Print this page

DUAL SHIELD 8000-Ni2

Dual Shield 8000-Ni2 is an all-position wire that deposits 2.5% Ni deposit with an 82 ksi (565 MPa) tensile strength.

Features

Dual Shield 8000-Ni2 is an all-position flux cored electrode that deposits 2.5% Ni deposit with an 82 ksi (565 MPa) minimum tensile strength. Dual Shield 8000-Ni2 may be used with CO2 or Argon mixtures. The Argon-CO2 mixtures reduce spatter and further improve weldability especially for small vertical-up fillets. Dual Shield 8000-Ni2 produces superior weld metal properties which make it most desirable for such applications as shipbuilding and heavy machinery construction. The weld metal analysis is similar to an E8018-C1 low Hydrogen electrode.

Dual Shield 8000-Ni2
  • Industry
  • Mobile Machinery
  • General Fabrication
  • Bridge Construction
  • Process
  • Welding Process
  • FCAW (Flux Core)

Classifications

  • Classifications/Approvals

    • ASME SFA 5.29
    • A.B.S.- 3YSA
    • AWS A5.29; E81T1-Ni2C/Ni2M
    • MIL-E-24403/1; MIL-81T1-Ni2C/Ni2M
    • CERTIFIED BY C.W.B.- AWS A5.29

Properties

Typical Properties
As Welded 75% Ar / 25% CO2  
Yield Strength 82 ksi, 565 MPa
Tensile Strength 90 ksi, 620 MPa
Reduction in Area 68 %
Elongation in 2" 27 %
As Welded CO2  
Yield Strength 80 ksi, 550 MPa
Tensile Strength 88 ksi, 605 MPa
Reduction in Area 67 %
Elongation in 2" 26 %
Typical Charpy V-Notch Impact Properties  
Testing Temperature 0ºF (-18ºC)  
As Welded CO2 62 ft.-lbs., 84 J
As Welded 75% Ar / 25% CO2 63 ft.-lbs., 69 J
Testing Temperature -20ºF (-29ºC)  
As Welded CO2 43 ft.-lbs., 58 J
As Welded 75% Ar / 25% CO2 47 ft.-lbs., 64 J
Testing Temperature -40ºF (-40ºC)  
As Welded CO2 39 ft.-lbs., 53 J
As Welded 75% Ar / 25% CO2 40 ft.-lbs., 54 J
Typical Undiluted Weld Metal Analysis  
CO2  
C .05 %
Mn 0.9 %
Si 0.3 %
P .012 %
S .010 %
Ni 2.2 %
75% Ar / 25% CO2  
C .05 %
Mn 1.1 %
Si 0.4 %
P .012 %
S .010 %
Ni 2.2 %

Part No.

8000-Ni2
Part No. Model / Product Description UPC
242200467 DS 8000-NI2 045X10#PSP 662303000066
242206613 DS 8000-NI2 052X33#PSP 662303025380
245020219 DS 8000-NI2 1/16X33#AWS 662303005931
245020383 DS 8000-NI2 1/16X60#CL 662303006037
245020391 DS 8000-NI2 045X60#CL 662303006044
245020409 DS 8000-NI2 045X33#AWS 662303006051
245020706 DS 8000-NI2 1/16X25#PSP 662303049058
245020722-03 DS 8000-NI2 052X15#PSP 662303059347
245020771 DS 8000-NI2 045X15#PSP 662303075378
245020979-03 DS 8000-NI2 1/16X15#PSP 662303059248
245020409-03 DS 8000-NI2 045X33#AWS 662303079024

SAW

Accessories

Depositions/Paramaters

Deposition Table
Diameter Amps Volts Wire Feed Speed Deposition Rate Efficiency
.035 in, 0.9 mm 130 A 22 288 ipm, 732 cm/min 3.2 lbs./hr., 1.45 kg./hr. 85 %
150 A 25 384 ipm, 975 cm/min 4.3 lbs./hr., 1.95 kg./hr. 85 %
200 A 27 576 ipm, 1463 cm/min 6.5 lbs./hr., 2.95 kg./hr. 85 %
250 A 30 784 ipm, 1991 cm/min 8.9 lbs./hr., 4.04 kg./hr. 86 %
.045 in, 1.2 mm 150 A 28 200 ipm, 508 cm/min 4.2 lbs./hr., 1.91 kg./hr. 86 %
210 A 29 300 ipm, 762 cm/min 6.3 lbs./hr., 2.86 kg./hr. 86 %
250 A 30 400 ipm, 1016 cm/min 8.5 lbs./hr., 3.86 kg./hr. 87 %
290 A 33 500 ipm, 1270 cm/min 10.7 lbs./hr., 4.85 kg./hr. 87 %
330 A 34 600 ipm, 1524 cm/min 12.7 lbs./hr., 5.76 kg./hr. 87 %
.052 in, 1.4 mm 155 A 25 150 ipm, 381 cm/min 4.4 lbs./hr., 2.00 kg./hr. 87 %
245 A 28 250 ipm, 635 cm/min 7.3 lbs./hr., 3.31 kg./hr. 86 %
310 A 33 350 ipm, 889 cm/min 10.2 lbs./hr., 4.63 kg./hr. 85 %
360 A 36 450 ipm, 1143 cm/min 13.3 lbs./hr., 6.03 kg./hr. 85 %
430 A 37 600 ipm, 1524 cm/min 17.6 lbs./hr., 7.98 kg./hr. 87 %
1/16 in, 1.6 mm 190 A 27 150 ipm, 381 cm/min 6.1 lbs./hr., 2.77 kg./hr. 87 %
300 A 30 250 ipm, 635 cm/min 10.2 lbs./hr., 4.63 kg./hr. 87 %
365 A 33 300 ipm, 762 cm/min 12.3 lbs./hr., 5.58 kg./hr. 86 %
410 A 33 350 ipm, 889 cm/min 14 lbs./hr., 6.35 kg./hr. 88 %
450 A 33 400 ipm, 1016 cm/min 16.1 lbs./hr., 7.30 kg./hr. 87 %
500 A 39 500 ipm, 1270 cm/min 20.1 lbs./hr., 9.11 kg./hr. 87 %
5/64 in, 2.0 mm 250 A 26 112 ipm, 284 cm/min 6.4 lbs./hr., 2.90 kg./hr. 85 %
350 A 28 176 ipm, 447 cm/min 10.5 lbs./hr., 4.76 kg./hr. 85 %
450 A 31 258 ipm, 655 cm/min 14.8 lbs./hr., 6.71 kg./hr. 85 %
3/32 in, 2.4 mm 350 A 30 124 ipm, 315 cm/min 9.6 lbs./hr., 4.35 kg./hr. 84 %
400 A 30 166 ipm, 422 cm/min 12.7 lbs./hr., 5.76 kg./hr. 85 %
450 A 31 197 ipm, 500 cm/min 15 lbs./hr., 6.80 kg./hr. 86 %
500 A 32 237 ipm, 602 cm/min 18.5 lbs./hr., 8.39 kg./hr. 86 %
550 A 34 278 ipm, 706 cm/min 21.3 lbs./hr., 9.66 kg./hr. 88 %
7/64 in, 2.8 mm 550 A 30 140 ipm, 356 cm/min 17.1 lbs./hr., 7.76 kg./hr. 85 %
625 A 34 161 ipm, 409 cm/min 19.6 lbs./hr., 8.89 kg./hr. 86 %
700 A 36 190 ipm, 483 cm/min 23 lbs./hr., 10.43 kg./hr. 86 %
1/8 in, 3.2 mm 600 A 32 111 ipm, 282 cm/min 16.2 lbs./hr., 7.35 kg./hr. 86 %
725 A 34 153 ipm, 389 cm/min 22.5 lbs./hr., 10.21 kg./hr. 86 %
850 A 38 194 ipm, 493 cm/min 29.2 lbs./hr., 13.25 kg./hr. 85 %

Extra Info

Shielding Gas

100% CO2 or Argon - CO2 mixtures up to 80% Argon

Complementary Products

Seismic Data

All listed prices are in U.S. dollars and represent the Manufacturer's Suggested Retail Price (MSRP) for sale in the United States. Actual selling price will be determined by the Distributor. Prices are subject to change without notice.