Coreshield 10 is a self-shielded flux cored welding wire designed for high speed single pass welding of thin gauge carbon, aluminized and galvanized steels.
Coreshield 10 is a self-shielded flux cored welding wire designed for high speed single pass welding of thin gauge carbon, aluminized and galvanized steels. Its low spatter and excellent bead appearance makes it an ideal choice for high production applications. The use of DCEN (electrode negative) minimizes the risk of burn-through. High deposition efficiencies make it an ideal choice for automation. Coreshield 10 produces good wetting characteristics at high speeds making it suitable for robotic applications. It is designed to be used on automotive components, semi-trailer frames and axles, hot water tanks and door frames.

| As Welded | |
|---|---|
| Transverse Tensile Strength | 92 ksi, 635 MPa |
| Longitudinal Guided Bend Test | Satisfactory |
| Typical Undiluted Weld Metal Analysis | |
| C | 0.05 % |
| Mn | 1.4 % |
| Si | 0.3 % |
| P | 0.015 % |
| S | 0.02 % |
| Al | 1.0 % |
| Ti | 1.0 % |
| Diameter | Amps | Volts | Wire Feed Speed | Deposition Rate | Efficiency | Electrical Stickout |
|---|---|---|---|---|---|---|
| .045 in, 1.2 mm | 80 A A | 13 | 60 ipm, 152 cm/min | 1.1 lbs./hr., .50 kg./hr. | 76 % | 1/2 inches, 12.7 mm |
| 150 A A | 17 | 118 ipm, 300 cm/min | 2.6 lbs./hr., 1.18 kg./hr. | 88 % | 1/2 inches, 12.7 mm | |
| 225 A A | 18 | 226 ipm, 574 cm/min | 5.1 lbs./hr., 2.31 kg./hr. | 90 % | 1/2 inches, 12.7 mm | |
| 1/16 in, 1.6 mm | 175 A A | 14 | 61 ipm, 155 cm/min | 2.1 lbs./hr., .95 kg./hr. | 73 % | 1/2 inches, 12.7 mm |
| 220 A A | 18 | 78 ipm, 198 cm/min | 3.3 lbs./hr., 1.50 kg./hr. | 83 % | 1/2 inches, 12.7 mm | |
| 275 A A | 19 | 108 ipm, 274 cm/min | 4.8 lbs./hr., 2.18 kg./hr. | 93 % | 1/2 inches, 12.7 mm | |
| 5/64 in, 2.0 mm | 250 A A | 20 | 58 ipm, 147 cm/min | 4.0 lbs./hr., 1.81 kg./hr. | 94 % | 3/4 inches, 19.1 mm |
| 300 A A | 21 | 85 ipm, 216 cm/min | 5.1 lbs./hr., 2.31 kg./hr. | 85 % | 3/4 inches, 19.1 mm | |
| 400 A A | 27 | 143 ipm, 363 cm/min | 9.2 lbs./hr., 4.17 kg./hr. | 90 % | 3/4 inches, 19.1 mm |
All listed prices are in U.S. dollars and represent the Manufacturer's Suggested Retail Price (MSRP) for sale in the United States. Actual selling price will be determined by the Distributor. Prices are subject to change without notice.