CORESHIELD 8Ni1

Coreshield 8-Ni1 is a self-shielded flux-cored wire designed to produce welds with outstanding impact toughness at temperatures as low as -60°F (-51°C).

Features

Coreshield 8-Ni1 is a self-shielded flux cored wire designed to produce welds with outstanding impact toughness at temperatures as low as -60°F (-51°C). It is suitable for all position welding including vertical down, and is especially suited for making root passes or handling poor fit up. It should only be run on DCEN (electrode negative). Coreshield 8-Ni1 can be used for welding offshore structures, bridges, storage tanks, and other applications where excellent impact toughness is specified and where self-shielding provides an advantage. It is also good for weathering grades of steels where color match is an important consideration.

Coreshield 8-Ni1
  • Industry
  • Shipbuilding
  • General Fabrication
  • Mobile Machinery
  • Civil Construction
  • Bridge Construction
  • Welding Process
  • FCAW (Flux Core)

Classifications

  • Classifications/Approvals

    • AWS A5.29; E70T-8Ni1 (equal to or greater than 3/32)
    • AWS A5.29; E71T-8Ni1 (equal to or smaller than 5/64)
    • ASME SFA 5.29

Properties

Typical Properties
As Welded  
Yield Strength 61 ksi, 425 MPa
Tensile Strength 76 ksi, 525 MPa
Elongation in 2" 30 %
Typical Charpy V-Notch Impact Properties  
Testing Temperature -20ºF (-29ºC) 119 ft.-lbs., 161 J
Testing Temperature -60ºF (-51ºC) 82 ft.-lbs., 111 J
Typical Undiluted Weld Metal Analysis  
C 0.04 %
Mn 1.3 %
Si 0.3 %
P 0.013 %
S 0.008 %
Ni 1.1 %
Al 0.8 %

Part No.

8-Ni1
Part No. Model / Product Description UPC
242203008 CS 8-NI1 5/64X50#CL 662303001353
242203032 CS 8-NI1 1/16X33#AWS 662303012823
242203040 CS 8-NI1 5/64X25#AWS 662303012946
242203057 CS 8-NI1 1/16X15#PSP 662303012847
242203065 CS 8-NI1 5/64X15#PSP 662303012854

SAW

Accessories

Depositions/Paramaters

Deposition Table
Diameter Amps Volts Wire Feed Speed Deposition Rate Efficiency Electrical Stickout
1/16 in, 1.6 mm 135 A 20 100 ipm, 254 cm/min 2.9 lbs./hr., 1.3 kg./hr. 72 % 5/8 inches, 15.9 mm
230 A 22 160 ipm, 406 cm/min 4.7 lbs./hr., 2.1 kg./hr. 74 % 5/8 inches, 15.9 mm
5/64 in, 2.0 mm 170 A 20 65 ipm, 165 cm/min 2.8 lbs./hr., 1.3 kg./hr. 71 % 3/4 inches, 19.1 mm
195 A 22 80 ipm, 203 cm/min 3.4 lbs./hr., 1.5 kg./hr. 72 % 3/4 inches, 19.1 mm
230 A 24 100 ipm, 254 cm/min 4.7 lbs./hr., 2.1 kg./hr. 73 % 3/4 inches, 19.1 mm
Seismic Data
Seismic Data
 

Extra Info

Procedure

Coreshield 8-Ni1 contains barium compounds. The exposure limit for barium may be exceeded before the exposure limit for total fume. Consult MSDS for more information

Complementary Products

Seismic Data

All listed prices are in U.S. dollars and represent the Manufacturer's Suggested Retail Price (MSRP) for sale in the United States. Actual selling price will be determined by the Distributor. Prices are subject to change without notice.