ALL-STATE 430 Paste

Low temperature solder in paste form.

Features

Cadmium free, low temperature, food grade solder in mesh form premixed with flux. For use on stainless and dissimilar metals.

Classifications

Properties

Typical Properties

Part No.

430 Paste
Part No. Model / Product Description UPC
69070080 A/S DYNAGRIP 430 PST SDR 8 OZ 662393003831

SAW

Accessories

Depositions/Paramaters

Extra Info

Same as 430 SLDR except that No. 430 solder in mesh form has been premixed with an active flux entending its range of applications. Used in Automobile radiator repair.

Procedure

When using on stainless steels, add 1 drop of Duzall flux to joint carrying paste before heating.