CRYO-SHIELD 308L

Cryo-Shield 308L is an all-position stainless steel cored wire designed for low temperature cryogenic applications.

Features

Cryo-Shield 308L is an all-position wire adaptable to a variety of shop and field erection applications. The use of argon/CO2 gas shielding is recommended for maximum toughness. Designed for cryogenic applications where good weld metal toughness is required. Applications include cryogenic vessel fabrication and process piping repair. Cyro-Shield 308L is guaranteed to produce a minimum of 15mils lateral expansion at -320ºF.

Cryo-Shield 308L was developed for the welding of types 304 & 304L stainless steels for the low temperature service, even down to liquid helium temperatures. This is done by controlling the composition and the ferrite content to give good toughness at temperatures of -320ºF (-196ºC) and lower.

Cryo-Shield 308L was developed for welding in all positions and performs particularly well in the vertical position with excellent slag removal.

* This item is subject to Industry Alloy Surcharges

Cryo-Shield 308L
  • Industry
  • Pipeline
  • General Fabrication
  • Process
  • Petrochemical
  • Welding Process
  • FCAW (Flux Core)

Classifications

  • Classifications/Approvals

    • ASME IX F No. 6
    • ASME II SFA 5.22 E308LT1-1/T1-4
    • AWS A5.22; E308LT1-1/T1-4

Properties

Typical Properties
As Welded using 75% Ar - 25% CO2  
Tensile Strength 80 ksi, 550 MPa
Yield Strength 65 ksi, 450 MPa
Elongation in 2" 45 %
Typical Undiluted Weld Metal Analysis  
75% Ar / 25% CO2  
C 0.03%
Mn 1.3%
Si 0.8%
Cr 19%
Ni 10.7%
Mo 0.1%
Cu 0.15%
Ferrite 4% FN

Part No.

308L
Part No. Model / Product Description UPC
252210000 CRYO-SH 308L 045X33#PSP VP 662303034832
252210026 CRYO-SH 308L 035X33#PSP VP 662303036140

SAW

Accessories

Depositions/Paramaters

Deposition Table
Diameter Amps Volts Wire Feed Speed Deposition Rate Efficiency
.035 in, 0.9 mm 100 A 23 265 ipm, 6.7 cm/min 2.9 lbs./hr., 1.3 kg./hr. 83.9 %
120 A 23 315 ipm, 8.0 cm/min 3.4 lbs./hr., 1.5 kg./hr. 81.4 %
140 A 25 405 ipm, 10.3 cm/min 4.6 lbs./hr., 2.1 kg./hr. 82.6 %
170 A 26 530 ipm, 13.5 cm/min 5.7 lbs./hr., 2.6 kg./hr. 81.8 %
.045 in, 1.2 mm 130 A 25 227 ipm, 5.8 cm/min 4.25 lbs./hr., 1.9 kg./hr. 84.0 %
165 A 26 341 ipm, 8.7 cm/min 6.14 lbs./hr., 2.8 kg./hr. 83.0 %
190 A 28 445 ipm, 11.3 cm/min 8.08 lbs./hr., 3.7 kg./hr. 84.0 %
220 A 30 567 ipm, 14.4 cm/min 10.24 lbs./hr., 4.6 kg./hr. 84.0 %
.062 in, 1.6 mm 170 A 25 154 ipm, 3.9 cm/min 5.34 lbs./hr., 2.4 kg./hr. 83.0 %
210 A 27 193 ipm, 4.9 cm/min 6.89 lbs./hr., 3.1 kg./hr. 82.5 %
250 A 28 243 ipm, 6.2 cm/min 8.57 lbs./hr., 3.9 kg./hr. 83.0 %
300 A 29 321 ipm, 8.2 cm/min 11.43 lbs./hr., 5.2 kg./hr. 83.0 %

Extra Info

Shielding Gas

75-80% Ar/Bal CO2