A self-fluxing brazing alloy for copper to copper (.001" to .002"). Do not use with ferrous metals. For best results use with All-State S-200 or No. 110 flux when joining copper to brass or bronze.
A self-fluxing alloy for copper to copper joining. Use where close fit-up cannot be maintained. Use All-State S-200 flux when joining brass or bronze metals. Additional sizes available upon request. Tip of rod colored light blue.

| Nominal Chemical Composition | |
|---|---|
| Phosphorous | 6 % |
| Silver | 5 % |
| Liquidus | 1485 °F, 643 °C |
| Brazing temperature range | 1300 to 1500 °F, 704 to 816 °C |
| Solidus | 1190 °F, 643 °C |
| Copper | Balance |
| Part No. | Model / Product Description | UPC |
|---|---|---|
| 69060041 | A/S SLFLO-5 1/16X36X10# | 662393003510 |
| 69060043 | A/S SFLO-5 050X1/8X18X25 | 662393003527 |
| 69060061 | A/S SIFLO-5 050X1/8X18X10X40 | 662393003565 |
| 69060062 | A/S SFLO-5 050X1/8X18X1# TB | 662393003572 |
| 69060066 | A/S SILFLO 5 3/32SQ 3/32X20X25 | 662393520260 |
| 69060065 | A/S SILFLO 5 3/32SQ 3/32X20X1# | |
| 69060067 | A/S SILFLO 5 1/8X20X1# | |
| 69060044 | A/S SFLO-5 1/8SQX36X10X60 | 662393003534 |
Clean joint area. Jigs and fixtures will help hold parts in place. Paint brass and bronze parts with All-State No. 110 or S-200 Flux. Use a large tip, heat broadly until flux liquifies or copper turns dull red. Apply sufficient alloy to fill joint. Do not overheat or remelt. Submerge in hot water and brush to remove flux. Ten percent sulfuric acid and water solution will restore copper color. Rinse with clear hot water.