Print this page

ALL-STATE 3 BARE

General purpose cast iron rod

Features

High quality general purpose-cast iron torch alloy. Flows at lower temperatures without melting base metal. Used for maintenance and repair of heavy and light castings. Use with All-State No.5 flux.

Classifications

Properties

Typical Properties
Typical Mechanical Properties  
Tensile Strength Up to 45 ksi, 31.65 kgs/mm2
Hardness 175 to 225 Brinell
Working Temperature 1500 °F, 816 °C
Color Match Good

Part No.

3 Bare
Part No. Model / Product Description UPC
69050004 A/S 3 1/8X16X10#X40# 662393014684
69050005 A/S 3 BARE 1/8X20X10 662393002391
69050008 A/S 3 3/16X16X10#X40# 662393014691
69050009 A/S 3 1/4X16X10#X40# 662393014707
69051003 A/S 3 1/8X16X1#X10# 662393014714
69051005 A/S 3 1/8X20X1#X10 662393014462

SAW

Accessories

Depositions/Paramaters

Extra Info

Commonly used for maintenance and production welding of both heavy and light castings.It is extensively used for repairing cracks and breaks,filling surface defects and building up worn or missing parts where highest quality work is required a machinable deposit is a must.Cylinder heads,blocks,manifolds are a few applications.

Procedure

Remove all scale,rust,dirt and grease.Use All-State Chamfer Rod or other means to vee out joint to 80 degrees.Preheat casting to 800°F.(427°C.) A large tip with a neutral flame should be used.Hold torch so that inner cone is 1/8""(3.2mm) to 1/4""(6.4mm)from base metal,continue to heat until an area about 1"" in diameter turns a dull red;dip heated end of rod into All-State No.5 flux and apply a small amount of alloy.Flow each deposit out continuing to add alloy and flux.Each pass should not be more than 1/4""(6.4mm)thick. Continue welding until job has been completed. Allow to cool slowly by covering with an insulating material.