SHIELD-BRIGHT 308L

Shield-Bright 308L was developed for out-of-position welding on type 304 or 304L steels.

Features

Shield-Bright 308L was developed for welding type 304L stainless steel and can also be used for welding types 301, 302, and 304 steels. It may also be used for welding types 321 and 347 if the service conditions do not exceed an approximate of 750°F (399°C).

Shield-Bright 308L was designed for welding in all position and performs particularly well in the vertical position with excellent slag removal.

* This item is subject to Industry Alloy Surcharges

Shield-Bright 308L
  • Industry
  • Shipbuilding
  • Process
  • Pipeline
  • General Fabrication
  • Mobile Machinery
  • Welding Process
  • FCAW (Flux Core)

Classifications

  • Classifications/Approvals

    • ASME II SFA 5.22 E308LT1-1/LT1-4
    • ASME IX F No. 6
    • CWB
    • TUV
    • MIL-STD-1689 APPLICATIONS-NAVY
    • ABS

Properties

Typical Properties
As Welded using 75% Ar - 25% CO2  
Tensile Strength 85 ksi, 580 MPa
Yield Strength 60 ksi, 410 MPa
Elongation in 2" 44 %
Typical Undiluted Weld Metal Analysis  
100% CO2  
C 0.03%
Mn 1.2%
Si 0.8%
Cr 19%
Ni 10%
Mo 0.1%
Cu 0.15%
Ferrite 7 FN
75% Ar / 25% CO2  
C 0.03%
Mn 1.2%
Si 0.9%
Cr 19%
Ni 10%
Mo 0.1%
Cu 0.15%
Ferrite 7 FN

Part No.

308L
Part No. Model / Product Description UPC
252200035 SB 308L 1/16X50#CL 662303007492
252200043 SB 308L 1/16X33#PSP VP 662303007508
252200050 SB 308L 045X33#PSP VP 662303007515
252200100 SB 308L 045X15#PSP VP/60CT 662303044473
252200175 SB 308L 045X10#PSP VP/60CT 662303007607
252200423 SB 308L 035X33#PSP VP 662303007720
252200449 SB 308L 035X10#PSP VP/60CT 662303007744
252201769 SB 308L 1/16X250#SPOP 662303080051

SAW

Accessories

Depositions/Paramaters

Deposition Table
Diameter Amps Volts Wire Feed Speed Deposition Rate Efficiency Electrical Stickout
.035 in, 0.9 mm 100 A 23 265 ipm, 6.7 cm/min 2.9 lbs./hr., 1.3 kg./hr. 83.9 % 1/2 - 1 inches, 12.5 - 25 mm
120 A 23 315 ipm, 8 cm/min 3.4 lbs./hr., 1.5 kg./hr. 81.4 % 1/2 - 1 inches, 12.5 - 25 mm
140 A 25 405 ipm, 10.3 cm/min 4.6 lbs./hr., 2.1 kg./hr. 82.6 % 1/2 - 1 inches, 12.5 - 25 mm
170 A 26 530 ipm, 13.5 cm/min 5.7 lbs./hr., 2.6 kg./hr. 81.8 % 1/2 - 1 inches, 12.5 - 25 mm
.045 in, 1.2 mm 130 A 25 227 ipm, 5.8 cm/min 4.25 lbs./hr., 1.9 kg./hr. 84 % 1/2 - 1 inches, 12.5 - 25 mm
165 A 26 341 ipm, 8.7 cm/min 6.14 lbs./hr., 2.8 kg./hr. 83 % 1/2 - 1 inches, 12.5 - 25 mm
190 A 28 445 ipm, 11.3 cm/min 8.08 lbs./hr., 3.7 kg./hr. 84 % 1/2 - 1 inches, 12.5 - 25 mm
220 A 30 567 ipm, 14.4 cm/min 10.24 lbs./hr., 4.6 kg./hr. 84 % 1/2 - 1 inches, 12.5 - 25 mm
1/16 in, 1.6 mm 170 A 25 154 ipm, 3.9 cm/min 5.34 lbs./hr., 2.4 kg./hr. 83 % 1/2 - 1 inches, 12.5 - 25 mm
210 A 27 193 ipm, 4.9 cm/min 6.89 lbs./hr., 3.1 kg./hr. 82.5 % 1/2 - 1 inches, 12.5 - 25 mm
250 A 28 243 ipm, 6.2 cm/min 8.57 lbs./hr., 3.9 kg./hr. 83 % 1/2 - 1 inches, 12.5 - 25 mm
300 A 29 321 ipm, 8.2 cm/min 11.43 lbs./hr., 5.2 kg./hr. 83 % 1/2 - 1 inches, 12.5 - 25 mm

Extra Info

Shielding Gas

75%Ar / 25%CO2 or 100% CO2