Shield-Bright 317L X-tra was developed to maximize performance in the flat and horizontal position when the addition of molybdenum improves corrosion resistance.
Shield-Bright 317L X-tra was developed for welding type 317 and 317L stainless where additional corrosion resistance that type 316L cannot provide. Carbon content 0.04% maximum.
Shield-Bright 317L X-tra was designed for welding in the flat position and for horizontal fillet welds with flat to concave beads with excellent slag removal.
* This item is subject to Industry Alloy Surcharges

| As Welded using 75% Ar - 25% CO2 | |
|---|---|
| Tensile Strength | 70 ksi, 480 MPa |
| Yield Strength | 90 ksi, 580 MPa |
| Elongation in 2" | 35 % |
| Typical Undiluted Weld Metal Analysis | |
| 100% CO2 | |
| C | 0.03% |
| Mn | 1.4% |
| Si | 0.6% |
| Cr | 19% |
| Ni | 12% |
| Mo | 3.5% |
| Cu | 0.15% |
| Ferrite | 9 FN |
| 75% Ar / 25% CO2 | |
| C | 0.03% |
| Mn | 1.5% |
| Si | 0.65% |
| Cr | 19% |
| Ni | 12.5% |
| Mo | 3.5% |
| Cu | 0.15% |
| Ferrite | 9 FN |
| Part No. | Model / Product Description | UPC |
|---|---|---|
| 252201223 | SBX 317L 045X33#PSP VP | 662303015640 |
| Diameter | Amps | Volts | Wire Feed Speed | Deposition Rate | Efficiency | Electrical Stickout |
|---|---|---|---|---|---|---|
| .035 in, 0.9 mm | 120 A | 23 | 315 ipm, 8 cm/min | 3.4 lbs./hr., 1.5 kg./hr. | 81.4 % | 1/2 - 1 inches, 12.5 - 25 mm |
| 140 A | 25 | 405 ipm, 10.3 cm/min | 4.6 lbs./hr., 2.1 kg./hr. | 82.6 % | 1/2 - 1 inches, 12.5 - 25 mm | |
| 170 A | 26 | 530 ipm, 13.5 cm/min | 5.7 lbs./hr., 2.6 kg./hr. | 81.8 % | 1/2 - 1 inches, 12.5 - 25 mm | |
| .045 in, 1.2 mm | 150 A | 25 | 259 ipm, 6.6 cm/min | 5 lbs./hr., 2.3 kg./hr. | 83.9 % | 1/2 - 1 inches, 12.5 - 25 mm |
| 200 A | 29 | 410 ipm, 10.4 cm/min | 7.7 lbs./hr., 3.5 kg./hr. | 84.2 % | 1/2 - 1 inches, 12.5 - 25 mm | |
| 300 A | 33 | 860 ipm, 21.9 cm/min | 16.9 lbs./hr., 7.7 kg./hr. | 87 % | 1/2 - 1 inches, 12.5 - 25 mm | |
| 1/16 in, 1.6 mm | 200 A | 25 | 172 ipm, 4.4 cm/min | 6.7 lbs./hr., 3.1 kg./hr. | 83.6 % | 1/2 - 1 inches, 12.5 - 25 mm |
| 240 A | 28 | 225 ipm, 5.7 cm/min | 8.1 lbs./hr., 3.7 kg./hr. | 83.6 % | 1/2 - 1 inches, 12.5 - 25 mm | |
| 400 A | 33 | 495 ipm, 12.58 cm/min | 18.9 lbs./hr., 8.6 kg./hr. | 85.5 % | 1/2 - 1 inches, 12.5 - 25 mm |
75%Ar / 25%CO2 or 100%CO2