Dual Shield 80-C3

Dual Shield 80-C3 is a flux cored wire designed for use with CO2 shielding. It
deposits a nominally 1% Ni weld metal with impact toughness at temperatures
as low as -20°F (-28°C). It features a stable arc and easily controlled weld
puddle. The thin cover of slag is easily removed, even from deep grooves.
Spatter levels are generally low. X-ray quality welds can easily be produced with
Dual Shield 80-C3

Features

Dual Shield 80-C3 is a flux cored electrode designed for use with CO2 shielding. It
deposits a nominally 1% Ni weld metal with impact toughness at temperatures
as low as -20°F (-28°C). It features a stable arc and easily controlled weld
puddle. The thin cover of slag is easily removed, even from deep grooves.
Spatter levels are generally low. X-ray quality welds can easily be produced with
Dual Shield 80-C3. Dual Shield 80-C3 is recommended for welding steels having 70 and 80 ksi minimum tensile strength steels that will be used in the as welded condition. It also produces a weld metal analysis that is suitable for weathering steels. It is recommended for making fillet and butt welds in 3/8” and thicker plate.

Dual Shield 80-C3
  • Welding Process
  • FCAW (Flux Core)

Classifications

  • Classifications/Approvals

    • AWS A5.29; E80T1-Ni1C
    • ASME SFA 5.29

Properties

Typical Properties
As Welded CO2  
Yield Strength 84 ksi, 580 MPa
Tensile Strength 94 ksi, 650 MPa
Elongation in 2" 22 %
Typical Charpy V-Notch Impact Properties  
Testing Temperature -20ºF (-29ºC)  
As Welded 53 ft.-lbs., 47 J
Typical Undiluted Weld Metal Analysis  
CO2  
C 0.06 %
Mn 1.3 %
Si 0.4 %
P 0.013 %
S 0.009 %
Ni 1.0 %

Part No.

80-C3
Part No. Model / Product Description UPC
245006200 DS 80-C3 5/64X60#CL WCRT 662303076962
245006218 DS 80-C3 3/32X60#CL WCRT 662303076979

SAW

Accessories

Depositions/Paramaters

Extra Info

Shielding Gas

100% CO2

Complementary Products

Seismic Data

All listed prices are in U.S. dollars and represent the Manufacturer's Suggested Retail Price (MSRP) for sale in the United States. Actual selling price will be determined by the Distributor. Prices are subject to change without notice.