Print this page

SHIELD-BRIGHT 309L X-tra

Shield-Bright 309L X-tra was developed to maximize performance in the flat and horizontal positions when joining stainless to mild or carbon steel.

Features

Shield-Bright 309L X-tra was developed for the welding of stainless steels to carbon or low alloy steels and for the first layer cladding of carbon and low alloy steels. Shield-Bright 309L X-tra was developed for welding in the flat position and for horizontal fillet welds with flat to concave beads with excellent slag removal.

For joining thick sections, it is preferred the non-stainless steel be buttered with a layer of Shield-Bright 309L X-tra and the joint completed with Shield-Bright 316L X-tra or 308L X-tra. The service temperature should not exceed approximately 750ºF (399ºC).

* This item is subject to Industry Alloy Surcharges

Shield-Bright 309L Xtra
  • Industry
  • Process
  • Shipbuilding
  • General Fabrication
  • Mobile Machinery
  • Welding Process
  • FCAW (Flux Core)

Classifications

  • Classifications/Approvals

    • ABS - AWS A5.22; E309LT0-1
    • AWS A5.22; E309LT0-1/T0-4
    • ABS - AWS A5.22; E309LT0-1
    • ASME II SFA 5.22 E309LT0-1/T0-4
    • MIL-STD-1689 APPLICATIONS-NAVY
    • ASME IX F No. 6
    • TUV
    • CERTIFIED BY C.W.B.- AWS A5.22
    • D.N.V.- 309L MS

Properties

Typical Properties
As Welded 75% Ar / 25% CO2  
Tensile Strength 87 ksi, 600 MPa
Yield Strength 70 ksi, 480 MPa
Elongation in 2" 35 %
Typical Undiluted Weld Metal Analysis  
As Welded CO2  
C 0.03 %
Mn 1.3 %
Si 0.7 %
Cr 24 %
Ni 12.5 %
Mo 0.1 %
Cu 0.1 %
Ferrite 16 FN
As Welded 75% Ar / 25% CO2  
C 0.03 %
Mn 1.4 %
Si 0.8 %
Cr 24.5 %
Ni 12.5 %
Mo 0.1 %
Cu 0.1 %
Ferrite 18 FN

Part No.

309L X-tra
Part No. Model / Product Description UPC
252201645 SBX 309L 045X33#PSP VP 662303052874
252201652 SBX 309L 1/16X33#PSP VP 662303052881
252202643 SBX 309L 045X10#PSP VP/60CT 662303055059

SAW

Accessories

Depositions/Paramaters

Deposition Table
Diameter Amps Volts Wire Feed Speed Deposition Rate Efficiency Electrical Stickout
.035 in, 0.9 mm 120 A 23 315 ipm, 8 cm/min 3.4 lbs./hr., 1.5 kg./hr. 81.4 % 1/2 - 1 inches, 12.5 - 25 mm
140 A 25 405 ipm, 10.3 cm/min 4.6 lbs./hr., 2.1 kg./hr. 82.6 % 1/2 - 1 inches, 12.5 - 25 mm
170 A 26 530 ipm, 13.5 cm/min 5.7 lbs./hr., 2.6 kg./hr. 81.8 % 1/2 - 1 inches, 12.5 - 25 mm
.045 in, 1.2 mm 150 A 25 259 ipm, 6.6 cm/min 5 lbs./hr., 2.3 kg./hr. 83.9 % 1/2 - 1 inches, 12.5 - 25 mm
200 A 29 410 ipm, 10.4 cm/min 7.7 lbs./hr., 3.5 kg./hr. 84.2 % 1/2 - 1 inches, 12.5 - 25 mm
300 A 33 860 ipm, 21.9 cm/min 16.9 lbs./hr., 7.7 kg./hr. 87 % 1/2 - 1 inches, 12.5 - 25 mm
1/16 in, 1.6 mm 200 A 25 172 ipm, 4.4 cm/min 6.7 lbs./hr., 3.1 kg./hr. 83.6 % 1/2 - 1 inches, 12.5 - 25 mm
240 A 28 225 ipm, 5.7 cm/min 8.1 lbs./hr., 3.7 kg./hr. 83.6 % 1/2 - 1 inches, 12.5 - 25 mm
400 A 33 495 ipm, 12.58 cm/min 18.9 lbs./hr., 8.6 kg./hr. 85.5 % 1/2 - 1 inches, 12.5 - 25 mm

Extra Info

Shielding Gas

75%Ar / 25%CO2 or 100%CO2

Complementary Products

Seismic Data