Shield-Bright 347H was developed for out-of-position welding when required in high temperature service on type 347.
Shield-Bright 347H was developed for the welding of stainless steel Types 321 and 347 where a minimum of 0.04% carbon is required. As with all 347 weld metals, for service at temperatures greater than 1000ºF (550ºC) it can be used in circumstances of lower stress and advisedly under creep conditions. Shield-Bright 347H can also be used for the welding of Types 302 and 304 stainless steels.
Shield-Bright 347H was developed for welding in all positions and performs particularly well in the vertical position with excellent slag removal.
* This item is subject to Industry Alloy Surcharges

| As Welded 75% Ar / 25% CO2 | |
|---|---|
| Tensile Strength | 95 ksi, 650 MPa |
| Yield Strength | 75 ksi, 520 MPa |
| Elongation in 2" | 35 % |
| Typical Undiluted Weld Metal Analysis | |
| As Welded 75% Ar / 25% CO2 | |
| C | 0.045 % |
| Mn | 1.1 % |
| Si | 0.85 % |
| Cr | 19.5 % |
| Ni | 9.7 % |
| Mo | 0.1 % |
| Cu | 0.5 % |
| Nb | 0.1 % |
| Ferrite | 6 FN |
| Part No. | Model / Product Description | UPC |
|---|---|---|
| 252201587 | SB 347H 045X33#PSP VP | 662303052010 |
| Diameter | Amps | Volts | Wire Feed Speed | Deposition Rate | Efficiency | Electrical Stickout |
|---|---|---|---|---|---|---|
| .035 in, 0.9 mm | 100 A | 23 | 265 ipm, 6.7 cm/min | 2.9 lbs./hr., 1.3 kg./hr. | 83.9 % | 1/2 - 1 inches, 12.5 - 25 mm |
| 120 A | 23 | 315 ipm, 8 cm/min | 3.4 lbs./hr., 1.5 kg./hr. | 81.4 % | 1/2 - 1 inches, 12.5 - 25 mm | |
| 140 A | 25 | 405 ipm, 10.3 cm/min | 4.6 lbs./hr., 2.1 kg./hr. | 82.6 % | 1/2 - 1 inches, 12.5 - 25 mm | |
| 170 A | 26 | 530 ipm, 13.5 cm/min | 5.7 lbs./hr., 2.6 kg./hr. | 81.8 % | 1/2 - 1 inches, 12.5 - 25 mm | |
| .045 in, 1.2 mm | 130 A | 25 | 227 ipm, 5.8 cm/min | 4.25 lbs./hr., 1.9 kg./hr. | 84 % | 1/2 - 1 inches, 12.5 - 25 mm |
| 165 A | 26 | 341 ipm, 8.7 cm/min | 6.14 lbs./hr., 2.8 kg./hr. | 83 % | 1/2 - 1 inches, 12.5 - 25 mm | |
| 190 A | 28 | 445 ipm, 11.3 cm/min | 8.08 lbs./hr., 3.7 kg./hr. | 84 % | 1/2 - 1 inches, 12.5 - 25 mm | |
| 220 A | 30 | 567 ipm, 14.4 cm/min | 10.24 lbs./hr., 4.6 kg./hr. | 84 % | 1/2 - 1 inches, 12.5 - 25 mm | |
| 1/16 in, 1.6 mm | 170 A | 25 | 154 ipm, 3.9 cm/min | 5.34 lbs./hr., 2.4 kg./hr. | 83 % | 1/2 - 1 inches, 12.5 - 25 mm |
| 210 A | 27 | 193 ipm, 4.9 cm/min | 6.89 lbs./hr., 3.1 kg./hr. | 82.5 % | 1/2 - 1 inches, 12.5 - 25 mm | |
| 250 A | 28 | 243 ipm, 6.2 cm/min | 8.57 lbs./hr., 3.9 kg./hr. | 83 % | 1/2 - 1 inches, 12.5 - 25 mm | |
| 300 A | 29 | 321 ipm, 8.2 cm/min | 11.43 lbs./hr., 5.2 kg./hr. | 83 % | 1/2 - 1 inches, 12.5 - 25 mm |
75%Ar / 25%CO2 or 100%CO2
All listed prices are in U.S. dollars and represent the Manufacturer's Suggested Retail Price (MSRP) for sale in the United States. Actual selling price will be determined by the Distributor. Prices are subject to change without notice.