An all-position electrode for high strength, dense and sound welds on dirty, oily or grease soaked castings. Deposits will rust to match the base metal. Non-machinable.
An AC/DC reverse all-position electrode for cast iron. For high strength,dense,sound welds where machinability is not needed.Excellent for dirty or grease soaked castings. Meets A5.15, Class Est.

| Typical Mechanical Properties | |
|---|---|
| Tensile Strength | 60 ksi, 42.19 kgs/mm2 |
| Color Match | Good |
| Current | AC/DC Reverse Polarity |
| Part No. | Model / Product Description | UPC |
|---|---|---|
| 69001019 | A/S *6IMP 1/8 DISPLAY PACK | 662303065591 |
| 69010026 | A/S 6IMP 1/8X14X10X40 | 662393000236 |
| 69010027 | A/S 6IMP 5/32X14X10X40 | 662393000243 |
| 69011026 | A/S 6IMP 1/8X14X1X10# | 662393014349 |
| 69015026 | A/S 6IMP 1/8X14X5# | 662393001493 |
| 69015027 | A/S 6IMP 5/32X14X5X40# | 000000000000 |
Recommended for welding extremely dirty or grease soaked castings,where other electrodes fail. Widely used on reclamation of motor housings,machine bases,levers and cams,farm machinery castings where machinability is not necessary. Recommended for a first pass for a good bond on dirty cast iron. May be finished with any All-State machinable electrode for cast iron.
Entire weld area should be clean. Cracks or edges may be grooved or beveled with All-State Chamfer Rod. Preheating to approximately 400° - 500°F.(204° - 260°C.),helps reduce stresses on complicated castings. Use lowest possible amperage that will give good fusion and "skip weld" whenever possible to distribute heat more evenly. Maintain an arc length of about 1/8" (3.2mm).Not recommended for DC straight polarity. Use AC or DC reverse polarity only.
All listed prices are in U.S. dollars and represent the Manufacturer's Suggested Retail Price (MSRP) for sale in the United States. Actual selling price will be determined by the Distributor. Prices are subject to change without notice.