ALL-STATE LOW FUMING BRONZE

A general purpose brazing rod for fabricating or repairing steels, cast iron, copper base metals, galvanized and malleable irons or any combination of these metals. Available as base or build-up repair.

Features

A bare torch rod for fabricating or repairing steels, cast iron, copper base metals, galvanized and malleable irons or any combination of these metals. Use All-State Brazaloy No.1, No.5, Brazo flux or All-State Jet Flux when using bare rod.

Classifications

Properties

Typical Properties
Typcial Mechanical Properties  
Tensile Strength Up to 60 ksi, 42.19 kgs/mm2
Working Temperature 1600 to 1600 °F, 871 to 871 °C

Part No.

Low Fuming Bronze
Part No. Model / Product Description UPC
69062009 A/S LFB BARE 3/16X36X1# 662303065409
69062030 A/S BRAZ CU LFB 1/16X36X1#X20# 662303065416
69063000 A/S LFB BARE 1/16X36X5X30 662393003640
69063001 A/S LFB BARE 3/32X36X5X30 662393003657
69063002 A/S LFB BARE 1/8X36X5X30 662393003664
69160511 A/S LFB BARE 3/32X36X1# 662393011973
69702030 A/S LFB BARE 3/32X36X25 F2 662303667795

SAW

Accessories

Depositions/Paramaters

Extra Info

Fabricating or repairing steels, cast iron, copper base metals, galvanized and malleable irons or any combination of these metals.

Procedure

Clean joint area. Heat base metal using a neutral flame. Dip the end of heated rod into All-State Brazo Flux and then apply to the work. Continue to heat. Melt a drop of alloy when flux turns liquid. Continue this procedure until job is complete. The All-State Jet Flux Dispenser is recommended for use with bare rods for convenience and speed.