DUAL SHIELD II 81-K2

Dual Shield II 81-K2 is an all-position flux cored electrode
developed for low alloy high strength steels where low temperature impact toughness is required. It is tested and certified to meet the new AWS A5.20 ‘D’ designation requirements, making this gas-shielded wire an excellent choice for demand critical welds when FEMA 353, D1.1 or D1.8 Seismic Supplement is utilized.

Features

The wire produces a smooth stable arc and low spatter levels using a 100% CO2 shielding gas. Dual Shield II 81-K2 was developed for higher tensile steels such as ASTM A302, A533 Class I and A537. Applications include ship fabrication, offshore oil rigs, and heavy equipment construction. This wire is an excellent choice for welding ASTM steels A302, A533 Class I and A537. Dual Shield II 81-K2 produces a smooth stable arc and low spatter levels using 100% CO2 shielding gas. Applications include ship building, offshore oilrigs, and heavy equipment construction.

Please see Related Links on the right side of this page to download the Seismic Data Sheet and Seismic Certifications.

Dual Shield II 81-K2
  • Industry
  • Mobile Machinery
  • Shipbuilding
  • Civil Construction
  • Rail Road Car
  • General Fabrication
  • Welding Process
  • FCAW (Flux Core)

Classifications

  • Classifications/Approvals

    • AWS A5.20: SEISMIC
    • AWS A5.29;E81T1-K2M-H8
    • AWS A5.29;E81T1-K2C-H8
    • ASME SFA 5.29

Properties

Typical Properties
As Welded CO2  
Tensile Strength 82 ksi, 570 MPa
Yield Strength 74 ksi, 515 MPa
Elongation in 2" 27 %
Reduction of Area 73 %
Typical Charpy V-Notch Impact Properties  
Testing Temperature 0ºF (-18ºC)  
As Welded CO2 100 ft.-lbs., 136 J
Testing Temperature -20ºF (-29ºC)  
As Welded CO2 89 ft.-lbs., 121 J
Testing Temperature -60ºF (-51ºC)  
As Welded CO2 60 ft.-lbs., 81 J
Typical Undiluted Weld Metal Analysis  
CO2  
C .025 %
Mn 1.18 %
Si .49 %
P .013 %
S .009 %
Ni 1.44 %

Part No.

II 81-K2
Part No. Model / Product Description UPC
245014865 DS II 81-K2 045X33#PSP VP 662303005658
245014931 DS II 81-K2 1/16X33#PSP VP 662303005726
245015102 DS II 81-K2 1/16X300#WR 662303068172
245015128 DS II 81-K2 1/16X60#CL 662303068165
245015136 DS II 81-K2 052X300#WR 662303075316

SAW

Accessories

Depositions/Paramaters

Deposition Table
Diameter Amps Volts Wire Feed Speed Deposition Rate Efficiency
.045 in, 1.2 mm 150 A 28 200 ipm, 508 cm/min 4.2 lbs./hr., 1.91 kg./hr. 86 %
210 A 29 300 ipm, 762 cm/min 6.3 lbs./hr., 2.86 kg./hr. 86 %
250 A 30 400 ipm, 1016 cm/min 8.5 lbs./hr., 3.86 kg./hr. 87 %
290 A 33 500 ipm, 1270 cm/min 10.7 lbs./hr., 4.85 kg./hr. 87 %
330 A 34 600 ipm, 1524 cm/min 12.7 lbs./hr., 5.76 kg./hr. 87 %
.052 in, 1.4 mm 155 A 25 150 ipm, 381 cm/min 4.4 lbs./hr., 2 kg./hr. 87 %
245 A 28 250 ipm, 635 cm/min 7.3 lbs./hr., 3.31 kg./hr. 86 %
310 A 33 350 ipm, 889 cm/min 10.2 lbs./hr., 4.63 kg./hr. 85 %
360 A 36 450 ipm, 1143 cm/min 13.3 lbs./hr., 6.03 kg./hr. 85 %
430 A 37 600 ipm, 1524 cm/min 17.6 lbs./hr., 7.98 kg./hr. 87 %
1/16 in, 1.6 mm 190 A 27 150 ipm, 38 cm/min 6.1 lbs./hr., 2.77 kg./hr. 87 %
300 A 30 250 ipm, 635 cm/min 10.2 lbs./hr., 4.63 kg./hr. 87 %
365 A 33 300 ipm, 762 cm/min 12.3 lbs./hr., 5.58 kg./hr. 86 %
410 A 33 350 ipm, 889 cm/min 14 lbs./hr., 6.35 kg./hr. 88 %
450 A 33 400 ipm, 1016 cm/min 16.1 lbs./hr., 7.3 kg./hr. 87 %
500 A 39 500 ipm, 1270 cm/min 20.1 lbs./hr., 9.11 kg./hr. 87 %

Extra Info

Shielding Gas

100% CO2

Complementary Products

Seismic Data

All listed prices are in U.S. dollars and represent the Manufacturer's Suggested Retail Price (MSRP) for sale in the United States. Actual selling price will be determined by the Distributor. Prices are subject to change without notice.