Print this page

SHIELD-BRIGHT 317L

Shield-Bright 317 was developed for out-of-position welding when the addition of Molybdenum improves corrosion resistance.

Features

Shield-Bright 317L is recommended for welding Type 317 and 317L stainless steel. It can also be used for Type 316L where additonal weld metal corrosion resistance, including pitting resistance, is required.This is used in industries where there is severe corrosion applications involving sulfuric and sulfurous acids and their salts.

Shield-Bright 317L was developed for welding in all position

* This item is subject to Industry Alloy Surcharges

Shield-Bright 317L
  • Industry
  • Pulp and Paper
  • Shipbuilding
  • Process
  • General Fabrication
  • Welding Process
  • FCAW (Flux Core)

Classifications

  • Classifications/Approvals

    • AWS A5.22; E317LT1-1/T1-4
    • ASME II SFA 5.22 E317LT1-1/LT1-4
    • ASME IX F No. 6

Properties

Typical Properties
As Welded using 75% Ar - 25% CO2  
Tensile Strength 70 ksi, 480 MPa
Yield Strength 90 ksi, 620 MPa
Elongation in 2" 35 %
Typical Undiluted Weld Metal Analysis  
75% Ar / 25% CO2  
C 0.03%
Mn 1.2%
Si 0.85%
Cr 19.5%
Ni 13%
Mo 3.5%
Cu 0.15%
Ferrite 9 FN

Part No.

317L
Part No. Model / Product Description UPC
252200159 SB 317L 045X33#PSP VP 662303007584

SAW

Accessories

Depositions/Paramaters

Deposition Table
Diameter Amps Volts Wire Feed Speed Deposition Rate Efficiency Electrical Stickout
.035 in, 0.9 mm 100 A 23 265 ipm, 6.7 cm/min 2.9 lbs./hr., 1.3 kg./hr. 83.9 % 1/2 - 1 inches, 12.5 - 25 mm
120 A 23 315 ipm, 8 cm/min 3.4 lbs./hr., 1.5 kg./hr. 81.4 % 1/2 - 1 inches, 12.5 - 25 mm
140 A 25 405 ipm, 10.3 cm/min 4.6 lbs./hr., 2.1 kg./hr. 82.6 % 1/2 - 1 inches, 12.5 - 25 mm
170 A 26 530 ipm, 13.5 cm/min 5.7 lbs./hr., 2.6 kg./hr. 81.8 % 1/2 - 1 inches, 12.5 - 25 mm
.045 in, 1.2 mm 130 A 25 227 ipm, 5.8 cm/min 4.25 lbs./hr., 1.9 kg./hr. 84 % 1/2 - 1 inches, 12.5 - 25 mm
165 A 26 341 ipm, 8.7 cm/min 6.14 lbs./hr., 2.8 kg./hr. 83 % 1/2 - 1 inches, 12.5 - 25 mm
190 A 28 445 ipm, 11.3 cm/min 8.08 lbs./hr., 3.7 kg./hr. 84 % 1/2 - 1 inches, 12.5 - 25 mm
220 A 30 567 ipm, 14.4 cm/min 10.24 lbs./hr., 4.6 kg./hr. 84 % 1/2 - 1 inches, 12.5 - 25 mm
1/16 in, 1.6 mm 170 A 25 154 ipm, 3.9 cm/min 5.34 lbs./hr., 2.4 kg./hr. 83 % 1/2 - 1 inches, 12.5 - 25 mm
210 A 27 193 ipm, 4.9 cm/min 6.89 lbs./hr., 3.1 kg./hr. 82.5 % 1/2 - 1 inches, 12.5 - 25 mm
250 A 28 243 ipm, 6.2 cm/min 8.57 lbs./hr., 3.9 kg./hr. 83 % 1/2 - 1 inches, 12.5 - 25 mm
300 A 29 321 ipm, 8.2 cm/min 11.43 lbs./hr., 5.2 kg./hr. 83 % 1/2 - 1 inches, 12.5 - 25 mm

Extra Info

Shielding Gas

75%Ar / 25%CO2 or 100%CO2

Complementary Products

Seismic Data