Dual Shield 8100-Ni2 is an all-position wire that deposits a nominal 2.5% Ni with an 80 ksi(550 Mpa) tensile.
Dual Shield 8100-Ni2 is an all-position flux cored electrode designed for use with 100% CO2 shielding gas. A wider operating range and low spatter with excellent all position capabilities can be expected. Dual Shield 8100-Ni2 has great welder appeal and good weld metal properties which make it desirable for applications such as shipbuilding, mobile machinery, offshore and heavy machinery construction.

| As Welded CO2 | |
|---|---|
| Yield Strength | 74 ksi, 510 MPa |
| Tensile Strength | 85 ksi, 580 MPa |
| Reduction in Area | 70 % |
| Elongation in 2" | 24 % |
| Typical Charpy V-Notch Impact Properties | |
| Testing Temperature 0ºF (-18ºC) | |
| As Welded CO2 | 64 ft.-lbs., 47 J |
| Testing Temperature -20ºF (-29ºC) | |
| As Welded CO2 | 32 ft.-lbs., 23 J |
| Testing Temperature -40ºF (-40ºC) | |
| As Welded CO2 | 20 ft.-lbs., 27 J |
| Typical Undiluted Weld Metal Analysis | |
| CO2 | |
| C | 0.06 % |
| Mn | 1.35 % |
| Si | .60 % |
| P | 0.011 % |
| S | 0.010 % |
| Ni | 2.20 % |
| Part No. | Model / Product Description | UPC |
|---|---|---|
| 245022009 | DS 8100-NI2 045X33#AWS | 662303075781 |
| 245022017 | DS 8100-NI2 052X33#AWS | 662303075798 |
| 245022025 | DS 8100-NI2 1/16X33#AWS | 662303075804 |
| 245022033 | DS 8100-NI2 045X15#PSP | 662303075811 |
| 245022041 | DS 8100-NI2 052X15#PSP | 662303075828 |
| 245022058 | DS 8100-NI2 1/16X15#PSP | 662303075835 |
100% CO2
All listed prices are in U.S. dollars and represent the Manufacturer's Suggested Retail Price (MSRP) for sale in the United States. Actual selling price will be determined by the Distributor. Prices are subject to change without notice.