Print this page

DUAL SHIELD 88-CM

Dual Shield 88-CM is a flux cored continuous wire depositing X-ray sound weld metal with a nominal analysis of 1.25% Cr, 0.5% Mo.

Features

Dual Shield 88-CM is a flux cored electrode depositing X-ray sound weld metal with a nominal analysis of 1.25% Cr, 0.5% Mo. The weld beads are slightly convex with very fine ripples and horizontal fillets have equal leg lengths. The arc is smooth and deeply penetrating and has minimal spatter. The weld metal analysis is similar to an E8018-B2 low Hydrogen electrode. Dual Shield 88-CM wire is used for the welding of such steel as 0.5% Cr - 0.5% Mo, 1% Cr - 0.5% Mo, and 1.25% Cr - 0.5% Mo. Dual Shield 88-CM is designed for single or multiple pass welds in the flat or horizontal fillet positions using 100% CO2 shielding gas.

DUAL SHIELD 88-CM
  • Industry
  • Power Generation
  • Pipeline
  • Welding Process
  • FCAW (Flux Core)

Classifications

  • Classifications/Approvals

    • AWS A5.29; E80T1-B2C
    • ASME SFA 5.29

Properties

Typical Properties
Stress Relieved 1 hr. @ 1275ºF (691ºC) CO2  
Yield Strength 72 ksi, 500 MPa
Tensile Strength 85 ksi, 585 MPa
Reduction in Area 55 %
Elongation in 2" 23 %
Typical Undiluted Weld Metal Analysis  
CO2  
C .07 %
Mn .55 %
Si .20 %
P .013 %
S .010 %
Cr 1.20 %
Mo .50 %

Part No.

88-CM
Part No. Model / Product Description UPC
245005434 DS 88-CM 3/32X60#CL 662303003807

SAW

Accessories

Depositions/Paramaters

Deposition Table
Diameter Amps Volts Wire Feed Speed Deposition Rate Efficiency
.035 in, 0.9 mm 130 A A 22 288 ipm, 732 cm/min 3.2 lbs./hr., 1.45 kg./hr. 85 %
150 A A 25 384 ipm, 975 cm/min 4.3 lbs./hr., 1.95 kg./hr. 85 %
200 A A 27 576 ipm, 1463 cm/min 6.5 lbs./hr., 2.95 kg./hr. 85 %
250 A A 30 784 ipm, 1991 cm/min 8.9 lbs./hr., 4.04 kg./hr. 86 %
.045 in, 1.2 mm 150 A A 28 200 ipm, 508 cm/min 4.2 lbs./hr., 1.91 kg./hr. 86 %
210 A A 29 300 ipm, 762 cm/min 6.3 lbs./hr., 2.86 kg./hr. 86 %
250 A A 30 400 ipm, 1016 cm/min 8.5 lbs./hr., 3.86 kg./hr. 87 %
290 A A 33 500 ipm, 1270 cm/min 10.7 lbs./hr., 4.85 kg./hr. 87 %
330 A A 34 600 ipm, 1524 cm/min 12.7 lbs./hr., 5.76 kg./hr. 87 %
.052 in, 1.4 mm 155 A A 25 150 ipm, 381 cm/min 4.4 lbs./hr., 2 kg./hr. 87 %
245 A A 28 250 ipm, 635 cm/min 7.3 lbs./hr., 3.31 kg./hr. 86 %
310 A A 33 350 ipm, 889 cm/min 10.2 lbs./hr., 4.63 kg./hr. 85 %
360 A A 36 450 ipm, 1143 cm/min 13.3 lbs./hr., 6.03 kg./hr. 85 %
430 A A 37 600 ipm, 1524 cm/min 17.6 lbs./hr., 7.98 kg./hr. 87 %
1/16 in, 1.6 mm 190 A A 27 150 ipm, 38 cm/min 6.1 lbs./hr., 2.77 kg./hr. 87 %
300 A A 30 250 ipm, 635 cm/min 10.2 lbs./hr., 4.63 kg./hr. 87 %
365 A A 33 300 ipm, 762 cm/min 12.3 lbs./hr., 5.58 kg./hr. 86 %
410 A A 33 350 ipm, 889 cm/min 14 lbs./hr., 6.35 kg./hr. 88 %
450 A A 33 400 ipm, 1016 cm/min 16.1 lbs./hr., 7.3 kg./hr. 87 %
500 A A 39 500 ipm, 1270 cm/min 20.1 lbs./hr., 9.11 kg./hr. 87 %
5/64 in, 2.0 mm 250 A A 26 112 ipm, 284 cm/min 6.4 lbs./hr., 2.9 kg./hr. 85 %
350 A A 28 176 ipm, 447 cm/min 10.5 lbs./hr., 4.76 kg./hr. 85 %
450 A A 31 258 ipm, 655 cm/min 14.8 lbs./hr., 6.71 kg./hr. 85 %
3/32 in, 2.4 mm 350 A A 30 124 ipm, 315 cm/min 9.6 lbs./hr., 4.35 kg./hr. 84 %
400 A A 30 166 ipm, 422 cm/min 12.7 lbs./hr., 5.76 kg./hr. 85 %
450 A A 31 197 ipm, 500 cm/min 15 lbs./hr., 6.8 kg./hr. 86 %
500 A A 32 237 ipm, 602 cm/min 18.5 lbs./hr., 8.39 kg./hr. 86 %
550 A A 34 278 ipm, 706 cm/min 21.3 lbs./hr., 9.66 kg./hr. 88 %
7/64 in, 2.8 mm 550 A A 30 140 ipm, 356 cm/min 17.1 lbs./hr., 7.76 kg./hr. 85 %
625 A A 34 161 ipm, 409 cm/min 19.6 lbs./hr., 8.89 kg./hr. 86 %
700 A A 36 190 ipm, 483 cm/min 23 lbs./hr., 10.43 kg./hr. 86 %
1/8 in, 3.2 mm 600 A A 32 111 ipm, 282 cm/min 16.2 lbs./hr., 7.35 kg./hr. 86 %
725 A A 34 153 ipm, 389 cm/min 22.5 lbs./hr., 10.21 kg./hr. 86 %
850 A A 38 194 ipm, 93 cm/min 29.2 lbs./hr., 13.25 kg./hr. 85 %

Extra Info

Shielding Gas

100% CO2

Complementary Products

Seismic Data

All listed prices are in U.S. dollars and represent the Manufacturer's Suggested Retail Price (MSRP) for sale in the United States. Actual selling price will be determined by the Distributor. Prices are subject to change without notice.