The best electrode for welding cast iron to itself, to ductile iron or to dissmilar metals. Deposit is strong, machinable and crack resistant without porosity on thick sections as well as dissimilar thickness. Spray-like transfer. Rod won't overheat at rated amperages. Weld deposit has excellent color match to base metal.
Unique AC/DC straight or reverse electrode for heavy sections of cast iron, ductile iron and dissimilar metals. Strong, machinable,crack resistant deposits without porosity, yet spatter free. No overheating at rated amperage.

| Typical Mechanical Properties | |
|---|---|
| Tensile Strength | Up to 80 ksi, 56.25 kgs/mm2 |
| Yield Strength | Up to 60 ksi, 42.19 kgs/mm2 |
| Elongation In 2" | 4-12 % |
| Hardness | 200 to 300 Brinell |
| Deposit | Magnetic |
| Color Match | Good |
| Part No. | Model / Product Description | UPC |
|---|---|---|
| 69001001 | A/S SUPER 4-60 DSPL PK (8RODS) | 662393000014 |
| 69010017 | A/S SUPER 4-60 3/32X9X5X40 | 662393000182 |
| 69010018.0000001 | A/S SUPER 4-60 1/8X14X5#X40# | 662393009666 |
| 69010019 | A/S SUPER 4-60 1/8X14X10X40 | 662393000199 |
| 69010024 | A/S SUPER 4-60 5/32X14X10X40 | 662393000229 |
| 69011020 | A/S SUPER 4-60 3/32X9X1# | 662393014165 |
| 69011022 | A/S SUPER 4-60 1/8X14X1# | 662393014172 |
| 69010018 | A/S SUPER 4-60 1/8X14X5#X40# | 662393009666 |
| 69010001 | A/S SUPER 4-60 3/32X12X5X40VAL | 662393520314 |
| 69011023 | A/S SUPER 4-60 3/32X12X1# | 662393668054 |
Heavy cast iron machine bases, pump and differential housings: build up applications on cast iron dies, cylinder heads, engine blocks, heavy equipment parts, gear teeth,sprockets; joining cast and ductile iron to steel and cast iron pipe/flanges, housings.