ALL-STATE 4IMP

Premium all-position electrode for welding thin sections of cast iron. Provides dense, machinable, non-cracking, porosity free welds. For filling defects, repairing cracks and build-up repair.

Features

Premium AC/DC reverse, all-position electrode for welding thin sections of cast iron. Provides dense, machinable non-cracking, porosity free welds. For filling defects repairing cracks, and build-up repair.

Classifications

Properties

Typical Properties
Typical Mechanical Properties  
Tensile Strength Up to 50 ksi, 35 kgs/mm2
Yield Strength Up to 40 ksi, 28 kgs/mm2
Elongation In 2" 2-4 %
Hardness 175 to 225 Brinell
Deposit Magnetic
Color Match Good

Part No.

4 IMP
Part No. Model / Product Description UPC
69001028 A/S *4IMP 1/8 DISPLAY PACK 662303065614
69001030 A/S 4IMP 3/32 DISPLAY PACK 662303065621
69210014 A/S 4IMP 3/32X9X1# 662393014356
69200014 A/S 4IMP 3/32X9X5X40 662303123451
69200015 A/S 4IMP 1/8X14X5X40 662393005538
69200016 A/S 4IMP 5/32X14X5X40 662393005545
69200017 A/S 4IMP 1/8X14X10X40 662393005552
69200018.0000001 A/S 4IMP 5/32X14X10X40 662393005569
69210015 A/S 4IMP 1/8X14X1#T 662393014363
69200018 A/S 4IMP 5/32X14X10X40 662393005569

SAW

Accessories

Depositions/Paramaters

Extra Info

Repairing breaks and cracks in thin sections of cast iron, filling holes and defects in castings, and building up missing or worn parts.

Procedure

Preheat is not necessary but warming to 400°F(204°C) will produce a softer and more machinable deposit. All-State Chamfer Rod may be used to "V" the joint before welding. Remove all dirt, grease, and foreign material by grinding. A medium arc should be used with stringer beads or narrow weave beads. Peening after each pass will help to relieve stresses.