Print this page

DUAL SHIELD II 90-K2

Dual Shield II 90-K2 is an all-position, high performance wire with low diffusible hydrogen levels.

Features

Dual Shield II 90-K2 is an all-position, high performance flux cored electrode with low diffusible hydrogen levels. This wire provides a smooth stable arc, low spatter, and easy slag removal similar to other Dual Shield II products.
Dual Shield II 90-K2 was developed for use on commercial grades of HY-80, ASTM A710, A514 and A517 and other similar HSLA low alloy steels.

Dual Shield II 90-K2
  • Welding Process
  • FCAW (Flux Core)

Classifications

  • Classifications/Approvals

    • AWS A5.29; E91T1-K2M
    • ASME SFA 5.29

Properties

Typical Properties
As Welded 75% Ar / 25% CO2  
Yield Strength 88 ksi, 605 MPa
Tensile Strength 94 ksi, 650 MPa
Elongation in 2" 23 %
Stress Relieved 10 hrs. @ 1075ºF (579ºC) 75% Ar / 25% CO2  
Yield Strength 76 ksi, 520 MPa
Tensile Strength 87 ksi, 600 MPa
Elongation in 2" 26 %
Typical Charpy V-Notch Impact Properties  
Testing Temperature -20ºF (-29ºC)  
As Welded 75% Ar / 25% CO2 101 ft.-lbs., 137 J
Testing Temperature -40ºF (-40ºC)  
As Welded 75% Ar / 25% CO2 90 ft.-lbs., 122 J
Testing Temperature -60ºF (-51ºC)  
As Welded 75% Ar / 25% CO2 63 ft.-lbs., 85 J
Typical Undiluted Weld Metal Analysis  
75% Ar / 25% CO2  
C .06 %
Mn 1.42 %
Si 0.33 %
P .014 %
S .010 %
Ni 1.5 %

Part No.

II 90-K2
Part No. Model / Product Description UPC
245013073 DS II 90-K2 1/16X33#PSP 662303004378
245013081 DS II 90-K2 045X33#PSP 662303004385
245013164 DS II 90-K2 1/16X60#CL 662303004446
245013594 DS II 90-K2 1/16X33#PSP VP 662303004750
245013172 DS II 90-K2 1/16X600#OMP 662303079116

SAW

Accessories

Depositions/Paramaters

Deposition Table
Diameter Amps Volts Wire Feed Speed Deposition Rate Efficiency
.035 in, 0.9 mm 130 A A 22 288 ipm, 732 cm/min 3.2 lbs./hr., 1.45 kg./hr. 85 %
150 A A 25 384 ipm, 975 cm/min 4.3 lbs./hr., 1.95 kg./hr. 85 %
200 A A 27 576 ipm, 1463 cm/min 6.5 lbs./hr., 2.95 kg./hr. 85 %
250 A A 30 784 ipm, 1991 cm/min 8.9 lbs./hr., 4.04 kg./hr. 86 %
.045 in, 1.2 mm 150 A A 28 200 ipm, 508 cm/min 4.2 lbs./hr., 1.91 kg./hr. 86 %
210 A A 29 300 ipm, 762 cm/min 6.3 lbs./hr., 2.86 kg./hr. 86 %
250 A A 30 400 ipm, 1016 cm/min 8.5 lbs./hr., 3.86 kg./hr. 87 %
290 A A 33 500 ipm, 1270 cm/min 10.7 lbs./hr., 4.85 kg./hr. 87 %
330 A A 34 600 ipm, 1524 cm/min 12.7 lbs./hr., 5.76 kg./hr. 87 %
.052 in, 1.4 mm 155 A A 25 150 ipm, 381 cm/min 4.4 lbs./hr., 2 kg./hr. 87 %
245 A A 28 250 ipm, 635 cm/min 7.3 lbs./hr., 3.31 kg./hr. 86 %
310 A A 33 350 ipm, 889 cm/min 10.2 lbs./hr., 4.63 kg./hr. 85 %
360 A A 36 450 ipm, 1143 cm/min 13.3 lbs./hr., 6.03 kg./hr. 85 %
430 A A 37 600 ipm, 1524 cm/min 17.6 lbs./hr., 7.98 kg./hr. 87 %
1/16 in, 1.6 mm 190 A A 27 150 ipm, 38 cm/min 6.1 lbs./hr., 2.77 kg./hr. 87 %
300 A A 30 250 ipm, 635 cm/min 10.2 lbs./hr., 4.63 kg./hr. 87 %
365 A A 33 300 ipm, 762 cm/min 12.3 lbs./hr., 5.58 kg./hr. 86 %
410 A A 33 350 ipm, 889 cm/min 14 lbs./hr., 6.35 kg./hr. 88 %
450 A A 33 400 ipm, 1016 cm/min 16.1 lbs./hr., 7.3 kg./hr. 87 %
500 A A 39 500 ipm, 1270 cm/min 20.1 lbs./hr., 9.11 kg./hr. 87 %
5/64 in, 2.0 mm 250 A A 26 112 ipm, 284 cm/min 6.4 lbs./hr., 2.9 kg./hr. 85 %
350 A A 28 176 ipm, 447 cm/min 10.5 lbs./hr., 4.76 kg./hr. 85 %
450 A A 31 258 ipm, 655 cm/min 14.8 lbs./hr., 6.71 kg./hr. 85 %
3/32 in, 2.4 mm 350 A A 30 124 ipm, 315 cm/min 9.6 lbs./hr., 4.35 kg./hr. 84 %
400 A A 30 166 ipm, 422 cm/min 12.7 lbs./hr., 5.76 kg./hr. 85 %
450 A A 31 197 ipm, 500 cm/min 15 lbs./hr., 6.8 kg./hr. 86 %
500 A A 32 237 ipm, 602 cm/min 18.5 lbs./hr., 8.39 kg./hr. 86 %
550 A A 34 278 ipm, 706 cm/min 21.3 lbs./hr., 9.66 kg./hr. 88 %
7/64 in, 2.8 mm 550 A A 30 140 ipm, 356 cm/min 17.1 lbs./hr., 7.76 kg./hr. 85 %
625 A A 34 161 ipm, 409 cm/min 19.6 lbs./hr., 8.89 kg./hr. 86 %
700 A A 36 190 ipm, 483 cm/min 23 lbs./hr., 10.43 kg./hr. 86 %
1/8 in, 3.2 mm 600 A A 32 111 ipm, 282 cm/min 16.2 lbs./hr., 7.35 kg./hr. 86 %
725 A A 34 153 ipm, 389 cm/min 22.5 lbs./hr., 10.21 kg./hr. 86 %
850 A A 38 194 ipm, 93 cm/min 29.2 lbs./hr., 13.25 kg./hr. 85 %

Extra Info

Shielding Gas

75% Argon/25% CO2

Complementary Products

Seismic Data

All listed prices are in U.S. dollars and represent the Manufacturer's Suggested Retail Price (MSRP) for sale in the United States. Actual selling price will be determined by the Distributor. Prices are subject to change without notice.