Print this page

CORESHIELD 11

Coreshield 11 Coreshield 11 is an all-position self-shielded flux-cored welding wire excellent for use on single or multiple pass lap, fillet and butt welds in all positions.

Features

Coreshield 11 is an all-position self-shielded flux cored welding wire meeting all requirements for the E71T-11 classification.Coreshield 11 is excellent for use on single or multiple pass lap, fillet and butt welds on mild steels in all welding positions. Limitations do exist for multipass welds in excess of 3/8" (9.5 mm). It produces smooth arc action, full slag coverage, easy slag removal, and low spatter. This product should find excellent acceptance in general purpose mild steel fabrication. In structural fabrication, the product can be used where no seismic requirements are present. Coreshield 11 is run DCEN.

Coreshield 11
  • Industry
  • Civil Construction
  • General Fabrication
  • Automotive
  • Welding Process
  • FCAW (Flux Core)

Classifications

  • Classifications/Approvals

    • ASME SFA 5.20
    • A.B.S.- AWS A5.20; E71T-11
    • Certified by CWB to CSA W48
    • AWS A5.20; E71T-11

Properties

Typical Properties
As Welded  
Yield Strength 63 ksi, 435 MPa
Tensile Strength 90 ksi, 620 MPa
Elongation in 2" 22 %
Typical Undiluted Weld Metal Analysis  
C 0.25 %
Mn 0.7 %
Si 0.4 %
P 0.01 %
S 0.01 %
Al 1.6 %

Part No.

11
Part No. Model / Product Description UPC
242201408 CS 11 045X33#AWS 662303000400
242201416 CS 11 5/64X25#AWS 662303000417
242201424 CS 11 1/16X33#AWS 662303000424
242201440 CS 11 045X10#PSP 662303000431
242201465 CS 11 1/16X10#PSP 662303000448
242201473 CS 11 5/64X50#CL 662303000455
242201481 CS 11 1/16X450#MP 662303068394
242201499 CS 11 045X500#OMP 662303077600
242201515 CS 11 1/16X50#CL 662303000462
242203503 CS 11 035X33#PSP 662303001414
242203511 CS 11 035X10#PSP 662303001421
242203552 CS 11 3/32X50#CL 662303051204
242203636 CS 11 1/16X600#OMP 662303079369

SAW

Accessories

Depositions/Paramaters

Deposition Table
Diameter Amps Volts Wire Feed Speed Deposition Rate Efficiency Electrical Stickout
.035 in, 0.9 mm 80 A A 15 81 ipm, 206 cm/min .9 lbs./hr., .41 kg./hr. 75 % 3/8 inches, 9.5 mm
120 A A 17 155 ipm, 394 cm/min 1.7 lbs./hr., .77 kg./hr. 77 % 3/8 inches, 9.5 mm
200 A A 17 392 ipm, 995 cm/min 4.5 lbs./hr., 2.04 kg./hr. 81 % 3/8 inches, 9.5 mm
.045 in, 1.2 mm 95 A A 15 54 ipm, 137 cm/min .9 lbs./hr., .41 kg./hr. 74 % 1/2 inches, 12.7 mm
150 A A 17 118 ipm, 300 cm/min 2.1 lbs./hr., .95 kg./hr. 79 % 1/2 inches, 12.7 mm
225 A A 18 140 ipm, 356 cm/min 2.6 lbs./hr., 1.18 kg./hr. 82 % 1/2 inches, 12.7 mm
1/16 in, 1.6 mm 160 A A 17 56 ipm, 142 cm/min 2.1 lbs./hr., .95 kg./hr. 78 % 5/8 inches, 15.9 mm
200 A A 18 76 ipm, 193 cm/min 2.9 lbs./hr., 1.32 kg./hr. 80 % 5/8 inches, 15.9 mm
275 A A 19 132 ipm, 335 cm/min 5.2 lbs./hr., 2.35 kg./hr. 81 % 5/8 inches, 15.9 mm
5/64 in, 2.0 mm 185 A A 19 50 ipm, 127 cm/min 2.4 lbs./hr., 1.09 kg./hr. 77 % 1 inches, 25.4 mm
250 A A 20 91 ipm, 231 cm/min 4.5 lbs./hr., 2.04 kg./hr. 79 % 1 inches, 25.4 mm
300 A A 21 135 ipm, 343 cm/min 6.6 lbs./hr., 2.99 kg./hr. 81 % 1 inches, 25.4 mm

Extra Info

Certified to ISO 17632-B-T49ZT11-1NA

Procedure

  • Coreshield 11 contains fluoride and barium compounds. The limit for soluble barium may be reached before the general fume limit of 5 mg/m3 is reached. Consult MSDS for more information.

Complementary Products