ALL-STATE SILFLO 0

A self-fluxing brazing alloy for copper to copper joining. For tight fitting joints (.001" to .002"). Do not use with ferrous metals. For best results use with All-State S-200 or No. 110 flux when joining copper to brass or bronze.

Features

A self-fluxing brazing alloy for copper to copper joining. For tight fitting (.001" to .002") areas. Use All-State S-200 flux when joining brass or bronze metals. Tip of rod colored grey.

Classifications

Properties

Typical Properties
Nominal Chemical Composition  
Phosphorous 7 %
Liquidus 1460 °F, 793 °C
Brazing temperature range 1350 to 1550 °F, 732 to 843 °C
Solidus 1310 °F, 710 °C
Copper Balance

Part No.

SILFLO 0
Part No. Model / Product Description UPC
69050053 A/S SILFLO 0 050X1/8X18X25# 662303065386
69050054 A/S SILFO 0 050X1/8X18X10X40 662393002551
69050055 A/S SILFO 0 050X1/8X18X1# 662393002568
69060030 A/S SILFO 0 1/16X36X10X60 662393003473
69060032 A/S SILFO 0 3/32X36X10X60 662393003480
69060033 A/S SILFO 0 1/8RDX36X10X60 662393003497
69060034 A/S SILFO 0 1/8SQX36X10X60 662393003503
69061030 A/S SILFLO CU 0 1/16RDX36X1# 662393003602
69061032 A/S SILFLO CU 0 3/32RDX36X1# 662393003619
69061033 A/S SILFO 0 1/8RDX36X1# 662393003626
69061034 A/S SILFLO CU 0 1/8SQX36X1#X 662393003633
69060035 A/S SILFO 0 1/4SQX36X10X60 662393519639

SAW

Accessories

Depositions/Paramaters

Extra Info

Procedure

Clean joint area. Jigs and fixtures will help hold parts in place. Paint brass and bronze parts with All-State No. 110 or S-200 Flux. Use a large tip, heat broadly until flux liquifies or copper turns dull red. Apply sufficient alloy to fill joint. Do not overheat or remelt. Submerge in hot water and brush to remove flux. Ten percent sulfuric acid and water solution will restore copper color. Rinse with clear hot water.

Complementary Products

Seismic Data

All listed prices are in U.S. dollars and represent the Manufacturer's Suggested Retail Price (MSRP) for sale in the United States. Actual selling price will be determined by the Distributor. Prices are subject to change without notice.