Area 67 %
Elongation in 2" 21 %
Stress Relieved 2 hrs. @ 1375ºF (746ºC) 75% Ar / 25% CO2  
Yield Strength 84 ksi, 580 MPa
Tensile Strength 98.5 ksi, 680 MPa
Reduction of Area 65 %
Elongation in 2" 20 %
Typical Undiluted Weld Metal Analysis  
CO2  
C .062 %
Mn .56 %
Si 0.57 %
P 0.015 %
S 0.008 %
Cr 5.05 %
Mo 0.57 %
75% Ar / 25% CO2  
C 0.071 %
Mn 0.63 %
Si 0.75 %
P .014 %
S .010 %
Cr 5.28 %
Mo 0.57 %

Part No.

B6
Part No. Model / Product Description UPC
258079037 DS B6 045X10#PSP VP/60CT 662303048860
258079045 DS B6 045X33#PSP VP 662303048877
258079052 DS B6 045X15#PSP VP 662303081485

SAW

Accessories

Depositions/Paramaters

Extra Info

Shielding Gas

100% CO2 or Argon / CO2 mixtures

Complementary Products

Seismic Data

All listed prices are in U.S. dollars and represent the Manufacturer's Suggested Retail Price (MSRP) for sale in the United States. Actual selling price will be determined by the Distributor. Prices are subject to change without notice.