ALL-STATE Low Fuming Bronze FC

General purpose brazing rod.

Features

The alloy is designed to meet today's high industrial standards. The flux coated rods have a waterless coating that gives a superior cleaning action and promotes wetting qualities.

Classifications

Properties

Typical Properties
Typcial Mechanical Properties  
Tensile Strength 60 ksi, 42.19 kgs/mm2
Working Temperature 1600 to 1600 °F, 871 to 871 °C

Part No.

Low Fuming Bronze FC
Part No. Model / Product Description UPC
69063006 A/S LFB FC 3/32X36X1# TUBE 662393011959
69063020 A/S LFB FC 3/32X36X5X30 662393003671
69063021 A/S LFB FC 1/8X36X5X30 662393003688

SAW

Accessories

Depositions/Paramaters

Extra Info

Fabricating or repairing steels, cast iron, copper base metals, galvanized and malleable irons or any combination of these metals.

Procedure

Clean joint area. Heat base metal using a neutral flame. Apply small amount of flux by melting the coating. Continue to heat. Melt a drop of alloy when flux turns liquid. Continue this procedure until job is complete. The All-State Jet Flux Dispenser is recommended for use with bare rods for convenience and speed.