SHIELD-BRIGHT 316L X-tra

Shield-Bright 316L X-tra was developed to maximize performance in the flat and horizontal positions when improved corrosion resistance is needed on 316 and 316L steels.

Features

Shield-Bright 316L X-tra was developed for the welding Type 316L stainless steel and also can be used for the other stainless steels including Types 316 and 304L. In a few cases, e.g. nitric acid service, Shield-Bright 316L X-tra should not be used to weld 304L. It was designed specifically for applications where the service environment can produce pitting corrosion.

Shield-Bright 316L X-tra was developed for welding in the flat position and for horizontal fillet welds with flat to concave beads with excellent slag removal.

* This item is subject to Industry Alloy Surcharges

Shield-Bright 316L X-tra
  • Industry
  • Pulp and Paper
  • General Fabrication
  • Process
  • Shipbuilding
  • Welding Process
  • FCAW (Flux Core)

Classifications

  • Classifications/Approvals

    • ASME II SFA 5.22 E316LT0-1
    • AWS A5.22; E316LT0-1/T0-4
    • Certified by CWB to AWS
    • DEUTSCHE BAHN
    • MIL-STD-1689 APPLICATIONS-NAVY
    • TUV
    • ABS - AWS A5.22; E316LT0-1
    • ASME IX F No. 6

Properties

Typical Properties
As Welded using 75% Ar - 25% CO2  
Tensile Strength 65 ksi, 450 MPa
Yield Strength 85 ksi, 580 MPa
Elongation in 2" 36 %
Typical Undiluted Weld Metal Analysis  
100% CO2  
C 0.03%
Mn 1.2%
Si 0.6%
Cr 18.5%
Ni 12%
Mo 2.7%
Cu 0.15%
Ferrite 7 FN
75% Ar / 25% CO2  
C 0.03%
Mn 1.3%
Si 0.6%
Cr 19%
Ni 12%
Mo 2.7%
Cu 0.15%
Ferrite 8 FN

Part No.

316L X-tra
Part No. Model / Product Description UPC
252201611 SBX 316L 1/16X50#CL 662303052102
252201660 SBX 316L 045X33#PSP VP 662303052898
252201678 SBX 316L 1/16X33#PSP VP 662303052904
252202668 SBX 316L 045X10#PSP VP/60CT 662303055073

SAW

Accessories

Depositions/Paramaters

Deposition Table
Diameter Amps Volts Wire Feed Speed Deposition Rate Efficiency Electrical Stickout
.035 in, 0.9 mm 120 A 23 315 ipm, 8 cm/min 3.4 lbs./hr., 1.5 kg./hr. 81.4 % 1/2 - 1 inches, 12.5 - 25 mm
140 A 25 405 ipm, 10.3 cm/min 4.6 lbs./hr., 2.1 kg./hr. 82.6 % 1/2 - 1 inches, 12.5 - 25 mm
170 A 26 530 ipm, 13.5 cm/min 5.7 lbs./hr., 2.6 kg./hr. 81.8 % 1/2 - 1 inches, 12.5 - 25 mm
.045 in, 1.2 mm 150 A 25 259 ipm, 6.6 cm/min 5 lbs./hr., 2.3 kg./hr. 83.9 % 1/2 - 1 inches, 12.5 - 25 mm
200 A 29 410 ipm, 10.4 cm/min 7.7 lbs./hr., 3.5 kg./hr. 84.2 % 1/2 - 1 inches, 12.5 - 25 mm
300 A 33 860 ipm, 21.9 cm/min 16.9 lbs./hr., 7.7 kg./hr. 87 % 1/2 - 1 inches, 12.5 - 25 mm
1/16 in, 1.6 mm 200 A 25 172 ipm, 4.4 cm/min 6.7 lbs./hr., 3.1 kg./hr. 83.6 % 1/2 - 1 inches, 12.5 - 25 mm
400 A 33 495 ipm, 12.58 cm/min 18.9 lbs./hr., 8.6 kg./hr. 85.5 % 1/2 - 1 inches, 12.5 - 25 mm

Extra Info

Shielding Gas

75%Ar / 25%CO2 or 100%CO2