Coreshield 15 is an all-position self-shielded flux cored welding wire for single pass applications. It produces smooth arc action, full slag coverage, easy slag removal and low spatter.
Coreshield 15 is an all-position self-shielded flux cored welding wire for single pass applications. Coreshield 15 produces smooth arc action, full slag coverage, easy slag removal, and low spatter. The use of DCEN (electrode negative) current minimizes the risk of burn-through. Coreshield 15 is excellent for use on lap and fillet welds on thin gauge galvanized and mild steels in all welding positions. The availability of .030" (0.8 mm) diameter makes it possible to use this product on materials as thin as 18 gauge (1.22 mm). The wire is particularly suitable for thin gauge materials 0.030 - 3/16" (0.8-4.8 in.) in galvanised, zinc-aluminum carbon, or aluminised carbon steels. In structural fabrications, the product can be used where no seismic requirements are present.

| As Welded | |
|---|---|
| Transverse Tensile Strength | 89 ksi, 615 MPa |
| Longitudinal Guided Bend Test | Satisfactory |
| Typical Undiluted Weld Metal Analysis | |
| C | 0.23 % |
| Mn | 0.7 % |
| Si | 0.4 % |
| P | 0.007 % |
| S | 0.01 % |
| Al | 2 % |
| Part No. | Model / Product Description | UPC |
|---|---|---|
| 242201606 | CS 15 035X33#AWS | 662303000554 |
| 242201614 | CS 15 045X33#AWS | 662303000561 |
| 242201630 | CS 15 1/16X33#AWS | 662303000585 |
| 242201648 | CS 15 035X10#PSP | 662303000592 |
| 242201655 | CS 15 045X10#PSP | 662303000608 |
| 242201663 | CS 15 1/16X10#PSP | 662303000615 |
| 242201671 | CS 15 1/16X50#CL | 662303000622 |
| 242201689 | CS 15 5/64X50#CL | 662303000639 |
| 242201812 | CS 15 030X10#PSP | 662303000745 |
| 242201820 | CS 15 035X2#4 SP | |
| 242201838 | CS 15 030X2#4 SP | |
| 242201853 | CS 15 030X1#4 SP | 662303048044 |
| 242201945 | CS 15 030X33#AWS | 662303000776 |
| 242202190 | CS 15 030X500#RL | 662303000905 |
| 242206001 | CS 15 035X500#RL | 662303001667 |
| 242206019 | CS 15 045X650#RL | 662303001674 |
| 242206035 | CS 15 045X450#MP | 662303001698 |
| 242206068 | CS 15 1/16X500#MP | 662303009113 |
| 242206076 | CS 15 052X450#MP | 662303029500 |
| 242202224 | CS 15 030X15#PSP | 662303081508 |
| 242202232 | CS 15 035X15#PSP | 662303081515 |
| 242202240 | CS 15 045X15#PSP | 662303081522 |
| 242203644 | CS 15 045X600#OMP | 662303079338 |
| 242203651 | CS 15 052X600#OMP | 662303079345 |
| 242203669 | CS 15 1/16X600#OMP | 662303079352 |
| Diameter | Amps | Volts | Wire Feed Speed | Deposition Rate | Efficiency | Electrical Stickout |
|---|---|---|---|---|---|---|
| .035 in, 0.9 mm | 80 A A | 15 | 81 ipm, 206 cm/min | .9 lbs./hr., .41 kg./hr. | 75 % | 3/8 inches, 9.5 mm |
| 120 A A | 17 | 155 ipm, 394 cm/min | 1.7 lbs./hr., .77 kg./hr. | 77 % | 3/8 inches, 9.5 mm | |
| 200 A A | 17 | 392 ipm, 995 cm/min | 4.5 lbs./hr., 2.04 kg./hr. | 81 % | 3/8 inches, 9.5 mm | |
| .045 in, 1.2 mm | 95 A A | 15 | 54 ipm, 137 cm/min | .9 lbs./hr., .41 kg./hr. | 74 % | 1/2 inches, 12.7 mm |
| 150 A A | 17 | 118 ipm, 300 cm/min | 2.1 lbs./hr., .95 kg./hr. | 79 % | 1/2 inches, 12.7 mm | |
| 225 A A | 18 | 140 ipm, 356 cm/min | 2.6 lbs./hr., 1.18 kg./hr. | 82 % | 1/2 inches, 12.7 mm | |
| 1/16 in, 1.6 mm | 160 A A | 17 | 56 ipm, 142 cm/min | 2.1 lbs./hr., .95 kg./hr. | 78 % | 5/8 inches, 15.9 mm |
| 200 A A | 18 | 76 ipm, 193 cm/min | 2.9 lbs./hr., 1.32 kg./hr. | 80 % | 5/8 inches, 15.9 mm | |
| 275 A A | 19 | 132 ipm, 335 cm/min | 5.2 lbs./hr., 2.35 kg./hr. | 81 % | 5/8 inches, 15.9 mm | |
| 5/64 in, 2.0 mm | 185 A A | 19 | 50 ipm, 127 cm/min | 2.4 lbs./hr., 1.09 kg./hr. | 77 % | 1 inches, 25.4 mm |
| 250 A A | 20 | 91 ipm, 231 cm/min | 4.5 lbs./hr., 2.04 kg./hr. | 79 % | 1 inches, 25.4 mm | |
| 300 A A | 21 | 135 ipm, 343 cm/min | 6.6 lbs./hr., 2.99 kg./hr. | 81 % | 1 inches, 25.4 mm |
Coreshield 15 contains barium and fluoride compounds. The limit for soluble barium may be reached before the general fume limit of 5 mg/m3 is reached. Consult MSDS for more information.