Print this page

DUAL SHIELD II 101-TM

Dual Shield II 101-TM is an all-position flux cored wire developed to meet the stringent requirements of the military specification.

Features

Dual Shield II 101-TM is an all-position flux cored electrode developed to meet the stringent requirements of the military specification. The excellent mechanical properties and low temperature impact toughness makes it an ideal choice for HY80 and HSLA80 steels. The smooth arc characteristics, low spatter levels, and easy post weld clean-up resemble other Dual Shield II products. Dual Shield II 101-TM was specially designed to weld HY-80 and A710 steels typically used in shipbuilding with 75% Ar / 25% CO2 shielding gas. This product is suitable for single or multipass welding applications.

DUAL SHIELD II 101-TM
  • Industry
  • General Fabrication
  • Mobile Machinery
  • Shipbuilding
  • Welding Process
  • FCAW (Flux Core)

Classifications

  • Classifications/Approvals

    • ASME SFA 5.29
    • QPL-24403/2; MIL-101TM
    • AWS A5.29; E81T1-K2M

Properties

Typical Properties
As Welded MIL-E-24403/2 Vertical-Up HY-80 Base Plate 75% Ar / 25% CO2  
Yield Strength 87 ksi, 605 MPa
Tensile Strength 97 ksi, 670 MPa
Reduction of Area 64 %
Elongation in 2" 24 %
As Welded MIL-E-24403/2 Vertical-Up A-710 Base Plate 75% Ar / 25% CO2  
Yield Strength 86 ksi, 595 MPa
Tensile Strength 95 ksi, 655 MPa
Reduction of Area 61 %
Elongation in 2" 23 %
AWS A5.29 Requirement 75% Ar / 25% CO2  
Yield Strength 86 ksi, 595 MPa
Tensile Strength 94 ksi, 655 MPa
Reduction of Area 64 %
Elongation in 2" 24 %
Typical Charpy V-Notch Impact Properties  
Testing Temperature 0ºF (-18ºC)  
As Welded MIL-E-24403/2 Vertical-Up HY-80 Base Plate 75% Ar / 25% CO2 68 ft.-lbs., 92 J
As Welded MIL-E-24403/2 Vertical-Up A-710 Base Plate 75% Ar / 25% CO2 70 ft.-lbs., 95 J
AWS A5.29 Requirement 75% Ar / 25% CO2 79 ft.-lbs., 107 J
Testing Temperature -60ºF (-51ºC)  
As Welded MIL-E-24403/2 Vertical-Up HY-80 Base Plate 75% Ar / 25% CO2 42 ft.-lbs., 57 J
As Welded MIL-E-24403/2 Vertical-Up A-710 Base Plate 75% Ar / 25% CO2 42 ft.-lbs., 57 J
AWS A5.29 Requirement 75% Ar / 25% CO2 49 ft.-lbs., 66 J
Typical Dynamic Tear Properties  
Testing Temperature 30ºF (-1ºC)  
As Welded 585 ft.-lbs., 793 J
Testing Temperature -20ºF (-29ºC)  
As Welded 385 ft.-lbs., 522 J
Typical Undiluted Weld Metal Analysis  
75% Ar / 25% CO2  
C .05 %
Mn 1.13 %
Si .30 %
P .013 %
S .010 %
Ni 1.72 %

Part No.

II 101-TM
Part No. Model / Product Description UPC
245013834 DS II 101-TM 1/16X33#PSP VP 662303004934
245014329 DS II 101-TM 045X11#PSP VP 662303080693

SAW

Accessories

Depositions/Paramaters

Deposition Table
Diameter Amps Volts Wire Feed Speed Deposition Rate Efficiency
.035 in, 0.9 mm 130 A A 22 288 ipm, 732 cm/min 3.2 lbs./hr., 1.45 kg./hr. 85 %
150 A A 25 384 ipm, 975 cm/min 4.3 lbs./hr., 1.95 kg./hr. 85 %
200 A A 27 576 ipm, 1463 cm/min 6.5 lbs./hr., 2.95 kg./hr. 85 %
250 A A 30 784 ipm, 1991 cm/min 8.9 lbs./hr., 4.04 kg./hr. 86 %
.045 in, 1.2 mm 150 A A 28 200 ipm, 508 cm/min 4.2 lbs./hr., 1.91 kg./hr. 86 %
210 A A 29 300 ipm, 762 cm/min 6.3 lbs./hr., 2.86 kg./hr. 86 %
250 A A 30 400 ipm, 1016 cm/min 8.5 lbs./hr., 3.86 kg./hr. 87 %
290 A A 33 500 ipm, 1270 cm/min 10.7 lbs./hr., 4.85 kg./hr. 87 %
330 A A 34 600 ipm, 1524 cm/min 12.7 lbs./hr., 5.76 kg./hr. 87 %
.052 in, 1.4 mm 155 A A 25 150 ipm, 381 cm/min 4.4 lbs./hr., 2 kg./hr. 87 %
245 A A 28 250 ipm, 635 cm/min 7.3 lbs./hr., 3.31 kg./hr. 86 %
310 A A 33 350 ipm, 889 cm/min 10.2 lbs./hr., 4.63 kg./hr. 85 %
360 A A 36 450 ipm, 1143 cm/min 13.3 lbs./hr., 6.03 kg./hr. 85 %
430 A A 37 600 ipm, 1524 cm/min 17.6 lbs./hr., 7.98 kg./hr. 87 %
1/16 in, 1.6 mm 190 A A 27 150 ipm, 38 cm/min 6.1 lbs./hr., 2.77 kg./hr. 87 %
300 A A 30 250 ipm, 635 cm/min 10.2 lbs./hr., 4.63 kg./hr. 87 %
365 A A 33 300 ipm, 762 cm/min 12.3 lbs./hr., 5.58 kg./hr. 86 %
410 A A 33 350 ipm, 889 cm/min 14 lbs./hr., 6.35 kg./hr. 88 %
450 A A 33 400 ipm, 1016 cm/min 16.1 lbs./hr., 7.3 kg./hr. 87 %
500 A A 39 500 ipm, 1270 cm/min 20.1 lbs./hr., 9.11 kg./hr. 87 %
5/64 in, 2.0 mm 250 A A 26 112 ipm, 284 cm/min 6.4 lbs./hr., 2.9 kg./hr. 85 %
350 A A 28 176 ipm, 447 cm/min 10.5 lbs./hr., 4.76 kg./hr. 85 %
450 A A 31 258 ipm, 655 cm/min 14.8 lbs./hr., 6.71 kg./hr. 85 %
3/32 in, 2.4 mm 350 A A 30 124 ipm, 315 cm/min 9.6 lbs./hr., 4.35 kg./hr. 84 %
400 A A 30 166 ipm, 422 cm/min 12.7 lbs./hr., 5.76 kg./hr. 85 %
450 A A 31 197 ipm, 500 cm/min 15 lbs./hr., 6.8 kg./hr. 86 %
500 A A 32 237 ipm, 602 cm/min 18.5 lbs./hr., 8.39 kg./hr. 86 %
550 A A 34 278 ipm, 706 cm/min 21.3 lbs./hr., 9.66 kg./hr. 88 %
7/64 in, 2.8 mm 550 A A 30 140 ipm, 356 cm/min 17.1 lbs./hr., 7.76 kg./hr. 85 %
625 A A 34 161 ipm, 409 cm/min 19.6 lbs./hr., 8.89 kg./hr. 86 %
700 A A 36 190 ipm, 483 cm/min 23 lbs./hr., 10.43 kg./hr. 86 %
1/8 in, 3.2 mm 600 A A 32 111 ipm, 282 cm/min 16.2 lbs./hr., 7.35 kg./hr. 86 %
725 A A 34 153 ipm, 389 cm/min 22.5 lbs./hr., 10.21 kg./hr. 86 %
850 A A 38 194 ipm, 93 cm/min 29.2 lbs./hr., 13.25 kg./hr. 85 %