Print this page

SHIELD-BRIGHT 309L

Shield-Bright 309L was developed for out-of-position welding when joining stainless to mild or carbon steel.

Features

Shield-Bright 309L was developed for welding stainless steel to carbon or low alloy steels and for the first layer cladding of carbon and low alloy steels. It was designed for welding in all positions and performs particularly well in the vertical position with excellent slag removal.

For joining thick sections, it is perferred the non-stainless steel be buttered with a layer of Shield-Bright 309L and the joint completed with Shield-Bright 316L or 308L. The service temperature should not exceed approximately 750ºF(399ºC).

* This item is subject to Industry Alloy Surcharges

Shield-Bright 309L
  • Industry
  • Process
  • Mobile Machinery
  • Shipbuilding
  • General Fabrication
  • Welding Process
  • FCAW (Flux Core)

Classifications

  • Classifications/Approvals

    • ASME II SFA 5.22 E309LT1-1/T1-4
    • ASME IX F No. 6
    • G.L.- AWS A5.22; E309LT1-4
    • MIL-STD-1689 APPLICATIONS-NAVY
    • TUV
    • ABS-AWS A5.22; E309LT1-1
    • AWS A5.22; E309LT1-1/T1-4
    • CERTIFIED BY C.W.B.- AWS A5.22

Properties

Typical Properties
As Welded 75% Ar / 25% CO2  
Tensile Strength 87 ksi, 600 MPa
Yield Strength 70 ksi, 480 MPa
Elongation in 2" 35 %
Typical Undiluted Weld Metal Analysis  
As Welded CO2  
C 0.03 %
Mn 1.2 %
Si 0.9 %
Cr 23.5 %
Ni 12.5 %
Mo 0.1 %
Cu 0.1 %
Ferrite 16 FN
As Welded 75% Ar / 25% CO2  
C 0.03 %
Mn 1.3 %
Si 0.9 %
Cr 24 %
Ni 12.5 %
Mo 0.1 %
Cu 0.1 %
Ferrite 18 FN

Part No.

309L
Part No. Model / Product Description UPC
252200068 SB 309L 045X33#PSP VP 662303007522
252200076 SB 309L 1/16X33#PSP VP 662303007539
252200126 SB 309L 1/16X50#CL 662303007560
252200258 SB 309L 045X15#PSP VP/60CT 662303007638
252200324 SB 309L 045X10#PSP VP/60CT 662303007652
252200324-02 SB 309L 045X10#PSP VP/60CT 662303060053
252200415 SB 309L 035X33#PSP VP 662303007713
252200431 SB 309L 035X10#PSP VP/60CT 662303007737

SAW

Accessories

Depositions/Paramaters

Deposition Table
Diameter Amps Volts Wire Feed Speed Deposition Rate Efficiency Electrical Stickout
.035 in, 0.9 mm 100 A 23 265 ipm, 6.7 cm/min 2.9 lbs./hr., 1.3 kg./hr. 83.9 % 1/2 - 1 inches, 12.5 - 25 mm
120 A 23 315 ipm, 8 cm/min 3.4 lbs./hr., 1.5 kg./hr. 81.4 % 1/2 - 1 inches, 12.5 - 25 mm
140 A 25 405 ipm, 10.3 cm/min 4.6 lbs./hr., 2.1 kg./hr. 82.6 % 1/2 - 1 inches, 12.5 - 25 mm
170 A 26 530 ipm, 13.5 cm/min 5.7 lbs./hr., 2.6 kg./hr. 81.8 % 1/2 - 1 inches, 12.5 - 25 mm
.045 in, 1.2 mm 130 A 25 227 ipm, 5.8 cm/min 4.25 lbs./hr., 1.9 kg./hr. 84 % 1/2 - 1 inches, 12.5 - 25 mm
165 A 26 341 ipm, 8.7 cm/min 6.14 lbs./hr., 2.8 kg./hr. 83 % 1/2 - 1 inches, 12.5 - 25 mm
190 A 28 445 ipm, 11.3 cm/min 8.08 lbs./hr., 3.7 kg./hr. 84 % 1/2 - 1 inches, 12.5 - 25 mm
220 A 30 567 ipm, 14.4 cm/min 10.24 lbs./hr., 4.6 kg./hr. 84 % 1/2 - 1 inches, 12.5 - 25 mm
1/16 in, 1.6 mm 170 A 25 154 ipm, 3.9 cm/min 5.34 lbs./hr., 2.4 kg./hr. 83 % 1/2 - 1 inches, 12.5 - 25 mm
210 A 27 193 ipm, 4.9 cm/min 6.89 lbs./hr., 3.1 kg./hr. 82.5 % 1/2 - 1 inches, 12.5 - 25 mm
250 A 28 243 ipm, 6.2 cm/min 8.57 lbs./hr., 3.9 kg./hr. 83 % 1/2 - 1 inches, 12.5 - 25 mm
300 A 29 321 ipm, 8.2 cm/min 11.43 lbs./hr., 5.2 kg./hr. 83 % 1/2 - 1 inches, 12.5 - 25 mm

Extra Info

Shielding Gas

75%Ar / 25%CO2 or 100%CO2

Complementary Products

Seismic Data

All listed prices are in U.S. dollars and represent the Manufacturer's Suggested Retail Price (MSRP) for sale in the United States. Actual selling price will be determined by the Distributor. Prices are subject to change without notice.