Coreshield 6 is an E70T-6 self-shielded flux-cored wire designed for flat and horizontal welds requiring Charpy V-notch properties. It is tested and certified to meet the new AWS A5.20 ‘D' designation requirements, making it an excellent choice for demand critical welds when FEMA 353, D1.1 or D1.8 Seismic Supplement is utilized.
Coreshield 6 is a high productivity, high deposition gasless flux cored wire. This self-shielded wire is ideal for single or multiple pass weld applications in addition to providing high deposition rates, low spatter, and good penetration. Because of its stiffer weld puddle, Coreshield 6 offers exceptional multi-pass weld stacking characteristics, produces excellent bead appearance and X-ray quality weld deposits.
Coreshield 6 is run DCEP (electrode positive).
Please see Related Links on the right side of this page to download the Seismic Data Sheet and Seismic Certifications.

| As Welded | |
|---|---|
| Yield Strength | 67 ksi, 465 MPa |
| Tensile Strength | 85 ksi, 590 MPa |
| Elongation in 2" | 26 % |
| Typical Charpy V-Notch Impact Properties | |
| Testing Temperature -20ºF (-29ºC) | 31 ft.-lbs., 42 J |
| Typical Undiluted Weld Metal Analysis | |
| C | 0.12 % |
| Mn | 0.8 % |
| Si | 0.2 % |
| P | 0.005 % |
| S | 0.008 % |
| Ni | 0.4 % |
| Al | 0.7 % |
| Part No. | Model / Product Description | UPC |
|---|---|---|
| 242207504 | CS 6 5/64X25#AWS | 662303067670 |
| 242207512 | CS 6 5/64X50#CL | 662303067687 |
| 242207520 | CS 6 3/32X50#CL | 662303067694 |
| 242207538 | CS 6 3/32X25#AWS | 662303070205 |
| 242207546 | CS 6 5/64X22#AWS | 662303070304 |
| 242207553 | CS 6 3/32X22#AWS | 662303070311 |
| 242207587-66 | CS 6 5/64X22#AWS VP | 662303073268 |
| 242207595 | CS 6 3/32X22#AWS VP | 662303071356 |
| 242207595-66 | CS 6 3/32X22#AWS VP | 662303073251 |
| 242207603 | CS 6 5/64X25#AWS VP FEMA | 662303076511 |
| Diameter | Amps | Volts | Wire Feed Speed | Deposition Rate | Efficiency | Electrical Stickout |
|---|---|---|---|---|---|---|
| 5/64 in, 2.0 mm | 275 A | 22 | 150 ipm, 381 cm/min | 6.4 lbs./hr., 2.9 kg./hr. | 78.1 % | 1 inches, 25.4 mm |
| 325 A | 23 | 200 ipm, 508 cm/min | 8.5 lbs./hr., 3.8 kg./hr. | 79.6 % | 1 inches, 25.4 mm | |
| 390 A | 24 | 300 ipm, 762 cm/min | 12.2 lbs./hr., 5.5 kg./hr. | 80.2 % | 1 inches, 25.4 mm | |
| 475 A | 27 | 400 ipm, 1016 cm/min | 16.3 lbs./hr., 7.3 kg./hr. | 80.3 % | 1 inches, 25.4 mm | |
| 535 A | 29 | 500 ipm, 1270 cm/min | 20.7 lbs./hr., 9.3 kg./hr. | 81.2 % | 1 inches, 25.4 mm | |
| 600 A | 31 | 600 ipm, 1524 cm/min | 25.7 lbs./hr., 11.5 kg./hr. | 81.7 % | 1 inches, 25.4 mm | |
| 3/32 in, 2.4 mm | 265 A | 22 | 100 ipm, 254 cm/min | 6.1 lbs./hr., 2.9 kg./hr. | 78.7 % | 1 inches, 25.4 mm |
| 365 A | 23 | 150 ipm, 381 cm/min | 9.3 lbs./hr., 4.2 kg./hr. | 79.8 % | 1 inches, 25.4 mm | |
| 415 A | 23 | 200 ipm, 508 cm/min | 12.5 lbs./hr., 5.6 kg./hr. | 80.9 % | 1 inches, 25.4 mm | |
| 530 A | 26 | 300 ipm, 762 cm/min | 19.0 lbs./hr., 8.5 kg./hr. | 81.8 % | 1 inches, 25.4 mm | |
| 615 A | 29 | 400 ipm, 1016 cm/min | 25.8 lbs./hr., 11.6 kg./hr. | 81.8 % | 1 inches, 25.4 mm |
| Seismic Data |
|---|
All listed prices are in U.S. dollars and represent the Manufacturer's Suggested Retail Price (MSRP) for sale in the United States. Actual selling price will be determined by the Distributor. Prices are subject to change without notice.