ALL-STATE CORECAST 8600

A flux cored tubular welding wire for joining cast iron to itself or to mild steeel. Ideal to use as an overlay and build-up to repair pumps, housings, molds, machine bases and castings. Use with 98%Argon/2% Oxygen shielding gas. Deposits are machinable.

Features

Continuous flux cored DC reverse composite electrode for joining cast iron to itself or mild steel. Use with 98% Argon/2%Oxygen shielding gas.Machinable.

Classifications

Properties

Typical Properties
Typical Mechanical Properties  
Tensile Strength 73 ksi, 505 kgs/mm2
Elongation In 2" 12 %
Color Match Excellent

Part No.

CORE-CAST 8600
Part No. Model / Product Description UPC
69807050 A/S CORE-CAST 8600 045X33#SPL 662393007679
69807051.0000002 A/S CORE-CAST 8600 035X33#SPL 662393007686
69807052 A/S CORE-CAST 8600 045X10#SPL 662393007693
69807053 A/S CORE-CAST 8600 035X10#SPL 662393007709
69807051 A/S CORE-CAST 8600 035X33#SPL 662393007686

SAW

Accessories

Depositions/Paramaters

Extra Info

Core-Cast 8600 is excellent for repair welding on highway vehicles,farm machinery,construction equipment,mining equipment and machine tools. Can be used for joining cast iron to mild steel,repairing damaged castings and overlaying of worn areas on castings,molds and pumps.

Procedure

  • For best results,set wire amperage and adjust voltage for smoothest operation.Use 98% Argon 2% Oxygen shielding gas. Wire will also operate in the short circuiting mode or with pulse arc,and under these conditions,may be usable out-of-position.Observe the usual precautions on preheat,joint preparation,and welding technique used with other cast iron welding processes.Light peening of each bead will reduce internal stresses and minimize cracking tendencies.